BS EN ISO 11299 — Plastics Piping Systems for Renovation of Underground Gas Supply Networks (General and Close-Fit Lining)

Plastics Piping Systems for Renovation of Underground Gas Supply Networks — Part 1: General & Part 3: Lining with Close-Fit Pipes (2013)

📐 BS EN ISO 11299 is the British Standard implementing the European Standard for plastics piping systems used in the renovation of underground gas supply networks. The standard was developed by ISO/TC 138 “Plastics pipes, fittings and valves for the transport of fluids”, taken over as a European standard by CEN/TC 155 “Plastics piping systems and ducting systems”, and published in the UK by BSI. This batch includes Part 1: General and Part 3: Lining with close-fit pipes, superseding the withdrawn BS EN 14408 series. It applies to the design and construction of trenchless renovation of medium- and low-pressure buried gas distribution networks, and is a key technical reference for gas network renewal and rehabilitation.

💡 The biggest difference between gas and water network renovation is the risk level: gas is flammable and explosive, so the renovation system must guarantee long-term tightness to prevent leaks from accumulating and igniting. This makes the requirements for materials, sealing, and acceptance far stricter than for water systems.

1. Scope and Overview of the Series 📌

BS EN ISO 11299 is directed at the renovation of buried gas supply networks and specifies general requirements, material selection, design criteria, installation practice, quality control, and acceptance methods for plastics piping systems used in renovation works. Part 1 provides the general provisions, terms and definitions, symbols and abbreviations applicable to the whole series, together with the classification of renovation methods and selection principles. Part 3 gives dedicated requirements for the close-fit lining technique.

The standard applies to the renovation of buried plastics or metal networks conveying natural gas. The renovated pipe must satisfy gas conveyance and long-term tightness requirements, accounting for the specific effects of the gas medium on materials, connections, and sealing. Because gas is combustible, the standard imposes stricter provisions on safety assessment, leak detection, and acceptance criteria.

🚨 Renovation of gas networks is high-risk work. Before construction, safety measures such as gas purging and depressurization, hot-work permits, and gas detection must be completed; after renovation, tightness testing and re-verification of sealing are mandatory — any leak could cause a serious accident.

2. Series Structure and Technical Highlights 🔧

PartStandard No.TitleMain Content
Part 1BS EN ISO 11299-1:2013GeneralTerms, symbols, classification of renovation methods, general design principles, material and system requirements, quality control foundations
Part 3BS EN ISO 11299-3:2013Lining with close-fit pipesMaterials, dimensions, installation process, reduction and reversion, connections, testing and acceptance of close-fit liners

The series follows a “general part plus specific technique part” structure: Part 1 establishes the common framework, while the later parts give detailed provisions for particular renovation technologies. This batch includes the general part and the close-fit lining part; other renovation technique parts are covered by the corresponding standards.

3. Key Technical Requirements 🔥

3.1 Materials and system performance

The plastics piping system used for renovation must satisfy both gas conveyance and structural strength requirements. The liner material must have sufficient long-term hydrostatic strength, resistance to gas permeation, corrosion resistance, and suitability for gas conveyance. System design must account for the condition of the host pipe, groundwater pressure, traffic loads, and the internal pressure and long-term tightness requirements after renovation.

3.2 The close-fit lining technique

Close-fit lining is a technique in which a plastics liner is reduced in cross-section, pulled into the host pipe, and then restored to conform closely to the host pipe wall. Common implementation methods include the fold-and-form method, reduction methods, and heat reversion / memory-reversion methods. After installation the liner fits tightly against the original pipe with virtually no annular gap, reducing the risk of gas retention and diffusion in the annulus under gas service conditions.

3.3 Design and installation control

The standard sets requirements for minimum liner wall thickness, reduction ratio, reversion recovery ratio, allowable bending radius, pulling load, connections, and end treatments. Prior to installation, CCTV inspection should be carried out to assess the condition of the host pipe; during installation, pulling speed and lubrication must be controlled; after installation, tightness testing and final inspection confirm that the renovated section is leak-free, wrinkle-free, and round.

✅ Key to acceptance: after installation the renovated section must pass tightness testing to verify overall sealing, and CCTV re-inspection to verify liner appearance and connection quality. The section may only be put into service when both structural integrity and gas-tight safety requirements are met.

4. Engineering Practice Essentials 🛠️

  • 🔍 Pre-assessment: use CCTV, leak detection and structural assessment to determine the type and severity of host pipe defects and decide whether close-fit lining is suitable.
  • 🔧 Material matching: select the thermoplastic liner according to gas type, operating pressure, temperature and site conditions, and verify gas suitability and long-term strength.
  • 📊 Installation execution: arrange gas purging, depressurization and hot-work management, control pulling load and reduction amount, and avoid scratching or excessive deformation of the liner.
  • 📋 Quality acceptance: carry out the tests required by the standard and issue CCTV reports and tightness test records as the basis for handover.

5. Frequently Asked Questions ❓

❓ Q: What is the difference between BS EN ISO 11299 and BS EN ISO 11298?
A: They share a similar structure, but BS EN ISO 11299 covers gas networks while BS EN ISO 11298 covers water networks. Gas systems emphasize long-term tightness, leak prevention, and fire/explosion protection, while water systems emphasize hygiene safety and compliance of materials in contact with drinking water.
❓ Q: Why is tightness so essential for gas renovation?
A: Gas is flammable and explosive, and leaked gas accumulating underground can cause explosions. The renovation system must therefore guarantee long-term sealing; no tiny leakage path is permitted, and strict tightness testing is required at acceptance.
❓ Q: Can the renovated pipe continue at the original pressure class?
A: The load capacity after renovation depends on liner wall thickness, material strength, and the residual structure of the host pipe. Structural design calculations per the standard are required, and verification by testing may be necessary to ensure the design internal pressure and external loads are satisfied.
🔍 Q: Why does the series only include the general part and the close-fit part?
A: This reflects the batch of documents published by BSI. The other renovation technique parts (such as CIPP and spiral winding) are specified in the corresponding ISO/EN standards; this article covers only the general part and the close-fit lining part in the collection.
🔒