🔬 The BS EN 60749 series is the UK implementation by BSI of IEC 60749, defining mechanical and climatic test methods for semiconductor devices — the core standard family for reliability evaluation of chips, discrete devices and integrated-circuit packages. It was prepared under the responsibility of UK Technical Committee EPL/47 (Semiconductors), classified under ICS 31.080.01. Each part is identical to the corresponding IEC 60749 document, so it is technically aligned with the international standard. The series comprises 13 parts covering a complete reliability and quality-verification matrix: resistance to soldering temperature, die shear strength, moisture sensitivity of surface-mount devices, high-temperature storage, temperature cycling, solderability and constant acceleration, among others.
During manufacturing, packaging, assembly and service, semiconductor devices are subjected to soldering heat, mechanical stress, humidity and temperature cycling. BS EN 60749 is the set of test methods built around package and interconnect reliability, distinct from electrical-performance specifications such as the IEC 60747 series; it focuses on physical and environmental reliability characterisation. Individual parts are self-contained yet complementary, and are widely used for device qualification, incoming inspection, failure analysis and process improvement.
Historically, the earlier parts such as -19 and -20-1 date from 2003–2009, while the later parts (-15, -21, -26, -27, -29, -34, -40, -42, -44, -7) were revised between 2010 and 2016, reflecting the continuous evolution of IC packaging (especially SMD and power devices) reliability requirements.
| Part | Subject | Core Test Content |
|---|---|---|
| BS EN 60749-7 | Internal moisture content | Residual moisture inside the package |
| BS EN 60749-15 | Resistance to soldering temperature (through-hole) | Appearance and electrical performance after dip/reflow |
| BS EN 60749-19 | Die shear strength | Adhesion strength between die and carrier |
| BS EN 60749-20 | Moisture + soldering heat (SMD) | Moisture sensitivity level (MSL) and reflow |
| BS EN 60749-20-1 | Handling, packing, labelling, shipping of SMDs | MSL labelling, dry packing and baking |
| BS EN 60749-21 | Solderability | Wetting of leads / terminations |
| BS EN 60749-26 | ESD sensitivity | HBM / MM electrostatic tests |
| BS EN 60749-27 | Intermittent operating life | Cyclic power ageing |
| BS EN 60749-29 | Latch-up | CMOS latch-up immunity |
| BS EN 60749-34 | Power cycling | Junction-temperature power cycling life |
| BS EN 60749-40 | Package warpage | Board-level warpage at reflow temperature |
| BS EN 60749-42 | Board-level temperature cycling of interconnects | Solder-joint reliability under temperature cycling |
| BS EN 60749-44 | Post lead-free moisture sensitivity | MSL evaluation for lead-free devices |
The original scope is confirmed as “resistance to soldering temperature for through-hole mounted devices”. The method immerses devices at a defined temperature (e.g. 260 °C wave or bath soldering) for a specified time, then inspects appearance, lead integrity and electrical performance. The 2010 edition (Ed.2) added a specification for lead-free solder chemical composition relative to the 2003 edition, reflecting the lead-free transition. This is the fundamental test for verifying a device’s tolerance to soldering thermal shock.
The original scope is confirmed as “die shear strength”. A shear tool pushes the die off the carrier (die pad/substrate) at a defined rate while the maximum shear force is recorded; shear strength is calculated per unit die area. This is the most direct and common destructive test for die-attach quality (eutectic, solder or conductive adhesive), and is especially critical for power and automotive devices. The 2003 edition plus A1:2010 added Note 2 to the scope.
The original scope is confirmed as “handling, packing, labelling and shipping of surface-mount devices sensitive to the combined effect of moisture and soldering heat”. This part is the operating specification for moisture-sensitivity-level (MSL) management: dry packing, humidity indicator cards, warning labels, floor life after opening and re-baking after moisture uptake — the core guarantee of SMD assembly yield.