BS EN 46 — Wood Preservatives — Determination of the Preventive Action against Recently Hatched Larvae of Hylotrupes bajulus (Linnaeus)

European Standard EN 46, implemented in the UK

The BS EN 46 series is the UK implementation of a European standard covering the determination of the preventive action of wood preservatives against the larvae of Hylotrupes bajulus (Linnaeus) (the European house longhorn beetle). Hylotrupes bajulus is an important wood-boring pest of softwood (pine, spruce, etc.) structural timber; its larvae bore inside roofs, trusses and beams, seriously threatening structural safety. The standard uses laboratory biological tests to evaluate the preservative’s preventive action against recently hatched larvae. Part 1 is the surface-treatment method, and Part 2 the ovicidal-effect method.

House longhorn larvae bore into the timber soon after hatching, so early prevention is key: the standard evaluates the preservative’s preventive ability from two angles — preventing larval entry (surface treatment) and killing eggs (ovicidal effect).

1. Scope and Series Structure

PartYearContent
BS EN 46-12016 (supersedes 2009)Wood preservatives — Determination of preventive action against recently hatched larvae of Hylotrupes bajulus — Part 1: Application by surface treatment (laboratory method)
BS EN 46-22016 (supersedes 2009)Wood preservatives — Determination of preventive action against recently hatched larvae of Hylotrupes bajulus — Part 2: Ovicidal effect (laboratory method)

Both parts were prepared with UK participation by Technical Committee B/515 (wood preservation) and adopted as British Standards (ICS 71.100.50). Part 1 evaluates whether larvae can bore in and survive after surface treatment; Part 2 evaluates the preservative’s killing action on eggs.

2. Hylotrupes bajulus Hazard and Protection Background

Hylotrupes bajulus adults lay eggs on softwood surfaces; hatched larvae bore into the timber. Its hazard characteristics include:

  • Preference for softwood: mainly attacks pine, spruce and fir, and is a major pest of European roof structural timber.
  • Structural damage: larval boring forms tunnels that weaken beams, trusses and boards, potentially causing structural failure.
  • Long-term damage: the larval boring phase can last several years, with damage accumulating over time.
  • Protection strategy: treat softwood with preservative to prevent larval entry and kill eggs.
House longhorn damage often develops inside the structure for years before detection; once adults emerge and obvious exit holes appear, the structure may be severely damaged. Preservation treatment should be carried out before timber members are installed.

3. Surface-Treatment Method (Part 1)

BS EN 46-1 specifies the surface-treatment test procedure:

  • Specimen preparation: use standard softwood specimens susceptible to the beetle, controlling dimensions, moisture content and grain.
  • Preservative treatment: apply the preservative to the specimen surface, simulating practical surface brushing or spraying.
  • Larval exposure: place recently hatched larvae on the treated specimen surface, specifying exposure number and time.
  • Validity determination: check whether larvae bore in, survive and feed, comparing with control specimens to assess preventive action.

The evaluation concerns ‘prevention’: whether the preservative prevents recently hatched larvae from boring into the timber and establishing feeding.

4. Ovicidal-Effect Method (Part 2)

BS EN 46-2 specifies the test method for the ovicidal effect:

  • Egg preparation: obtain Hylotrupes eggs and store them under standard conditions.
  • Preservative treatment: expose eggs to a treated surface or preservative coating.
  • Hatching observation: observe egg hatching and larval survival under standard temperature and humidity.
  • Ovicidal determination: compare with untreated controls to evaluate the preservative’s effect on hatching and larval survival.

The ovicidal effect complements surface treatment: even if larvae do not directly contact the treated surface, the preservative can break the hazard source by killing eggs.

5. Engineering Practice and Applications

  • Structural timber preservation: treat load-bearing softwood (roofs, trusses, beams) to prevent Hylotrupes attack.
  • Product evaluation: evaluate the preservative’s preventive action and ovicidal effect against the beetle by standard biological tests.
  • Dose and effectiveness: establish a dose-effect relationship through different dose tests to determine the effective dose.
  • Acceptance and QC: incorporate biological testing into type testing and factory inspection of treated timber.
Engineering recommendation: for structural softwood in Hylotrupes-sensitive areas, use preservatives validated by standard biological tests and ensure adequate dose and penetration depth; after installation, avoid exposing untreated faces by field cutting, and re-apply where necessary.

6. Frequently Asked Questions

Q: What does BS EN 46 determine?
A: It determines the preventive action of wood preservatives against recently hatched larvae of Hylotrupes bajulus, and the ovicidal effect of the preservative.
Q: What is the difference between Parts 1 and 2?
A: Part 1 is the surface-treatment method, evaluating the ability to prevent larval boring and feeding; Part 2 is the ovicidal-effect method, evaluating the killing action on eggs.
Q: Why is Hylotrupes particularly damaging to structural timber?
A: Its larvae bore inside softwood for long periods, weakening beams and trusses, and damage develops within the structure and is hard to detect early.
Q: When is preservation treatment most effective?
A: Treat timber members before installation to avoid later exposing untreated faces by cutting; if field-machined after installation, re-apply preservative to cut surfaces.
Q: How is a preservative judged effective against Hylotrupes?
A: Compare larval boring, survival and feeding on treated and control specimens, and egg hatching and larval survival, per the standard, to assess preventive action and ovicidal effect.
🔒