BS EN 62135 — Resistance Welding Equipment (Safety Requirements and Electromagnetic Compatibility)

UK implementation of IEC 62135 — Part 1: Safety Requirements for Design, Manufacture and Installation; Part 2: Electromagnetic Compatibility (EMC) Requirements

🔧 BS EN 62135 is the British Standard implementation of IEC 62135, maintained by BSI Technical Committee WEE/6 (Electric arc welding equipment). The technical content is identical to IEC 62135. The series specifies safety and electromagnetic compatibility requirements for resistance welding equipment (such as spot welding machines, seam welding machines and projection welding machines) and is a key standard for the design, manufacture, installation and use of such equipment. Resistance welding joins workpieces by passing a large current for a short time through the joint, generating resistive heat. The characteristic features are the very high secondary-circuit current (up to tens of kiloamperes), the pulsed DC or mains-frequency nature of the welding current, and significant switching transients and magnetic-field leakage, which makes safety and EMC requirements particularly important.

💡 The operating current of resistance welding equipment is far higher than that of ordinary industrial equipment. During welding, a strong magnetic field is produced around the secondary circuit and energy is released in narrow pulses. Without control, such equipment can affect power quality, nearby electronic equipment and operator health — which is exactly why IEC 62135 separates “safety” and “electromagnetic compatibility” into two independent parts.

1. Overview of the Standard Series 📌

The BS EN 62135 series is maintained by BSI Technical Committee WEE/6 (Electric arc welding equipment), with UK experts participating in the work of IEC TC 26 (Electric welding). The series comprises two parts: Part 1 (2015 edition) supersedes the 2008 edition and specifies safety requirements for the design, manufacture and installation of resistance welding equipment; Part 2 (2015 edition) supersedes the 2008 edition and specifies EMC requirements. Both parts are based on IEC 62135 and are adopted as European standards by CENELEC. As stated in the standard, compliance with a British Standard does not confer immunity from legal obligations, and users remain responsible for correct application.

Within the safety and EMC framework, resistance welding equipment must satisfy both the general machinery and electrical safety requirements and the specific clauses applicable to its particular mode of operation. Part 1 and Part 2 are used together: the former addresses personal and equipment safety, the latter addresses electromagnetic environmental compatibility.

2. Structure and Main Parts of the Series 🧩

The BS EN 62135 files covered by this article comprise two parts:

Standard numberYearTitleKey content
BS EN 62135-1:20152015Part 1: Safety requirements for design, manufacture and installationSafety requirements for design, manufacture and installation of resistance welding equipment, covering protection against electric shock, thermal and mechanical protection, welding circuit, control and interlocking, installation and use instructions
BS EN 62135-2:20152015Part 2: Electromagnetic compatibility (EMC) requirementsEmission and immunity requirements for resistance welding equipment, covering conducted and radiated emissions, harmonics, voltage fluctuations and flicker, and immunity tests

3. Key Technical Requirements 🔧

3.1 Part 1: Safety Requirements Highlights

  • Protection against electric shock: requirements are specified separately for the mains, control and welding circuits, using protective earthing, double insulation or safety extra-low voltage, to prevent operators from touching live parts.
  • Special nature of the welding circuit: the welding secondary circuit normally has a low voltage but a very high current. The standard requires strict rules on the connection and insulation of the welding gun, electrodes, cables and joints, to prevent overheating and shock caused by the large current.
  • Mechanical and thermal protection: requirements are placed on the clamping mechanism, guards and electrode cooling system to prevent crushing, burning and overheating, and measures are required against weld spatter.
  • Control and interlocking: requirements on start, stop, emergency stop, safety interlocks and two-hand operation ensure that the operator’s hands are clear of the danger zone before welding can take place.
  • Installation and use information: the manufacturer must provide installation, operating and maintenance instructions that define electrical connection, earthing, cooling water and gas supply requirements.

3.2 Part 2: EMC Requirements Highlights

Resistance welding equipment is a typical strong electromagnetic disturbance source, and its EMC requirements comprise both emission limits and immunity:

  • Conducted and radiated emission: limits the disturbance voltage and disturbance power emitted into the mains and into space, to avoid interference with nearby communication, measurement and control systems.
  • Harmonic currents: limits the harmonic current injected into the mains by the equipment (especially thyristor-controlled mains-frequency resistance welders), protecting power quality.
  • Voltage fluctuations and flicker: limits the voltage fluctuation and flicker caused by welding pulses, preventing lighting flicker and nuisance tripping of sensitive equipment.
  • Immunity: verifies stable operation of the equipment under electrostatic discharge, radio-frequency electromagnetic fields, electrical fast transients, surges and voltage dips.
⚠️ The “large-current, narrow-pulse” nature of resistance welding makes harmonic and flicker problems especially significant. When several welders are fed from the same supply circuit, harmonics add up and can readily exceed power-quality limits. The supply design should account for the synchronisation of welder operation, phase-control and power-factor correction.

4. Testing and Conformity Assessment 🧪

The safety tests of Part 1 include insulation resistance and dielectric withstand, protective-earthing continuity, temperature rise, mechanical strength, emergency-stop function and interlock tests. The EMC tests of Part 2 are carried out in accordance with the CISPR series and the IEC 61000 series, including disturbance voltage, disturbance power, harmonics, flicker and immunity tests. After completing type testing, the manufacturer places the product on the market through a self-declaration of conformity or third-party certification. It is important that the welder is tested in a representative operating state (for example, with representative welding parameters) and with the auxiliary devices specified by the standard, so that the test results are representative.

✅ In practice, earthing and shielding are often the key to solving EMC problems in resistance welding equipment: good protective earthing and cable screening significantly reduce conducted disturbance; adding filters to the control cabinet, shielding the secondary circuit and shortening wiring further suppress radiated emission.

5. Engineering Practice 🛠️

  • 🔍 Selection and reference: when purchasing resistance welding equipment, check the type-test reports and CE declarations of conformity to BS EN 62135-1 and BS EN 62135-2, and pay attention to rated capacity, duty cycle and cooling method.
  • 🔧 Supply design: select the transformer and cable cross-section according to the rated capacity, duty cycle and diversity factor; fit appropriate overcurrent and short-circuit protection; and where necessary add reactive-power compensation and filtering.
  • 📊 Site installation and acceptance: after installation, verify earthing continuity, protective-device operation, cooling system and interlock functions, and carry out trial welds to confirm weld quality.
  • 📋 Maintenance and monitoring: periodically check electrode wear, cooling-water flow and cable insulation, and monitor harmonics and voltage fluctuation to prevent deterioration of EMC and power quality.

6. Frequently Asked Questions ❓

❓ Q: Does resistance welding equipment only need to satisfy the safety requirements of Part 1?
A: No. Part 1 addresses personal and equipment safety, while Part 2 addresses electromagnetic compatibility; together they form a complete basis for conformity assessment. Without EMC conformity, the product cannot satisfy the EMC Directive on the European market.
❓ Q: Why are harmonic problems especially prominent in resistance welding equipment?
A: Resistance welding uses thyristors or inverters to control the current, so the welding current is a pulsed waveform rich in harmonics; because the welding time is short and the duty cycle is low, voltage fluctuation and flicker are also pronounced. When several welders share one supply, the harmonics add up and require particular attention.
❓ Q: How does BS EN 62135 relate to general machinery safety standards such as EN 60204-1?
A: BS EN 62135 is the specific standard for resistance welding equipment and adds the special requirements of the welding circuit on top of general machinery electrical safety (for example EN 60204-1). Compliance with BS EN 62135 is normally regarded as satisfying the corresponding general safety requirements, but the whole risk assessment and Machinery Directive aspects should still be considered.
🔍 Q: What is the effect of duty cycle on selection?
A: Resistance welding machines work at high current for short periods, and their rated capacity is normally given at a certain duty cycle. During selection, check the temperature rise and transformer capacity against the actual welding cycle and load duration, to avoid long-term overload causing overheating and insulation ageing.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *