BS EN ISO 00105 — Textiles Tests for Colour Fastness Standard Series (ISO 105)

Textiles — Tests for Colour Fastness Standard Series (ISO 105)

🧵 BS EN ISO 105 (files numbered BS EN ISO 00105 in this batch) is the UK national implementation by BSI of the ISO 105 family of colour-fastness test methods, comprising about 35 parts. It is the fundamental method system by which the textile, dyeing, garment and testing industries evaluate the ability of dyes and textiles to resist colour change during use and processing. Maintained under technical committee TCI/81 (Colour fastness and colour measurement of textiles), it uses the “Part — Series — Method” structure covering light, washing, rubbing, perspiration, water, weathering and assessment principles. The series is widely referenced by global procurement specs, eco-labels and regulations.

⚠️ Some parts are scanned versions, compiled from public-domain knowledge: this series includes several scans (e.g. B03, B04, B08, N04, N05, P01/P02, X02, X10/X11/X12, X14). This article synthesises the publicly available ISO 105 framework; specific reagents, grey scales and test conditions should be taken from the official BSI published version.

1. Series Overview and Structure 📌

ISO 105 uses a “Part + letter-series + method-number” system: Part A is general and assessment, Part B light and weathering, Part C washing and domestic laundering, Part D colour-fastness to physical properties, Part E water/sweat/seawater/water spotting, Part F adjacent fabrics, Part G solvents and dry-cleaning, Part X special methods, Part P/N special-purpose methods.

  • Part A (General): A01 general principles, A02 grey scale for colour change, A03 grey scale for staining, A04 instrumental assessment of staining, A11 digital-imaging grading.
  • Part B (Light/Weather): B01 daylight, B02 xenon-arc, B03 weathering, B04 mercury lamp (humid heat).
  • Part C (Washing): C06 domestic washing, C08 boiling.
  • Part E (Water/Perspiration): E01 water, E04 perspiration, E02 seawater, E03 water spotting.
  • Part X/P/N (Special): X12 rubbing, P01 dry heat, N series chemical reagents.

2. Series Composition and Key Topics 🔧

Standard No.SubjectSeriesTypical Content
EN ISO 105-A01General principlesPart ACommon conditions for all fastness tests
EN ISO 105-A02Grey scale for colour changePart AVisual 1–5 grade for colour change
EN ISO 105-A04Instrumental staining assessmentPart AMeasurement of adjacent-fabric staining
EN ISO 105-A11Digital imaging gradingPart AGrades by digital-image techniques
EN ISO 105-B02Artificial light (xenon)Part BXenon-arc light-fastness test
EN ISO 105-C06Domestic washingPart CWash at varied temp/detergent
EN ISO 105-E04PerspirationPart EAcid/alkali artificial sweat staining
EN ISO 105-X12RubbingPart XDry/wet rubbing colour transfer
EN ISO 105-P01Dry heat (ironing)Part PEffect of hot pressing on colour
EN ISO 105-N05Chlorinated solventsPart NColour stability in dry-cleaning solvent
💡 EN ISO 105-A11 introduces digital-image technology to determine fastness grades, replacing part of the visual grey-scale grading with camera and software, improving inter-laboratory consistency and lowering human error — a powerful complement to traditional grey-scale grading.

3. Key Technical Requirements 🔥

Assessment principles (Part A). A01 sets common conditions (temperature, humidity, adjacent-fabric combination, specimen size); A02 (colour change) and A03 (staining) use grey scales for 1–5 visual grading — grade 5 no change, grade 1 severe change; A04 quantifies adjacent-fabric staining instrumentally.

Light and weathering (Part B). B02 uses a xenon-arc lamp to simulate daylight, controlling exposure by blue-wool references or radiant dose and assessing colour change; B03 further assesses outdoor weathering (light + rain + temperature).

Washing and perspiration (Part C/E). C06 grades wash fastness by temperature, alkalinity and mechanical action; E04 uses acid/alkali artificial sweat to assess fastness of skin-contact textiles, relevant to skin-contact safety.

Rubbing (X12). A white cotton cloth rubs the specimen dry and wet to assess surface-colour transfer to the white cloth.

4. Engineering Practice Essentials 🛠️

  • 🔍 Contract references: apparel and home-textile specs list the ISO 105 parts required and minimum grades (e.g. wash 4, light 5).
  • 🔧 Lab consistency: adopt A11 digital imaging or unified grey scales with standard light to reduce grading divergence.
  • 📊 Eco and regulation: combine with eco-labels (e.g. OEKO-TEX) and chemical regulations, treating fastness as an indirect control of harmful substances.
  • 📋 Reporting: report the part number, grade, adjacent fabric and conditions for traceability.

5. Test Equipment and Grade Management 🖥️

Reliable fastness grading depends on standardised equipment and grade management: light-fastness tests need a xenon lamp with the specified spectral irradiance (filter combinations, radiant-dose control) and exposure controlled by blue-wool references or dose; washing and perspiration tests use prescribed temperature/time and soap/artificial-sweat recipes, with specimens assembled with adjacent fabrics per each part’s stitching layout. Grey scales should be checked periodically for colour drift to avoid grade offset, and grading should be done under standard illumination (e.g. D65) in a light cabinet, by observers validated for normal colour vision and trained.

For result management, laboratories should keep condition records (exposure time, temperature, solution concentration) and Lab colour data (when using instrument/method A04/A11) for dispute review. Batch consistency can be monitored with reference fabrics run per batch to detect instrument and operator drift. On the eco/regulatory side, fastness grades are often combined with substance restrictions (banned azo dyes, sensitising disperse dyes), making grading part of supply-chain compliance — grades are thus both quality indicators and trade-compliance evidence and must be archived properly.

6. Frequently Asked Questions ❓

❓ Q: Is BS EN ISO 105 identical to ISO 105?
A: Yes. The series adopts ISO 105 text identically with only a UK national foreword; the technical clauses are the same, and you can cite the ISO 105-X numbers directly.
❓ Q: What does grade 5 on grey scales A02/A03 mean?
A: Grade 5 means no visible change from the original (best); grade 1 means severe colour change or staining (worst), with half-grade steps in between.
❓ Q: How do light (B02) and weathering (B03) differ?
A: B02 uses a xenon arc to simulate daylight and assesses only light-induced change; B03 adds spray/humidity/temperature cycling to simulate outdoor climate.
🔍 Q: Can digital imaging (A11) replace visual grading?
A: A11 provides a repeatable imaging method as a complement or alternative for batch testing, but contested results are still decided by visual grading under standard illumination.
🔒