BS EN ISO 13934 — Tensile Properties of Fabrics (Strip and Grab Methods)

Textiles — Tensile Properties of Fabrics: Determination of Maximum Force and Elongation at Maximum Force (Strip Method); Determination of Maximum Force (Grab Method)

🧵 BS EN ISO 13934 is the British Standard (BSI) series that adopts the European Standard, itself identical to an International Standard, for determination of the tensile properties of fabrics. The series specifies two methods: Part 1 uses the strip method to determine maximum force and elongation at maximum force; Part 2 uses the grab method to determine maximum force. Tensile properties (breaking force and elongation) are among the most important mechanical properties of fabrics, widely used to evaluate the strength and toughness of woven, knitted, and nonwoven fabrics and in quality acceptance. The technical content was jointly prepared by ISO/TC 38 “Textiles” and CEN/TC 248, and introduced into the British Standards system by BSI.

💡 Fabric tensile properties reflect its resistance to external force. The strip method evaluates the overall strength/elongation of a full-width specimen, while the grab method evaluates local strength with a partially clamped specimen; they serve different applications and are not directly interchangeable.

1. Series Overview 📌

The series covers ICS 59.080.30 (Textile testing) and has two parts:

StandardTitleMain Content
BS EN ISO 13934-1:2013Textiles — Tensile properties of fabrics — Part 1: Determination of maximum force and elongation at maximum force using the strip methodDetermines fabric maximum force and elongation at maximum force by the strip method
BS EN ISO 13934-2:2014Textiles — Tensile properties of fabrics — Part 2: Determination of maximum force using the grab methodDetermines fabric maximum force by the grab method

Part 1 was published in 2013, superseding BS EN ISO 13934-1:1999; Part 2 was published in 2014, superseding BS EN ISO 13934-2:1999. In the UK, technical responsibility is vested in committee TCI/24, Physical testing of textiles.

⚠️ This Standard applies to fabric tensile-property determination but not to elastic fabrics (e.g., high-stretch) or certain special structures, which may need dedicated test methods; confirm applicability before selection.

2. Strip Method (Part 1) 📏

Part 1 specifies determination of fabric maximum force and elongation at maximum force at a constant rate of extension. The strip method uses a full-width strip specimen of specified width, stretched along its length at a specified gauge length and extension rate to rupture, recording maximum force (breaking force) and the corresponding elongation.

Specimen preparation and conditioning significantly affect results: specimens should be conditioned in a standard atmosphere (typically 20 °C, 65% RH) and sampled separately in warp and weft directions; strip width, gauge length, and extension rate follow the Standard. A sufficient number of tests (typically 5 per direction) should be averaged.

  • Specimen: width per the Standard (e.g., 50 mm), length meeting gauge length, sampled in warp and weft.
  • Conditioning: equilibrate in a standard atmosphere for consistent moisture content, reducing hygroscopic differences.
  • Testing: constant extension rate (e.g., 100 mm/min or per the Standard), record force–elongation curve.
  • Calculation: average maximum force and elongation at maximum force over tests.
💡 The strip method stretches the full-width specimen and better reflects overall fabric strength/elongation. Mount the specimen flat and crease-free to avoid slippage at the jaws or premature rupture.

3. Grab Method (Part 2) 📊

Part 2 specifies determination of fabric maximum force by the grab method. The grab method clamps only the central part of the specimen (typically smaller clamp width); the edges are free, closer to the local tensile loading in actual use. The measured force is usually lower than the strip method, because only the clamped region carries the main load.

MethodClampingMeasuredTypical Use
Strip method (Part 1)Full widthMaximum force, elongation at max forceOverall fabric strength/elongation
Grab method (Part 2)Partial (central)Maximum forceLocal strength evaluation

The grab method also requires standard conditioning, separate warp/weft sampling, and sufficient repetition, reporting mean maximum force and coefficient of variation. Because clamping differs, grab and strip results are not directly comparable; choose based on the fabric’s actual use and acceptance requirement.

⚠️ The strip and grab methods use different principles and results are not directly interchangeable. When evaluating fabric strength, state clearly which method is used in the product standard to avoid disputes from mixing methods.

4. Engineering Practice and Application 🛠️

Fabric tensile-property determination is widely used in textiles, apparel, home textiles, and technical textiles:

  • 🔍 Raw-material and process optimization: assess the effect of fibre, yarn structure, and weaving/knitting process on fabric strength and elongation.
  • 🧪 Quality acceptance: sample-test breaking force and elongation of woven, knitted, and nonwoven fabrics.
  • 📋 Product development: provide strength/ductility design input for apparel, home textiles, and industrial fabrics.
  • 🌿 Ageing evaluation: assess durability under washing, light, and humid heat through tensile-property change.
✅ Standardized fabric tensile-property measurement provides reliable, comparable mechanical indicators for textile quality control, product development, and performance evaluation.

5. Frequently Asked Questions ❓

❓ Q: How do the strip and grab methods differ?
A: The strip method clamps the full width and measures maximum force and elongation at maximum force; the grab method clamps only the central part and measures maximum force. Clamping differs, so results are not directly interchangeable.
❓ Q: Why must specimens be conditioned?
A: Textile fibres are hygroscopic; moisture content affects strength/elongation. Conditioning to equilibrium in a standard atmosphere (e.g., 20 °C, 65% RH) removes moisture differences and ensures comparability.
❓ Q: Why is grab-method force usually lower than strip-method?
A: The grab method clamps only the specimen centre; edges are free, so stress concentrates in the clamped region and the full width is not utilized, giving lower maximum force.
❓ Q: How many tests should be performed?
A: The Standard typically requires at least 5 valid tests per direction, averaged, with the coefficient of variation reported; increase for less uniform fabrics.
🔍 Q: Does this Standard apply to elastic fabrics?
A: It mainly covers general fabrics; high-stretch fabrics may need dedicated methods or adjusted extension rate — confirm applicability.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply