Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
🔥 BS EN 60754 is the British Standards Institution series adopting European Standard EN 60754, identical to IEC 60754, which specifies test methods for gases evolved during combustion of materials from cables (including insulation and sheath). The series characterises the toxic/acidic gas release of halogen-containing cable materials under fire conditions. Part 1 covers the determination of the halogen acid gas content; Part 2 covers the determination of acidity (by pH measurement) and conductivity. The series was prepared by Technical Committee GEL/20/18, Electric Cables — Fire testing, and together with BS EN 60754-1/-2 supersedes the earlier BS EN 50267 series.
The BS EN 60754 series is identical to IEC 60754, prepared by IEC/TC 20 “Electric cables”, and was adopted in the UK by Subcommittee GEL/20/18, Electric Cables — Fire testing, of Technical Committee GEL/20. The 2014 editions of Part 1 (including the IEC corrigendum of November 2013) and Part 2 jointly supersede BS EN 50267-1, 50267-2-1, 50267-2-2 and 50267-2-3 (1999 editions). The series specifies the apparatus, methods and result expression for sampling and determining gases produced from cable material samples (insulation, sheath, filler) under controlled combustion, for assessing the acidic and corrosive gas release characteristics of materials in fire.
| Standard Number | Title | IEC Reference | Main Content |
|---|---|---|---|
| BS EN 60754-1:2014 | Test on gases evolved during combustion of materials from cables — Part 1: Determination of the halogen acid gas content | IEC 60754-1:2011 + corrigendum Nov. 2013 | Collect combustion gases in an absorption solution and determine hydrogen halide (acid gas) content |
| BS EN 60754-2:2014 | Test on gases evolved during combustion of materials from cables — Part 2: Determination of acidity (by pH measurement) and conductivity | IEC 60754-2:2011 | Absorb combustion gases in water and determine the pH and conductivity of the solution |
Part 1 specifies the method for determining halogen acid gas content: a sample of cable material of known mass is combusted in a tube furnace at a specified temperature (e.g. 800 ℃), the evolved gases are collected in an absorption solution (such as water or alkali), and the halide ions (mainly chlorine, bromine, fluorine) are determined by chemical analysis (e.g. titration or ion-selective electrode), expressed as a percentage of the sample mass. This method assesses the halogen level of the material and is the basis for halogen-free judgement and limit compliance.
Part 2 specifies the method for determining acidity and conductivity: the combustion gases are led into deionised water for absorption, and the pH and conductivity of the solution are measured. pH reflects the acidity of the solution (the more acidic, the lower the pH), while conductivity reflects the total ion content. These two parameters assess the corrosivity of the combustion gases to the environment and are important indices for evaluating low-acidity cable materials.
| Test Item | Measured Parameter | Test Points | Evaluation Significance |
|---|---|---|---|
| Halogen acid gas content | Halide ion mass percentage | Tube furnace combustion, absorption collection, chemical analysis | Halogen level and halogen-free judgement basis |
| Acidity determination | Absorption solution pH | Absorb combustion gases in water, measure pH | Degree of gas acidity/corrosivity |
| Conductivity determination | Absorption solution conductivity | Absorb combustion gases in water, measure conductivity | Total ion content in the solution |
The series specifies the requirements for the tube furnace, combustion tube, absorption bottles, gas-flow control and connecting tubing, and specifies the sample preparation, combustion temperature, gas flow and absorption solution as test conditions, together with the method for calculating and expressing results. Tests should be performed in repeat conditions and reported in a specified manner to ensure comparability between laboratories.