🔬 BS EN 62047 is the British Standards Institution (BSI) adoption of the International Electrotechnical Commission standard IEC 62047 (Semiconductor devices — Micro-electromechanical devices) as the European standard EN 62047 (via CENELEC). The series defines the terminology, test methods, mechanical and material characterisation means for Micro-Electro-Mechanical Systems (MEMS) devices, providing a unified technical language for the design verification, material screening and reliability assessment of MEMS accelerometers, gyroscopes, pressure sensors, micromirrors, RF switches and similar devices. It is maintained by BSI Technical Committee EPL/47 (Semiconductors) and classified under ICS 31.080.99 (other semiconductor devices).
MEMS devices integrate mechanical structures with electronic circuits on silicon substrates or thin films, and their performance heavily depends on thin-film mechanics, residual stress, thermal expansion behaviour and fatigue life. The IEC 62047 family uses Part 1 (Terms and definitions) to unify the basic concepts of the MEMS field, then defines “micro-scale mechanical tests” and “material characterisation methods” in individual parts: micro-pillar compression (Part 10) for compressive/yield behaviour of thin films, coefficient of linear thermal expansion (Part 11) for temperature stability, and cantilever/film bending and fatigue tests for long-term reliability. These methods are designed specifically for specimens at the micro-to-sub-millimetre scale and cannot directly use macroscopic material test standards.
| Part / Document | Main Content | Topic |
|---|---|---|
| BS EN 62047-1 (2016) | Terms and definitions | Unified MEMS terminology system |
| BS EN 62047-5 (2011) | Mechanical tests on thin-film materials | Tensile/compressive mechanical properties of thin films |
| BS EN 62047-7 / 8 / 9 (2011) | Beam and film bending tests | Cantilever deflection, Young’s modulus, residual stress |
| BS EN 62047-10 (2011) | Micro-pillar compression test | Compression strength and stress-strain of sub-micro/micro columns |
| BS EN 62047-11 (2013) | CTE of free-standing materials | Thermal stability and thermal matching design |
| BS EN 62047-12~14 (2011–2012) | Fatigue and adhesion tests | Microstructure fatigue life, static friction, stiction |
| BS EN 62047-15~17 (2015) | Impact / vibration / acceleration tests | Shock resistance, vibration, dynamic reliability |
| BS EN 62047-18~22 (2013–2014) | Device characteristics & process tests | Film stress gradient, electro-thermal actuation, process characterisation |
| BS EN 62047-25 / 26 (2016) | Electrochemical / functional tests | Functional verification of MEMS actuators and sensors |
A micron-scale cylinder (micro-pillar) fabricated on a thin-film or bulk-silicon material is loaded with a nanoindenter / micro-compression rig to obtain the compressive strength, plastic deformation and fracture characteristics of the material at micro scale, used to validate process materials (e.g. polysilicon, silicon nitride, metal films).
For free-standing (substrate-unconstrained) MEMS thin-film materials, the linear expansion coefficient is determined through controlled heating and deformation measurement, providing a basis for thermal matching and temperature-drift compensation in bimorph structures.