BS EN ISO 00148 — Metallic Materials — Charpy Pendulum Impact Test Standard Series

Test method, verification of testing machines, and preparation & characterisation of V-notch reference specimens (implementing ISO 148)

⚙️ BS EN ISO 148 is the British Standards Institution (BSI) adoption of EN ISO 148, identical to ISO 148, covering metallic materials — Charpy pendulum impact test. The series is maintained by BSI Technical Committee ISE/101/4 (Toughness testing), classified under ICS 77.040.10 (Mechanical testing of metals). The Charpy impact test is a classic method for evaluating the toughness of metallic materials: a notched specimen is broken by a striking pendulum, and the absorbed energy (impact absorption energy) reflects the material’s resistance to brittle fracture. It is widely used for quality inspection, low-temperature toughness evaluation and failure analysis of steels and other metals. The series specifies the Charpy pendulum impact test method, verification of testing machines, and preparation and characterisation of Charpy V-notch reference specimens.

💡 The core of the impact test is the “energy criterion”: the pendulum released from a specified height breaks the specimen, and the energy difference from the pendulum’s remaining height is the absorbed energy KV (J). The higher the absorbed energy, the better the material’s toughness; the value is very sensitive to notch, temperature and test conditions, so conditions must be strictly standardised.

1. Scope and Basic Framework 📌

The series was prepared by ISO TC 164 (Mechanical testing of metals) in collaboration with European ECISS/TC 101, comprising three parts, all under ICS 77.040.10:

StandardSubjectCorresponding ISOKey Content
BS EN ISO 148-1:2016Test methodISO 148-1:2016Charpy pendulum impact test method (a newer edition has superseded this)
BS EN ISO 148-2:2016Verification of testing machinesISO 148-2:2016Verification of impact testing machines (pendulums)
BS EN ISO 148-3:2016Preparation and characterisation of reference specimensISO 148-3:2016Preparation and characterisation of Charpy V-notch reference specimens
⚠️ Note the edition: the 2016 edition of Part 1 superseded the 2010 edition, and some earlier parts already have newer editions published; when using this series, verify the latest effective edition and note the version required by PPAP/purchase documents.

2. Series Structure and Technical Points 🔧

2.1 Part 1: Test method

BS EN ISO 148-1 specifies the Charpy pendulum impact test method for metallic materials, covering specimen shape and dimensions (standard specimen 55 mm × 10 mm × 10 mm with a V-notch), notch geometry, test apparatus, test temperature, test procedure, result calculation (absorbed energy, lateral expansion, etc.) and reporting format. It is the core of the series, specifying “how to perform an impact test correctly”.

2.2 Part 2: Verification of testing machines

BS EN ISO 148-2 specifies the verification method for impact testing machines, including checks of pendulum energy, striking centre, anvil and striker geometry, and friction loss, ensuring the machine’s measurement results are accurate and traceable. Regular verification is a prerequisite for credible impact data.

2.3 Part 3: Preparation and characterisation of reference specimens

BS EN ISO 148-3 specifies the preparation and characterisation of Charpy V-notch reference specimens. Reference specimens are standard specimens used to verify testing machines and laboratory capability; their preparation, uniformity inspection and absorbed-energy calibration must conform to the requirements, ensuring data comparability between laboratories.

3. Key Technical Requirements and Test Parameters 🔍

Key technical essentials of the Charpy impact test include:

  • Specimen geometry: standard specimen dimensions and V-notch (depth, angle, root radius) must conform to the standard; notch-machining deviations directly affect results.
  • Pendulum and striking conditions: pendulum energy, striking velocity, striker and anvil geometry, and striking-centre position must meet standard requirements.
  • Test temperature: the specimen must be stabilised at the specified temperature (e.g. room temperature or low temperature) and transferred quickly before breaking; results are invalid if temperature deviation exceeds limits.
  • Absorbed energy: the absorption energy calculated from the pendulum potential-energy change, the quantitative indicator of toughness; where required, record lateral expansion and fracture appearance.
  • Result validity and statistics: the number of specimens per test and the treatment of invalid results (e.g. specimen not fully broken, jammed) follow the standard.
✅ The series adopts a “test method — machine verification — reference specimen” three-part structure: first use Part 1 to standardise how the test is done, then use Part 2 to ensure the machine measures accurately, and finally use Part 3 to provide traceable reference specimens — together ensuring the reliability and cross-laboratory comparability of impact data.

4. Test Methods and Quality Assurance 🧪

A typical test and quality-assurance flow includes:

  • Specimen preparation and inspection: machine the notched specimen per the standard and check dimensions and notch root radius.
  • Temperature conditioning: place the specimen at the specified temperature in a controlled medium and hold for the specified time.
  • Impact test: quickly transfer the specimen to the anvil, strike and break it with the pendulum, and record the absorbed energy.
  • Machine verification: periodically verify pendulum energy, striking centre and geometric parameters per Part 2.
  • Reference-specimen validation: use calibrated reference specimens per Part 3 to verify the machine and inter-laboratory capability.

Results are reported per the standard format, noting the test temperature, specimen type and notch type.

5. Engineering Practice and Application 🛠️

  • 🔍 Steel quality inspection: structural steel, pressure-vessel steel and low-temperature steel use impact absorption energy as a toughness acceptance indicator.
  • 🔧 Low-temperature toughness evaluation: perform impact tests at low temperature to evaluate the ductile-brittle transition behaviour and service safety of materials.
  • 📊 Welding procedure qualification: impact tests of welded joints are used to evaluate the toughness of the filler metal, procedure and heat-affected zone (HAZ).
  • 📋 Failure analysis and research: use impact data to help determine the cause of brittle fracture and assess the effects of heat treatment and alloying.

6. Frequently Asked Questions ❓

❓ Q: What does the Charpy impact absorption energy (KV) represent?
A: It represents the energy absorbed by the pendulum in breaking a standard notched specimen, reflecting the material’s toughness; the higher the absorption energy, the stronger the resistance to brittle fracture. It is a relative indicator, affected by notch, temperature and specimen dimensions.
❓ Q: What do Parts 1, 2 and 3 address?
A: Part 1 specifies “how to test” (method), Part 2 ensures “whether the machine is accurate” (verification), and Part 3 provides “standard traceable reference specimens” to validate the test system — together forming a complete quality-assurance chain.
❓ Q: Why is test temperature so critical?
A: Metal toughness varies significantly with temperature, and many steels transition from ductile to brittle at low temperatures. Specimen temperature deviation changes the absorption energy result, so the standard requires holding at the specified temperature and quick transfer to minimise temperature drift.
🔍 Q: What is the difference between instrumented and non-instrumented impact testing?
A: Non-instrumented (conventional) impact records only the total absorption energy; instrumented impact records the force-displacement (or force-time) curve during impact, providing more detailed information such as initiation and propagation energy, useful for in-depth study of fracture behaviour.
❓ Q: How is cross-laboratory comparability of impact data ensured?
A: Test strictly per Part 1, verify machines per Part 2, use calibrated reference specimens per Part 3 for validation, and participate in inter-laboratory comparisons; only when test conditions, equipment and specimens all conform to the standard are data comparable.
🔒
正在加载下载地址,请稍候 10 秒