🧪 BS EN 60455 is the British Standard implementing the European standard EN 60455, which is identical to IEC 60455. The series covers resin based reactive compounds used for electrical insulation — the liquid or flowable thermosetting systems that are applied by impregnation, casting, trickling or vacuum pressure impregnation and then cured in place to form a solid insulating and mechanically supportive structure. It is a primary reference for selecting, testing and accepting insulating resin systems used in motors, transformers, instrument transformers and switchgear. Within the batch there are eight documents spanning the 1998 to 2015 editions, structured as Part 1 (definitions and general requirements), Part 2 (methods of test) and Part 3 (individual material specifications organised as numbered sheets).
The BS EN 60455 family is built under the IEC/TC 15 (Solid electrical insulating materials) and CENELEC framework and is divided into three tiers. Part 1 gives the terminology and general requirements. Part 2 specifies the test methods. Part 3 contains individual material specifications, each published as a “Sheet” describing one class of resin system. The batch of eight files covers the 1998 definitions edition, the 2015 revised test methods edition, and material sheets published between 2003 and 2013.
| Standard | Year | Core subject | Status |
|---|---|---|---|
| BS EN 60455-1 | 1998 | Definitions and general requirements — terminology, classification principles and general inspection rules | Current |
| BS EN 60455-2 | 2015 | Methods of test — revised test procedures, supersedes the 1999 edition | Current |
| BS EN 60455-3-1 | 2003 | Sheet 1: Unfilled epoxy resinous compounds | Current |
| BS EN 60455-3-2 | 2003 | Sheet 2: Filled epoxy resin compounds (e.g. quartz-filled systems) | Current |
| BS EN 60455-3-3 | 2003 | Sheet 3: Polyurethane and other thermosetting resin compounds | Current |
| BS EN 60455-3-4 | 2003 | Sheet 4: Specific resin systems classified by material type | Current |
| BS EN 60455-3-5 | 2006 | Sheet 5: Extended resin compound types and performance criteria | Current |
| BS EN 60455-3-8 | 2013 | Sheet 8: Newer resin systems complementing earlier sheets | Current |
The logic of the family is clear: Part 1 is the general clause, Part 2 is the method, and Part 3 is the product. A user typically selects a material type from Part 3, verifies it using the methods in Part 2, and keeps communication consistent through the definitions in Part 1.
Part 1 defines the core terms — reactive compound, resin, hardener, reaction inhibitor, solvent — and establishes a classification framework based on the base resin type and curing mechanism. The general requirements cover marking, packaging, storage conditions and the general rules for acceptance inspection, laying the common foundation for the subsequent sheets. It superseded the 1978 edition of BS 5664-1, aligning UK practice with the international insulating materials terminology system.
The 2015 edition of the test methods introduced new test items and more explicit sample preparation procedures. It covers viscosity, density, reactivity (gel time), electric strength, dielectric dissipation factor, breakdown voltage and the mechanical properties of the cured body. Because resin performance is highly dependent on mix ratio and cure schedule, the standard stresses that tests must be carried out under specified mixing, degassing, casting and curing conditions to guarantee comparability of results.
Each sheet sets the model designation, test methods and performance limits for a specific resin system. For example, the unfilled epoxy compounds of 3-1 must satisfy specified electric strength, thermal class and process viscosity requirements; the filled systems of 3-2 add requirements on filler dispersion and water absorption. During selection, the user must read the relevant sheet together with the test methods of Part 2.