🔬 BS EN 61189 is the British Standard implementing the EN 61189 series, corresponding to IEC 61189, covering test methods for electrical materials, printed boards and other interconnection structures and assemblies. It is developed within IEC/TC 91 (Electronics assembly technology), with the UK represented by EPL/501. The value of the family is that it turns materials-to-process-to-performance questions in PCB manufacturing and electronic assembly into standardised, repeatable tests: from the melting temperature of solder alloys, to the relative permittivity and loss tangent of base materials at high frequency, to the general test procedures for interconnection structures. The eight documents in this batch span editions from 2013 to 2016.
BS EN 61189 uses a “part plus numbered method” structure: topics are assigned to part numbers (Part 2 for interconnection-structure materials, Part 3 for printed boards, Part 5 for assemblies), and each test method carries an additional identifier (for example -719 or -721). The eight files in this batch span several parts and reflect a multi-level test demand from material level, through board level, to assembly level.
| Standard | Year | Core subject | Object |
|---|---|---|---|
| BS EN 61189-11 | 2013 | Measurement of melting temperature or melting temperature ranges of solder alloys | DTA/DSC thermal analysis of lead-free and leaded solders |
| BS EN 61189-2-719 | 2016 | Relative permittivity and loss tangent of materials for interconnection structures (500 MHz to 10 GHz) | High-frequency dielectric characterisation |
| BS EN 61189-2-721 | 2015 | Measurement of permittivity and loss of copper-clad laminate at microwave frequencies using a split-post dielectric resonator (SPDR) | Non-destructive measurement of CCL |
| BS EN 61189-3-719 | 2016 | Test methods for printed boards (interconnection structures) | PCB structural and performance testing |
| BS EN 61189-5-1 | 2016 | General methods for assemblies (1) | Soldered assemblies and placement quality |
| BS EN 61189-5-2 | 2015 | General methods for assemblies (2) | Solder joint reliability related tests |
| BS EN 61189-5-3 | 2015 | General methods for assemblies (3) | Cleanliness, solderability and others |
| BS EN 61189-5-4 | 2015 | General methods for assemblies (4) | Stress and environmental tests |
The melting temperature of a solder alloy determines the setting of the reflow oven profile. Part 11 prescribes thermal analysis (differential thermal analysis DTA or differential scanning calorimetry DSC) to determine the melting temperature or melting temperature range of the alloy. A eutectic alloy yields a single melting peak, while a non-eutectic system gives the temperature interval between the solidus and the liquidus, providing the basis for setting the process window.
Part 2-719 covers the measurement of relative permittivity and loss tangent from 500 MHz to 10 GHz for interconnection structure materials; Part 2-721 addresses copper-clad laminates, using a split-post dielectric resonator (SPDR) for non-destructive measurement at microwave frequencies. Both methods stress sample flatness, thickness and copper treatment, because the accuracy of Dk/Df measurement depends strongly on geometry and boundary conditions.
The Part 5 sub-documents address assembled electronic assemblies: soldering quality inspection, solder-joint reliability, solderability, cleanliness and stress tests. Unlike material-level tests, assembly-level tests focus on the combined result of the process chain, and test samples are usually taken from production to represent the real manufacturing state.