BS EN 62044 — Cores Made of Soft Magnetic Materials Measuring Methods Standard Series (General, Low and High Excitation Magnetic Properties)

Cores Made of Soft Magnetic Materials — Measuring Methods: General, Magnetic Properties at Low Excitation and at High Excitation

🧲 BS EN 62044 is the British Standard (BSI) series adopting the IEC 62044 family for the measuring methods of soft magnetic material cores, providing unified test methods for magnetic properties of ferrite and iron-powder cores. The series comprises 62044-1 (Generic specification), 62044-2 (Magnetic properties at low excitation) and 62044-3 (Magnetic properties at high excitation level), developed under BSI Technical Committee EPL/51 (Transformers, inductors, magnetic components and ferrite materials). Cores are widely used in switch-mode power supplies, transformers, inductors and filters; permeability and loss directly determine component performance.

💡 The core is the “magnetic heart” of the magnetic path of inductors and transformers: measuring permeability and loss uniformly per BS EN 62044 ensures comparable performance and consistent quality across manufacturers.

1. Series Structure and Scope 📌

StandardTitleCore Content
BS EN 62044-1Generic specificationGeneral requirements for core measurement, including measurement environment, terminology, test coils and windings, measuring systems and data handling.
BS EN 62044-2Magnetic properties at low excitationMethods for measuring magnetic properties such as permeability and loss at low excitation.
BS EN 62044-3Magnetic properties at high excitation levelMethods for measuring core magnetic properties at high excitation (power application range).
⚠️ Part 1 is the generic base; Parts 2 and 3 give specific methods for low- and high-excitation applications. Choose the appropriate part for the application.

2. Basic Concepts of Core Magnetic Properties 🔧

Key magnetic properties of soft magnetic materials include:

  • Permeability (μ): the ratio of flux density B to magnetic field strength H, reflecting the material’s magnetising ability, including initial, effective and amplitude permeability.
  • Core loss: the power dissipated during alternating magnetisation, comprising hysteresis loss, eddy-current loss and residual loss.
  • Flux density (B): magnetic flux per unit area; cores must avoid saturation in use.
  • Quality factor (Q): the ratio of reactance to resistance, reflecting the loss characteristics of an inductive component.
✅ The distinction between low- and high-excitation properties is important: small-signal (low excitation) applications focus on permeability and Q, while power applications (high excitation) focus more on loss and saturation.

3. Low-Excitation Magnetic Property Measurement (62044-2) 🔬

Part 2 specifies methods for measuring core magnetic properties under low excitation, typically using an LCR meter or impedance analyser to measure coil inductance and loss, computing effective permeability and quality factor. Suited to small-signal inductors, filters and resonant-circuit cores.

💡 Low-excitation measurement is “small-signal” characterisation: within the low-excitation range where permeability is approximately constant with field, measured inductance and Q can be used directly in inductor design.

4. High-Excitation Magnetic Property Measurement (62044-3) ⚡

Part 3 specifies methods for measuring core magnetic properties at high excitation levels (power application range), measuring core loss and magnetisation characteristics at larger flux densities. It applies to cores in switch-mode power-supply transformers, chokes and power inductors. Measurement typically uses power measurement, oscilloscope methods or automatic magnetisation-curve test systems, yielding core-loss versus flux-density relationships and hysteresis loops.

🚨 High-excitation measurement must consider heat dissipation and temperature rise: at higher flux densities loss increases and temperature rises, potentially changing material properties; control excitation level and measurement duration.

5. Engineering Practice Essentials 🛠️

  • 🔍 Selection: choose core material and size by operating frequency, flux density and loss requirements.
  • 🔧 Winding design: compute turns and inductance from measured effective permeability and magnetic-path dimensions.
  • 📊 Loss control: power applications must account for core loss and temperature rise; select low-loss materials and optimise flux density.
  • 📋 Quality control: incoming inspection measures permeability and loss per the standard to ensure batch and product consistency.

6. Frequently Asked Questions ❓

❓ Q: Why distinguish low- and high-excitation measurement?
A: Low excitation suits small-signal applications (permeability, Q); high excitation suits power applications (loss, saturation). They address different magnetic properties and use cases.
❓ Q: What is the difference between effective and initial permeability?
A: Initial permeability is the material permeability in the zero-field limit; effective permeability is the overall equivalent permeability of the magnetic path considering core geometry and air gap, used in practical design.
❓ Q: What components make up core loss?
A: Hysteresis, eddy-current and residual loss. At high frequency, eddy-current and residual loss grow; material selection and structure design must consider all.
🔍 Q: Why does permeability measurement need standard windings?
A: To ensure comparable results, the standard specifies uniform test coils, turns and conditions, avoiding measurement deviation from winding differences.
❓ Q: What does the standard require of the measurement environment?
A: Specifies conditions such as ambient temperature, humidity and measurement frequency; cores should be environmentally preconditioned before measurement for accurate, repeatable results.
🔒