📷 BS EN ISO 17636 specifies methods for radiographic testing of welds, one of the core standards in the non-destructive testing (NDT) of welded joints. The series consists of two parts: Part 1 covers X- and gamma-ray techniques with film, while Part 2 covers X- and gamma-ray techniques with digital detectors; together they replace the withdrawn BS EN 1435:1997. The UK standards BS EN ISO 17636-1:2013 and BS EN ISO 17636-2:2013 are identical implementations of EN ISO 17636-1:2013 and EN ISO 17636-2:2013, prepared by BSI Technical Committee WEE/46 (Non-destructive testing).
Radiographic testing uses X-rays or gamma rays emitted from a source to pass through the welded joint. Since internal defects (porosity, slag inclusions, lack of fusion, cracks) attenuate radiation differently from the base material, they produce distinct images on film or a digital detector, enabling the detection of internal weld defects. The method is particularly sensitive to volumetric defects (porosity, slag) and is widely used for welds in pressure vessels, boilers, and pipelines.
The series consists of two parts, both classified under ICS 25.160.40 (Welded joints). They were developed by ISO/TC 44 (Welding and allied processes), converted to European standards by CEN/TC 121 (Welding), and adopted as British Standards by BSI.
| Standard | Title | Published | Imaging Mode |
|---|---|---|---|
| BS EN ISO 17636-1:2013 | NDT of welds — Radiographic testing — Part 1: X- and gamma-ray techniques with film | Jan 2013 | Film imaging (conventional radiography) |
| BS EN ISO 17636-2:2013 | NDT of welds — Radiographic testing — Part 2: X- and gamma-ray techniques with digital detectors | Jan 2013 | Digital detector imaging (DR) |
Radiographic testing uses radiation from an X-ray unit or gamma-ray source (e.g., Ir-192, Se-75, Co-60) to penetrate the welded joint. The difference in attenuation between defects and base material produces an image, and the type and size of defects are determined by observing the defect images (density differences). The type and energy of the source should be selected according to the thickness and density of the material to ensure adequate penetration and image contrast.
Attention should be paid to geometric unsharpness (determined by source focal-spot size and focal distance) and the effect of scattered radiation, controlled by increasing focal distance and using filters and lead shielding. The standard specifies the source-to-object distance, beam direction, and film/detector position.
The standard specifies two technique classes (A and B): Class A is the basic technique, while Class B is the improved technique (higher sensitivity). Class B generally requires a smaller source size, a larger focal distance, or stricter image-quality requirements to achieve higher detection sensitivity. The choice of technique class should be based on the importance of the weld and the acceptance requirements.
| Comparison | Part 1 (Film technique) | Part 2 (Digital detector technique) |
|---|---|---|
| Imaging medium | Radiographic film (darkroom processing) | Digital detector (real-time/static imaging) |
| Image recording | Film (long-term archiving) | Digital image (storage and transmission) |
| Image-quality evaluation | IQI (wire/hole type) + density | IQI + grey level and contrast |
| Typical use | Traditional testing, site inspection | High-efficiency testing, digital management |
The standard sets explicit requirements for image quality, including the image quality index of the IQI, the density or grey-level range of the film/digital image, and limits on geometric unsharpness. The IQI is typically of the wire or hole type, placed on the source side; the image quality index evaluated after testing must meet the class requirement specified in the standard.
Image-quality evaluation also includes checking sharpness and contrast and avoiding artefacts (scratches, static marks, light leaks, uneven development) that could hinder defect interpretation. Digital detector technique also requires detector calibration (e.g., dark-field and gain correction) to remove pixel non-uniformity and dead pixels.