🥊 BS EN ISO 00179 (i.e. BS EN ISO 179) is the British adoption of the European standard EN ISO 179, identical to the ISO 179 series, which specifies methods for determining the Charpy impact properties of plastics. Impact properties reflect a material’s toughness under high-speed deformation and are a key selection criterion for plastics in structural parts, packaging, automotive components, and other applications. The Charpy impact test applies an impact load to a notched or unnotched specimen via a pendulum and measures the energy consumed in fracture, thereby evaluating the material’s impact resistance. The series was prepared by ISO/TC 61 (Plastics) in cooperation with CEN/TC 249 (Plastics), providing a standard method for the uniform evaluation of plastics impact properties.
This series applies to rigid plastics and plastic products for Charpy impact determination, and also to reinforced plastics and fibre composites. Tests are carried out under specified specimen geometry, notch type, and impact conditions to determine the energy-absorption characteristics under impact loading. The standard gives complete requirements for specimen dimensions, notch types, pendulum parameters, test procedure, and result calculation.
Two parts are included in this batch:
| Standard | Corresponding ISO | Main Content | Feature |
|---|---|---|---|
| BS EN ISO 179-1:2010 | ISO 179-1:2010 | Non-instrumented impact test: specimen, pendulum, procedure, impact-strength calculation | Routine quality control, simple and fast |
| BS EN ISO 179-2:1999+A1:2012 | ISO 179-2:1997+Amd.1:2011 | Instrumented impact test: force-time recording, initiation and propagation energy analysis | Materials research and failure analysis |
BS EN ISO 179-1 is the basic method. The specimen is a rectangular bar that may be V-notched, U-notched, or unnotched. After the pendulum is released and strikes the specimen, the energy absorbed in fracture is determined from the pendulum’s potential-energy loss. The standard specifies standard specimen dimensions (e.g. 80 mm × 10 mm × 4 mm), notch dimensions, pendulum energy, impact velocity, and gives the impact-strength (kJ/m²) calculation formula. The 2010 edition supersedes the 2001 edition, revising some test details.
BS EN ISO 179-2 adds a load transducer and signal-recording system to the specimen and pendulum, continuously recording the load as a function of time during impact to produce a force-time or force-displacement curve. This allows the total impact energy to be decomposed into initiation energy and propagation energy, providing deeper insight into toughness and fracture behaviour. Amendment A1:2012 updates Clause 9 and adds Annex D. Instrumented testing demands more from equipment and operators and is suited to materials development, failure analysis, and quality tracing.
Specimens should be prepared by the specified method (injection moulding, compression moulding, or machining), with a flat, defect-free surface and dimensions per the standard. Before testing, specimens should be conditioned (temperature and humidity) as required to ensure comparable results.
The pendulum’s nominal energy should be adequate so the residual energy after fracture is not less than a specified proportion; impact velocity and pendulum geometry should meet standard requirements. Notch type (V/U) and notch machining quality directly affect results and must be tightly controlled.
Impact strength is calculated as the fracture energy divided by the specimen cross-sectional area (for notched specimens, the net area at the notch). Results should report impact-strength value, specimen type, notch type, and test conditions, and where appropriate the mean and scatter.
Part 2 requires the load transducer to have sufficient frequency response and a sampling rate that meets the resolution of the force-time curve. The determination of initiation and propagation energy relies on characteristic points of the curve (such as peak load) and gives a clear data-processing method.