🧱 BS EN 846 is the UK national standard implementing the European standard series EN 846 “Methods of test for ancillary components for masonry”, prepared by CEN/TC 125 (Masonry) with UK participation through Technical Committee B/519 and its Subcommittees B/519/3 (Ancillary components) and B/519/1 (Masonry units). The series specifies test methods for the load-bearing performance, dimensions, deformation, and durability of ties, anchors, lintels, brackets, hangers, and similar ancillary components, serving as the companion test standard to the EN 845 product specification series.
Although ancillary components for masonry (such as wall ties, lintels, brackets, and hangers) are small in size, they are critical to the overall stability of masonry structures and the load-bearing and safety of door/window openings. The EN 846 series is organised by component type and performance parameter: from tension/compression and shear performance of wall ties, load capacity of anchors, to dimensions and bow of lintels, load-deflection characteristics of brackets, and the resistance to impact, abrasion, and corrosion of organic (anti-corrosion) coatings. During the transition period, the UK retained existing BS standards; once the EN 845/846 package is complete, the corresponding old BS standards are progressively withdrawn.
| Part | Test Object / Performance | Edition |
|---|---|---|
| Part 2 | Tension and compression tests of ties/anchors | 2000 |
| Part 3 | Shear (transverse) tests of ties/anchors | 2000 |
| Part 4 | Bending (fatigue/flexural) tests of ties/anchors | 2002 (2005) |
| Part 5 | Deformation (lateral displacement) characteristics of ties/anchors | 2012 |
| Part 6 | Ultimate slip/pull-out of ties/anchors in masonry | 2012 |
| Part 7 | Tension and compression of ties/anchors (in mortar) | 2012 |
| Part 8 | Load-displacement and shear stiffness of anchors/connections | 2000 (2006) |
| Part 9 | Flexibility/deformation of flexible ties | 2016 |
| Part 10 | Load capacity and load-deflection characteristics of brackets | 2000 |
| Part 11 | Dimensions and bow of lintels | 2000 |
| Part 13 | Resistance to impact, abrasion and corrosion of organic coatings | 2001 |
| Part 14 | Performance of masonry/components under environmental conditions (durability) | 2012 |
Brackets support cantilevered masonry or decorative elements. This standard specifies the test method for applying a vertical load to a bracket and measuring its load capacity (ultimate load) and load-deflection characteristic curve: the bracket is mounted in a specified test rig, loaded in stages to failure or to a specified deflection, and the load-displacement relationship is recorded to evaluate load capacity and stiffness.
Lintels span door/window openings to support the masonry above. This standard specifies the method of measuring the length, cross-section dimensions, and bow (the camber/warp along the length) of lintels, to control straightness and ensure accurate opening dimensions and uniform loading after installation. Measurements are made under defined support and datum conditions, with allowable tolerances for dimensions and bow.
Ancillary components (especially ties and brackets) often use organic coatings (e.g. a further protective coating over galvanising) to improve corrosion resistance. This standard specifies test methods for the resistance of organic coatings to impact (falling weight/ball), abrasion (wear test), and corrosion (salt spray/immersion), important for evaluating long-term durability. This part supports the EN 845-1 and EN 845-2 product specifications.
The series specifies tension, compression, shear (transverse), bending, and deformation tests for wall ties and anchors, together with ultimate slip/pull-out, load-displacement, and shear-stiffness determinations, ensuring ties reliably connect inner and outer leaves, transmit lateral wind loads, and accommodate temperature/moisture movements.