🌡️ BS EN 60216 is the European Standard series on the thermal endurance (thermal life) of electrical insulating materials, whose technical content is identical to IEC 60216 (adopted by CENELEC from IEC). The thermal endurance of insulating materials determines the life of motors, transformers, windings and other electrical equipment under high-temperature operation. This series provides the complete methodology for deriving long-term thermal parameters through accelerated thermal-ageing tests: from ageing procedures and test criteria to the statistical calculation of thermal endurance characteristics. The assessment of insulation-system temperature classes (A, E, B, F, H) and of the temperature index (TI) depends on this series.
The IEC 60216 series has a long history, formerly BS 5691; around 1995 it moved into the IEC 60216 numbering, adopted by CENELEC as EN 60216 and published by BSI (for example BS EN 60216-2:2005, BS EN 60216-3:2002). The 2013 edition of IEC 60216-1:2013 (6th edition) separated the former “simplified method” into IEC 60216-8:2013, leaving Part 1 focused on general ageing procedures and result evaluation. The UK participates through GEL/112 (Evaluation and qualification of electrical insulating materials and systems) and its predecessor GEL/15.
| Standard | Subject | Content Focus |
|---|---|---|
| BS EN 60216-1:2013 | Ageing procedures and evaluation of test results | General accelerated thermal-ageing procedure and statistical evaluation |
| BS EN 60216-2:2005 | Choice of test criteria | Guidance on selecting the ageing criterion (end-point performance) |
| BS EN 60216-3:2002 | Instructions for calculating thermal endurance characteristics | Steps for computing the thermal-life curve, TI and temperature limits |
| BS EN 60216-4-1:2006 | Ageing ovens; single-chamber ovens | Equipment requirements and verification of ageing ovens |
| BS EN 60216-5:2008 | Ageing ovens; further guidance | Additional oven performance and temperature-uniformity content |
| BS EN 60216-6:2006 | Determination of thermal endurance indices | Assessment of the temperature index (TI) and related thermal indicators |
| BS EN 60216-8:2013 | Simplified procedures | Calculating thermal endurance characteristics by simplified procedures |
Part 1 specifies the general procedure of thermally ageing the material at several temperature points above the working temperature, periodically removing samples to measure a chosen property (such as tensile strength, breakdown voltage, mass loss) until the failure criterion is reached, and evaluating the results statistically (typically least-squares regression with confidence limits) to obtain the thermal-life line (Arrhenius/linearised temperature-life relationship).
Part 2 guides the choice of an “appropriate test criterion” — which dielectric or mechanical property should be used as the life end-point. Part 3 gives step-by-step instructions for calculating thermal endurance characteristics (such as the temperature at a given life, and the temperature index) from multiple ageing datasets, including sample counts, test-point distribution and statistical-processing requirements.
The credibility of ageing results depends heavily on oven temperature uniformity and control precision; Part 4-1 (and Part 5) specify equipment requirements and verification methods for single-chamber ageing ovens. Part 8 provides simplified calculation procedures for limited data, enabling smaller enterprises without a full dataset to obtain usable thermal-endurance estimates.