BS EN 62329 — Heat-shrinkable Moulded Shapes Standard Series

Specification requirements for shape dimensions, material requirements and compatibility performance (implementing IEC 62329)

🔥 BS EN 62329 is the British Standards Institution (BSI) adoption of EN 62329, identical to IEC 62329, covering heat-shrinkable moulded shapes for electrical purposes. The series is maintained by BSI Technical Committee GEL/15 (Solid electrical insulating materials) through Subcommittee GEL/15/5 (Flexible insulating sleeving for electrical purposes), classified under ICS 29.035.01. Heat-shrinkable moulded shapes are pre-formed, three-dimensional moulded products used in electrical, electronic and cable-harness systems for insulation, sealing, strain relief and mechanical protection — when heated they shrink to conform tightly to the protected component, forming a robust, weather-resistant and electrically insulating outer layer. The series specifies shape dimensions, material requirements and compatibility (system) performance, providing tests and acceptance criteria for specific material types.

💡 Unlike plain heat-shrink tubing, moulded shapes are pre-formed three-dimensional forms (e.g. breakouts, boots, cones, caps) commonly used at cable bifurcations, terminal seals and connector boot areas; this series provides a unified specification language for these mouldings.

1. Scope and Basic Framework 📌

The series was prepared by IEC TC 15 (Solid electrical insulating materials) and comprises three sheets, all under ICS 29.035.01. The series is organised around “Part 3: Specification requirements for shape dimensions, material requirements and compatibility performance” and is subdivided by material and application as follows:

StandardSubjectCorresponding IECKey Content
BS EN 62329-3-100:2010Heat-shrinkable moulded shape dimensions (Sheet 100)IEC 62329-3-100:2010Specification requirements for shape dimensions
BS EN 62329-3-101:2010Polyolefin, semi-rigid, limited fire hazard moulded shapes (Sheet 101)IEC 62329-3-101:2010Material requirements and system performance
BS EN 62329-3-102:2010Elastomeric, semi-rigid moulded shapes (Sheet 102)IEC 62329-3-102:2010Material requirements and system performance
⚠️ Note the “Sheet 100/101/102” structure: Sheet 100 gives the common dimensional system for all moulded shapes; Sheets 101 and 102 respectively address polyolefin and elastomeric materials, specifying their material properties and post-shrink system (compatibility) performance.

2. Series Structure and Technical Points 🔧

2.1 Sheet 100: Moulded shape dimensions

BS EN 62329-3-100 specifies the dimensional series and tolerances for heat-shrinkable moulded shapes, including measurement and allowable deviation of key dimensions (internal diameter, wall thickness, length, branch angle, etc.) before and after shrinkage. It provides a unified dimensional system for design and selection, enabling interchangeability and matching between similar products from different manufacturers, together with test methods for dimension measurement.

2.2 Sheet 101: Polyolefin, semi-rigid, limited fire hazard moulded shapes

BS EN 62329-3-101 applies to heat-shrinkable moulded shapes based on polyolefin, semi-rigid, with limited fire hazard. The standard specifies material requirements (e.g. tensile strength, elongation at break, density, flame retardancy and heat resistance) and system performance (sealing, chemical resistance, ageing resistance and electrical insulation after shrinkage over cables/joints), together with the relevant test methods and required results.

2.3 Sheet 102: Elastomeric, semi-rigid moulded shapes

BS EN 62329-3-102 applies to heat-shrinkable moulded shapes based on elastomeric, semi-rigid materials. Elastomeric materials offer higher flexibility and elastic recovery, suitable for applications demanding vibration resistance, flexing or high sealing performance. The standard likewise specifies material requirements and system performance, with corresponding test methods and criteria.

3. Key Technical Requirements and Performance Criteria 🔍

Across the sheets, the technical essentials for heat-shrinkable moulded shapes can be summarised as:

  • Shrink characteristics: when heated to the specified temperature (shrink temperature), the moulding must shrink to predetermined dimensions while maintaining form; the standard specifies shrink ratio, shrink temperature and post-recovery dimensional stability.
  • Mechanical properties: tensile strength, elongation at break, hardness and flexibility; semi-rigid materials must retain sufficient rigidity while offering adequate resistance to mechanical damage.
  • Electrical insulation performance: dielectric strength, volume resistivity and related indicators must satisfy electrical insulation requirements, ensuring a reliable insulating barrier after shrinkage.
  • Flame retardancy and limited fire hazard: limited-fire-hazard materials must meet specified flame-retardant classification and low smoke/low toxicity characteristics, suitable for applications sensitive to fire safety such as railways and ships.
  • Environmental and chemical resistance: heat ageing, ozone, oil, solvent and weathering resistance must match the service environment.
  • System (compatibility) performance: after shrinkage the moulding forms a “system” with the protected component; interfacial sealing, adhesion and long-term reliability are key assessment points.
✅ The defining feature of the series is the dual requirement of “material requirements + system performance”: it assesses both the material properties of the moulding itself and the performance of the system formed after shrinkage over the protected object, closely reflecting real engineering application.

4. Test Methods and Conformity Assessment 🧪

Each sheet systematically defines test items, typically including:

  • Dimension measurement: measurement of dimensions and tolerances before and after shrinkage per Sheet 100.
  • Mechanical tests: tensile strength, elongation at break, hardness, compression set, etc.
  • Electrical tests: dielectric strength, volume resistivity, permittivity and dissipation factor.
  • Heat ageing and thermal tests: retention of properties after ageing at specified temperature and duration.
  • Flame retardancy tests: assessment of burning behaviour, smoke density and toxic gases for the limited-fire-hazard classification.
  • System compatibility tests: shrinkage of the moulding over the specified cable/joint, verifying sealing, adhesion, medium resistance and insulation.

Test results must be compared with the requirement values specified in the standard; the product is deemed to conform to the relevant sheet only when all requirements are met.

5. Engineering Practice and Application 🛠️

  • 🔍 Cable harness and bifurcation: breakout mouldings at cable bifurcations and terminal transitions provide insulation, sealing and strain relief.
  • 🔧 Connector boot protection: connector boot mouldings secure the cable and prevent bending damage and moisture ingress.
  • 📊 Railways and ships: limited-fire-hazard mouldings (Sheet 101) are used where fire protection and low smoke/toxic gas emission are required, such as trains and vessels.
  • 📋 Vibration and sealing applications: elastomeric mouldings (Sheet 102) suit equipment with high vibration and the need for elastic sealing.

6. Frequently Asked Questions ❓

❓ Q: How does BS EN 62329 differ from heat-shrink sleeving standards (e.g. BS EN 60684)?
A: BS EN 60684 addresses flexible insulating sleeving (continuous tubular forms), while BS EN 62329 addresses pre-formed mouldings (three-dimensional shapes such as breakouts, boots and cones). Materials and test methods overlap, but the product form and selection emphasis differ.
❓ Q: What is the relationship between Sheets 100, 101 and 102?
A: Sheet 100 provides the common dimensional system; Sheet 101 (polyolefin semi-rigid, limited fire hazard) and Sheet 102 (elastomeric semi-rigid) specify the detailed requirements of the two material families and their system performance. Select Sheet 101 or 102 by material family, then determine dimensions per Sheet 100.
❓ Q: What is “system performance” (compatibility performance)?
A: It refers to the performance of the whole formed after the moulding shrinks over the protected cable or joint — including interfacial sealing, adhesion, medium resistance and insulation reliability — which the standard requires to be verified by prescribed system tests.
🔍 Q: How do I choose between polyolefin and elastomeric mouldings?
A: Polyolefin mouldings (Sheet 101) are stiffer, flame retardant and economical for general electrical protection; elastomeric mouldings (Sheet 102) offer better flexibility and elastic recovery for vibration, flexing and high-sealing applications.
❓ Q: How is conformity with BS EN 62329 demonstrated?
A: Perform type tests per the test methods of the relevant sheet, compare results with the requirement values, and check the manufacturer’s dimensional, material and performance data sheets. For limited fire hazard, also confirm the flame-retardant and smoke/toxic classifications.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *