☀️ BS EN 61215 is the British Standard (BSI) adoption of the IEC 61215 series covering design qualification and type approval of terrestrial photovoltaic (PV) modules, prepared by Technical Committee GEL/82 (Photovoltaic Energy Systems). PV modules convert sunlight into electricity and are the core generating units of PV power plants; their long-term reliability directly determines plant generation performance and investment return. Design qualification and type approval is the process of verifying, through a series of standardized accelerated-ageing and environmental tests, whether a module design can operate reliably outdoors over the long term — the key basis for a module entering the market, gaining certification and obtaining financing endorsement.
💡 Design qualification of a PV module is not a one-time pass certificate: it verifies the long-term reliability of “that design” (not “that batch of products”) under typical outdoor conditions. Passing qualification means the design has the technical basis to enter the market; actual supply still requires production-conformity control.
1. Series Overview and Structure 📌
The BS EN 61215 series consists of three parts: Part 1 specifies test requirements — the common test framework of the series; Part 1-1 specifies special test requirements for crystalline silicon modules; Part 2 specifies the detailed test procedures. The series partially supersedes the 2005 edition of BS EN 61215 and is subdivided by module technology type (crystalline silicon, thin film, etc.) to suit the characteristics of different cell technologies. Together with parts such as BS EN 61215-1-2, -1-3 and -1-4 (thin-film and other technologies), the series forms a complete PV module qualification system.
| Standard | Title | Principal Technical Content | Status |
| BS EN 61215-1:2016 | Terrestrial photovoltaic (PV) modules — Design qualification and type approval — Part 1: Test requirements | General test requirements, test sequence and acceptance criteria for module design qualification | Partially supersedes 2005 edition |
| BS EN 61215-1-1:2016 | Part 1-1: Special requirements for testing of crystalline silicon photovoltaic (PV) modules | Special requirements for test items, quantities and sequence for crystalline silicon modules | Partially supersedes 2005 edition |
| BS EN 61215-2:2017 | Part 2: Test procedures | Detailed test procedures and methods for each accelerated-ageing and environmental test | First edition 2017 |
⚠️ The standards do not purport to include all necessary provisions of a contract; users are responsible for correct application, and compliance with a British Standard does not of itself confer immunity from legal obligations. Additional evaluation for special climates (high temperature, high humidity, salt mist, high wind, hail) should be considered in the actual installation environment.
2. Part 1: Test Requirements 🧪
BS EN 61215-1:2016 specifies the general test requirements for design qualification of terrestrial PV modules, including number of test samples, test sequence, acceptance criteria and reporting requirements. The part establishes the overall framework of module qualification testing and defines the order and sample-allocation principles between the various tests (thermal cycling, damp heat, humidity freeze, UV preconditioning, mechanical load, etc.). Acceptance criteria are typically expressed by power degradation, visual defects, insulation performance and safety. Part 1 is used together with the technology-specific special requirements (such as Part 1-1) and the test procedures of Part 2.
💡 Test sequence design is the core logic of qualification: different environmental stresses interact and shadow one another, and the sequence affects the final result. The test sequence in Part 1 aims to simulate, with a limited set of samples, the cumulative stress a module experiences outdoors, thereby exposing design defects efficiently.
3. Part 1-1: Special Requirements for Crystalline Silicon Modules 🔬
BS EN 61215-1-1:2016 specifies special test requirements for crystalline silicon PV modules. Crystalline silicon modules are the mainstream technology; their cells are sensitive to temperature, humidity, mechanical stress and UV radiation. The standard defines specific test items, required sample quantities and test sequence for such modules. Building on the Part 1 general framework, it details the qualification test configuration for crystalline silicon modules so that results represent the true reliability of the technology. It corresponds to Parts 1-2, 1-3, etc. for other cell technologies (film types).
⚠️ Different cell technologies fail by different mechanisms: crystalline silicon modules are sensitive to micro-cracks, soldering failures and hot spots, while thin-film modules are more sensitive to moisture ingress and light-induced degradation. Parts such as “1-1” must therefore be selected according to the actual technology — crystalline silicon tests cannot substitute for thin-film module qualification.
4. Part 2: Test Procedures 🛠️
BS EN 61215-2:2017 specifies the test procedures required for module qualification, including detailed methods, conditions, sample arrangement and judgment for thermal cycling, damp heat (85/85), humidity freeze, UV preconditioning, mechanical load, hail impact, bypass-diode thermal performance, insulation and dielectric strength, and ground continuity tests. The part converts the test requirements into executable standard operations and is the direct basis for laboratories conducting module qualification. The 2017 edition is the first edition of IEC 61215-2, separating and systematizing the test procedures from the 2005 edition of BS EN 61215.
✅ Standardized test procedures guarantee repeatability and comparability: only when different laboratories execute the same procedures are the results comparable and acceptable. This is also the basis for global mutual recognition of module qualification certificates and financing acceptance.
5. Engineering Practice Essentials 🛠️
- 🔍 Selection and certification: choose modules with a valid design-qualification certificate (e.g., IEC 61215 certification) from an accredited body; check that the certificate covers the module model and technology type.
- 🔧 Incoming inspection and consistency: perform receipt sampling per production-conformity requirements; verify power class, appearance, marking and safety performance to prevent substandard goods.
- 📊 Installation and O&M: install per design loads and mounting methods to avoid micro-cracks; monitor power degradation, hot spots and insulation anomalies in O&M to detect early degradation.
- 📋 Special climate evaluation: in special environments (high temperature, high humidity, salt mist, high wind/sand), supplement qualification and selection per relevant additional standards or risk assessment.
6. Frequently Asked Questions ❓
❓ Q: What is the difference between BS EN 61215-1 and BS EN 61215-2?
A: Part 1 specifies test requirements (which tests, sample quantities, sequence and criteria); Part 2 specifies test procedures (how each test is executed in detail). They are used together: Part 1 answers “what to test and how to judge”, Part 2 answers “how to do it”.
❓ Q: Does passing design qualification mean the module is permanently reliable?
A: No. Design qualification confirms the long-term reliability of a specific design under standard tests — a “design-level” confirmation. Actual products are still affected by production-process consistency, raw-material variation and field environment; batch quality must be ensured through production-conformity inspection and field monitoring.
❓ Q: Are qualification tests for crystalline silicon and thin-film modules identical?
A: Not entirely. Both share the Part 1 common test requirements, but each follows the specific requirements of Parts 1-1, 1-2, 1-3, etc. to determine the exact test configuration, because their failure mechanisms and sensitive stresses differ. When selecting, verify the technology type covered by the certificate.
🔍 Q: Why is the damp heat (85/85) test important?
A: The damp heat test (85°C / 85% RH) simulates module ageing in high-temperature, high-humidity environments, mainly testing the moisture resistance and corrosion resistance of the encapsulation, backsheet and edge seals. It exposes failure modes such as moisture ingress, delamination and electrical performance decay — one of the key tests for assessing long-term module reliability.