Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
📐 BS EN 61212 is the UK adoption of the IEC 61212 series, specifying industrial rigid round laminated tubes and rods based on thermosetting resins for electrical purposes. This batch covers two sheets of Part 3 “Specifications for individual materials”: Sheet 1 for round laminated rolled tubes and Sheet 2 for round laminated moulded tubes. Such materials are widely used as structural supports, insulating bushings and winding formers in motors, transformers, switchgear and capacitors.
| Standard | Sheet | Subject | Adoption |
|---|---|---|---|
| BS EN 61212-3-1:2013 | Sheet 1 | Rolled laminated tubes | Identical to IEC 61212-3-1:2013, replaces 2006 ed. |
| BS EN 61212-3-2:2013 | Sheet 2 | Moulded laminated tubes | Identical to IEC 61212-3-2:2013, replaces 2006 ed. |
Part 3 is the “Specifications for individual materials”; each sheet specifies one particular laminated tube material’s composition, performance requirements and test methods. It sits on top of Part 1 (definitions and general requirements) and Part 2 (test methods), giving material grades comparable electrical, thermal and mechanical data.
Laminated tubes are classified by reinforcement and resin system. Typical combinations include paper/phenolic (balanced mechanical and electrical), cotton fabric/phenolic (high mechanical strength) and glass fabric/epoxy (high electrical and thermal performance). The standard sets resin content, density, flexural strength, axial and radial electric strength, insulation resistance, water absorption and thermal class for each type.
| Property | Meaning | Design focus |
|---|---|---|
| Flexural strength | Resistance to deformation | Structural support selection |
| Axial/radial electric strength | Breakdown capability | Determines bushing voltage rating |
| Insulation/volume resistivity | Long-term insulation stability | Critical in humid environments |
| Water absorption | Moisture resistance | Outdoor and humid duty |
| Thermal class | Continuous operating temperature | Matches motor/transformer rise |
BS EN 61212 sits with BS EN 60216 (thermal endurance of electrical insulating materials), BS EN 60464 (varnishes), BS EN 60505 (insulation system evaluation) and BS EN 60664 (insulation coordination) in the electrical insulation specification system. As structural-and-insulating components, laminated tubes rely on the combined effect of thermal class, ambient humidity and electrical stress. Selection should jointly weigh electric strength, mechanical strength and thermal class against equipment temperature rise and partial-discharge risk.
In practice laminated tubes are used for motor slot wedges, transformer lead insulation, switchgear insulating rods and capacitor housings. Over long operation they may degrade by moisture absorption, thermal ageing and electrical ageing. Recommend sampling flexural strength, electric strength and water absorption at incoming inspection, then measure insulation resistance and dissipation factor at overhaul intervals, building a “grade — service time — performance” archive to support condition-based maintenance.
| Application | Key property | Failure mode |
|---|---|---|
| Motor slot wedge | Mechanical strength, thermal | Thermal ageing, vibration fatigue |
| Transformer lead | Electric strength, water absorption | Moisture creepage |
| Insulating rod | Flexural, radial withstand | Mechanical fracture |
| Capacitor housing | Dielectric, thermal | Electrical ageing |
In summary, the selection and maintenance of laminated-tube insulation must balance electrical, mechanical and thermal performance, combining the BS EN 61212 material specification with equipment duty and maintenance strategy to achieve both safety and economy.