🛡️ BS EN 61331 is the British Standard (BSI) adoption of the IEC 61331 series covering protective devices against diagnostic medical X-radiation, prepared under Subcommittee CH/62/2 (Diagnostic imaging equipment) of Technical Committee CH/62 (Electrical equipment in medical practice). X-ray diagnosis (fluoroscopy, radiography, CT, interventional procedures) is indispensable in disease diagnosis and treatment, but the ionizing radiation exposure of patients and medical staff must be kept as low as reasonably achievable. The series specifies methods for determining the attenuation properties of diagnostic X-ray protective materials, as well as performance requirements for translucent protective plates, protective clothing and other protective devices — an important basis for radiation protection design in medical institutions and for procurement and acceptance of protective equipment.
The BS EN 61331 series consists of three parts: Part 1 specifies the determination of attenuation properties of materials, the metrological basis of the series; Part 2 specifies requirements for translucent protective plates; Part 3 specifies requirements for protective clothing, protective devices and accessories. The three parts cover the full chain from material performance measurement to finished protective-device inspection. The 2014 series supersedes the 2002 editions and updates the attenuation determination methods and protection requirements.
| Standard | Title | Principal Technical Content | Status |
|---|---|---|---|
| BS EN 61331-1:2014 | Protective devices against diagnostic medical X-radiation — Part 1: Determination of attenuation properties of materials | Determination of the X-ray attenuation performance (e.g., lead equivalence) of protective materials | Supersedes 2002 edition |
| BS EN 61331-2:2014 | Part 2: Translucent protective plates | Attenuation, optical, mechanical and durability performance requirements for translucent X-ray protective plates | Supersedes 2002 edition |
| BS EN 61331-3:2014 | Part 3: Protective clothing, protective devices and accessories | Performance requirements and test methods for protective clothing (e.g., lead aprons), protective devices and accessories | Supersedes 2002 edition |
BS EN 61331-1:2014 specifies methods for determining the attenuation properties of diagnostic X-ray protective materials. The core performance of a protective material is its attenuation capability, typically expressed as “lead equivalence” — the thickness of lead that produces the same attenuation of the radiation beam under specified X-ray quality (tube voltage and filtration). The part specifies standardized X-ray conditions (tube voltage, total filtration, geometrical arrangement), measurement apparatus and attenuation calculation methods, ensuring that attenuation data for different materials and different laboratories are comparable. The 2014 edition updates the radiation conditions and measurement details to better match modern X-ray equipment.
BS EN 61331-2:2014 specifies requirements for translucent protective plates. Translucent plates are used where visibility must be maintained while providing protection in X-ray examination rooms (e.g., observation windows, protective screens), typically made of lead glass or transparent lead-containing organic materials. The part specifies attenuation performance (lead equivalence), optical performance (transmittance, clarity), mechanical strength, dimensions and marking, together with corresponding test methods. The 2014 edition is the second edition of IEC 61331-2, updating test methods and requirements.
BS EN 61331-3:2014 specifies requirements for protective clothing, protective devices and accessories (such as lead aprons, thyroid collars, protective eyewear and gonad protection). Part 3 specifies the attenuation performance (lead equivalence), coverage area, dimensions and wearing comfort, marking and instructions, cleaning and maintenance requirements, and test methods for these personal protective devices. The 2014 edition is the second edition of IEC 61331-3, updating the regional-protection requirements and test methods for protective clothing, balancing protection effectiveness with ease of use.