BS EN 60811 — Electric and Optical Fibre Cables Insulating and Sheathing Materials Test Methods Standard Series

Electric and optical fibre cables — Insulating and sheathing materials test methods (equivalent to IEC 60811, 46 documents)

🔌 This article is a scanned-version write-up based on public-domain knowledge. BS EN 60811 is the UK-implemented series of test methods for insulating and sheathing materials of electric and optical fibre cables, adopted by BSI from the restructured IEC 60811 and maintained by Technical Committee GEL/20 (Electric cables, Subcommittee GEL/20/17, Low voltage), classified under ICS 29.035.01 and 29.060.20. This batch contains 46 documents, using the 2012-restructured numbering: -100 general (-1-1/-1-2 legacy general application with thermal ageing), -200 pre/post-ageing elastomer properties, -300 thermal/irradiation ageing of thermoplastic and XLPE, -400 polyethylene (PE) materials, -500 polyvinyl chloride (PVC) materials, plus specialised methods such as heat shrink, hot set and thermal deformation. It is the foundation of quality control for insulation and sheathing materials of wires and cables (low- and medium-voltage power cables and optical cables), used with harmonised product standards such as BS EN 50525.

💡 After the 2012 restructuring, 60811 numbers parts by “material family × test type”: -100 general rules, -2xx general elastomers, -3xx thermoplastic/XLPE, -4xx polyethylene, -5xx PVC. Determine the material type first, then select the corresponding test part.

1. Overview and Scope 📌

BS EN 60811-100:2012 is the series general rules, identical to IEC 60811-100:2012, and governs the replacement of the legacy -1-1/-1-2/-1-3/-1-4 (general application and thermal ageing methods). The material shows -1-1/-1-2:1995 were the early general application (including thermal ageing), -2-1:1998 general tests (tensile and elongation), -4-1/-4-2:2004 polyethylene-specific methods, and -5-1:2000 PVC methods. The new structure rewrites them as -100/-200/-300/-400/-500/-600 families, where -200/-201/-202/-203 are elastomer pre/post-ageing properties, -301/-302 thermoplastic ageing, -401 to -412 PE-specific, -501 to -513 PVC-specific, and -601 to -607 others (heat shrink, oil immersion etc.).

The scope covers testing and assessment of insulation and sheathing materials of low- and medium-voltage power cables, wires and optical cables; the results are combined with harmonised standards such as BS EN 50525 (low-voltage cables) and BS EN 60228 (conductors) for product conformance.

⚠️ Specimen condition (sampling direction, dumbbell die, ageing temperature and time) must be strictly consistent. Different materials (PVC/PE/elastomer) map to different parts; wrong method selection invalidates the tensile/elongation judgement.

2. Series Composition and Technical Points 🔧

The table below lists principal parts of the series (based on the real file list in the material, covering the legacy -1-1/-1-2/-1-3/-1-4/-2-1/-3-1/-3-2/-4-1/-4-2/-5-1 and the new -100 to -607).

StandardSubjectEditionRemark
BS EN 60811-100General rules2012New-structure general
BS EN 60811-200/-201/-202/-203Elastomer: pre/post-ageing general2012Tensile, elongation, ageing
BS EN 60811-301/-302Thermoplastic/XLPE: post-ageing2012Thermal ageing
BS EN 60811-401 … -412Polyethylene (PE) specific2012PE-related tests
BS EN 60811-501 … -513PVC specific2012Hot deformation, oil etc.
BS EN 60811-601 … -607Other specific2012Heat shrink, oil etc.
BS EN 60811-1-1 / -1-2Legacy general application / ageing1995Replaced by -100
BS EN 60811-2-1Legacy general tests1998Replaced by -2xx
BS EN 60811-4-1 / -4-2Legacy PE methods2004Replaced by -4xx
BS EN 60811-5-1Legacy PVC method2000Replaced by -5xx

The file list shows the 2012 edition restructured the 1995–2004 legacy (-1-x/-2-x/-3-x/-4-x/-5-x) into the -100 to -607 new structure; the new system groups by material family, making it easier to reference from cable product standards. Legacy -2-1:1998 is explicitly marked “scan” in the list, indicating its scanned origin.

💡 In practice, “tensile strength + elongation at break + retention after ageing” is the most basic pass/fail combination for insulation/sheathing; hot set (XLPE) and heat shrink verify cross-linking degree and dimensional stability for medium-voltage cables.

3. Key Technical Requirements 🔥

Key technical elements and indicators of the cable-material test series include:

  • Tensile strength and elongation: -2xx specifies tensile strength and elongation before/after ageing and specimen preparation.
  • Thermal ageing: -201/-202/-301/-302 determine retention after ageing at specified temperature and time, assessing thermal life.
  • Hot set (cross-linked): elongation and permanent set under high-temperature load verify XLPE cross-linking degree.
  • Hot deformation and heat shrink: -5xx/-601 verify dimensional stability of PVC and PE.
  • Oil immersion/environment: -501/-601 etc. assess resistance in oil-contaminated environments.
  • Low-temperature tests: low-temperature bending and impact (some parts) verify flexibility in cold environments.
  • Mass loss: mass loss at high temperature, indirectly assessing thermal stability.
🚨 The dumbbell specimen cutting and oven-temperature uniformity directly decide result reliability. The ageing oven must be calibrated periodically; specimens must be heated uniformly at the centre of the specified zone to avoid local overheating and data distortion.

4. Engineering Application 🛠️

  • 🔍 Type testing: per the BS EN 50525 etc. product-standard requirements, select the corresponding -2xx/-4xx/-5xx parts to complete pre/post-ageing properties.
  • 📋 Incoming and process control: sample insulation and sheathing compounds for tensile/elongation and ageing retention to control batch consistency.
  • 🔧 Cross-link verification: medium-voltage XLPE cables use hot set to verify cross-linking, preventing under-cure thermal deformation and electrical failure.
  • ♻️ Version transition: the -100 etc. 2012 edition supersedes the legacy (-1-x/-2-x …); companies should update test procedures and product-standard references.
✅ A “material type — test part — pass limit” mapping table, run with calibrated ageing ovens, guarantees international comparability and compliance efficiency of cable-material tests.

5. Frequently Asked Questions ❓

❓ How do the new and legacy BS EN 60811 numbers correspond?
Answer: After the 2012 restructuring, legacy -1-1/-1-2 (general application and thermal ageing) are replaced by -100/-200/-201 etc.; -2-1 (general tests) merges into -2xx; -4-x (PE) and -5-x (PVC) are replaced by -4xx and -5xx respectively.
❓ Which material is the hot-set test for?
Answer: Mainly for cross-linked materials such as XLPE; elongation and permanent set under high-temperature load determine whether the cross-linking degree is sufficient.
❓ How are specific conditions confirmed given the “scan” files?
Answer: Most of the 46 documents are scan-based. This article is based on the machine-readable forewords (-100/-1-1/-1-2) and public-domain knowledge of IEC 60811; specific temperatures, times and limits should be taken from the official BSI version.
❓ Are BS EN 60811 and IEC 60811 the same?
Answer: Technically identical; BS EN 60811 is the UK national adoption of IEC 60811, and the BS EN designation governs in the UK market.
🔒