BS EN 62333 — Noise Suppression Sheet for Digital Devices and Equipment Standard Series

Definitions and general properties, measuring methods and characterisation of parameters (implementing IEC 62333)

🧲 BS EN 62333 is the British Standards Institution (BSI) adoption of EN 62333, identical to IEC 62333, covering noise suppression sheets for digital devices and equipment. The series is maintained by BSI Technical Committee EPL/51 (Transformers, inductors, magnetic components and ferrite materials), classified under ICS 29.100.10. A noise suppression sheet is a flexible, high-permeability magnetic sheet (typically a polymer-based soft magnetic composite or ferrite-filled sheet) applied to the surface of digital devices or electronic modules to suppress high-frequency electromagnetic interference (EMI) and electromagnetic noise by absorbing or dissipating noise energy. It is commonly used near electronic equipment, communication modules, digital circuit boards and connectors. The series specifies terminology and general properties, measuring methods, and characterisation of parameters.

💡 Unlike conventional shielding sheets, a noise suppression sheet does not rely primarily on conductive shielding and reflection; it uses the magnetic loss of the magnetic material to absorb/dissipate high-frequency noise energy over a wide band, being particularly effective at tens of MHz to several GHz.

1. Scope and Basic Framework 📌

The series was prepared by IEC TC 51 (Magnetic components and ferrite materials) and comprises three parts, all under ICS 29.100.10. The series structure is:

StandardSubjectCorresponding IECKey Content
BS EN 62333-1:2006Definitions and general propertiesIEC 62333-1:2006Terms, definitions and general properties
BS EN 62333-2:2006+A1:2015Measuring methodsIEC 62333-2:2006+A1:2015Measuring methods for noise suppression performance (amendment adds a clause)
BS EN 62333-3:2010Characterisation of parametersIEC 62333-3:2010Characterisation methods for noise suppression sheet parameters
⚠️ Sequence of use: first understand terminology and general properties via Part 1, then characterise sheet parameters (permeability, magnetic loss) via Part 3, and finally evaluate noise suppression performance using the prescribed measuring methods of Part 2. Part 2 explicitly states it is to be used in conjunction with Part 1.

2. Series Structure and Technical Points 🔧

2.1 Part 1: Definitions and general properties

BS EN 62333-1 defines terms (e.g. noise suppression sheet, noise suppression factor, complex permeability) and specifies general properties — composition, structure, thickness, dimensions, mechanical properties and environmental adaptability — providing a common basis for subsequent measurement and characterisation.

2.2 Part 2: Measuring methods

BS EN 62333-2 specifies measuring methods for evaluating noise suppression performance, typically quantifying the suppression capability by measuring the insertion loss or S-parameters of a transmission-line/coupling system before and after installing the sheet. The standard gives the measurement apparatus, specimen arrangement, frequency range and data-processing method. The 2015 amendment (A1) added clauses to refine measurement details.

2.3 Part 3: Characterisation of parameters

BS EN 62333-3 specifies methods for characterising the parameters of the noise suppression sheet — how to extract and characterise the complex permeability, magnetic loss angle and related parameters from measurement data, enabling quantitative comparison of different sheets and providing data for material selection and design simulation.

3. Key Technical Requirements and Performance Criteria 🔍

The core performance of a noise suppression sheet can be understood along the following dimensions:

  • Complex permeability: the real part reflects the magnetising capability, and the imaginary part (magnetic loss) reflects the absorption/dissipation capability; the larger the magnetic loss over a wide band, the better the suppression.
  • Noise suppression factor / insertion loss: in the standard measurement system, the transmission attenuation or insertion loss caused by the sheet is a direct indicator of its suppression capability.
  • Frequency range: the sheet should be designed for the target noise frequency (typically tens of MHz to several GHz), with sufficient magnetic loss within the working band.
  • Thickness and placement: sheet thickness, distance from the noise source/coupling path and mounting method affect suppression; the standard provides corresponding measurement arrangements to standardise evaluation.
  • Mechanical and reliability: the sheet should have appropriate flexibility, adhesion and temperature/humidity resistance to suit assembly and operating environments.
✅ The key contribution of the series is turning “suppression effect” into a measurable, comparable quantitative indicator: through the standard measuring methods of Part 2 and parameter characterisation of Part 3, noise suppression sheets from different manufacturers and formulations can be compared and selected on a common scale.

4. Test Methods and Conformity Assessment 🧪

Typical tests and characterisation include:

  • Transmission parameter measurement: measure S-parameters or insertion loss on a standard transmission line/microstrip/coupling device, yielding the insertion-loss versus frequency curve.
  • Complex permeability measurement: measure the complex permeability (μ′ and μ″) as a function of frequency by impedance or resonance methods.
  • Noise suppression factor: calculate and report per the arrangement specified in Part 2.
  • Geometric and mechanical measurement: thickness, dimensions, flexibility, adhesion strength, etc.
  • Environmental tests: retention of performance after temperature, humidity and ageing.

Results should be recorded per the standard’s reporting format for cross-comparison and selection.

5. Engineering Practice and Application 🛠️

  • 🔍 PCB EMI suppression: attach noise suppression sheets near high-speed digital signal lines, clock lines and connectors to reduce near-field coupling and common-mode noise.
  • 🔧 Communication and RF modules: attach inside RF front-ends, antennas and shielding cans to suppress harmonics and spurious emission.
  • 📊 Portable electronic devices: attach inside smartphones and tablets to improve EMC performance and suppress internal noise crosstalk.
  • 📋 Automotive electronics and industrial control: use near power electronics, motor drives and sensor interfaces to improve electromagnetic immunity.

6. Frequently Asked Questions ❓

❓ Q: How do noise suppression sheets differ from conductive shielding materials?
A: Conductive shielding (e.g. copper foil, conductive adhesive) blocks electromagnetic waves mainly by reflection and conduction; a noise suppression sheet absorbs and dissipates high-frequency noise energy through magnetic loss, being particularly effective for near-field coupling noise at high frequencies and not requiring grounding.
❓ Q: How should the three parts of BS EN 62333 be used together?
A: Part 1 gives terminology and general properties, Part 3 gives parameter characterisation, and Part 2 gives measuring methods and states it is used with Part 1. To evaluate a sheet, first understand its definition, then characterise its parameters, and finally evaluate suppression performance by the standard measuring method.
❓ Q: Why is “complex permeability” a key parameter?
A: The imaginary part (μ″) represents magnetic loss, directly determining the sheet’s ability to convert electromagnetic energy into heat; the real part (μ′) determines magnetising capability. The larger μ″ over a wide band, the better the high-frequency noise suppression.
🔍 Q: Can a noise suppression sheet completely eliminate EMI?
A: No. It mainly suppresses near-field noise in specific frequency bands and coupling paths; for far-field radiation, conducted interference and low-frequency magnetic fields, shielding, filtering and grounding are also required.
❓ Q: How do I compare the performance of different noise suppression sheets?
A: Use the standard measuring method and arrangement of BS EN 62333-2 to measure the insertion-loss versus frequency curve, and cite the parameter characterisation results of Part 3, to compare different sheets on a common scale.
🔒