BS EN ISO 10407 — Petroleum and Natural Gas Industries: Rotary Drilling Equipment — Inspection and Classification of Used Drill Stem Elements Standard Series

The BS EN ISO 10407 series for rotary drilling equipment — inspection and classification of used drill stem elements

🛢️ BS EN ISO 10407 is the British Standard series on petroleum and natural gas industries — rotary drilling equipment, developed jointly by ISO/TC 67 (Materials, equipment and offshore structures for petroleum, petrochemical and natural gas industries) and CEN/TC 12, with UK participation through BSI committee PSE/17/-/4 (Drilling and production equipment for petroleum and natural gas industries). In rotary drilling, the drill string (rotating drill tools made of drill pipe, drill collars, tool joints, stabilisers, etc.) withstands enormous torque, tension, bending and vibration loads, making it a critical element of drilling safety. The series provides systematic methods for the inspection and classification of used (old) drill stem elements, and is an important basis for re-use, quality traceability and safety control of drilling tools.

💡 “Classification” of drill stem elements is the management of re-use value based on damage degree and remaining life: correct classification both ensures drilling safety and avoids premature scrapping and waste.

1. Scope and General Framework 📌

The series applies to drill stem elements in rotary drilling equipment; this batch corresponds to Part 2: Inspection and classification of used drill stem elements (the standard is available in both English and Russian text versions). This part specifies the inspection content, inspection methods, defect assessment, classification criteria and re-use determination for used drill pipe, drill collars, tool joints, lifting subs and other drill stem elements.

During service, drill stem elements undergo wear, corrosion, fatigue, erosion and mechanical damage, and their load capacity decreases with service time. This part determines the damage state of the element through systematic inspection and classifies it according to the standard, providing the basis for continued use, downgraded use or scrapping.

⚠️ If a drill string fails downhole, it can cause stuck pipe, lost-in-hole or even blowout. Inspection and classification of used drill stem elements must be carried out rigorously and must not rely on visual experience alone.

2. Series Composition and Technical Scope 🧱

Standard PartSubjectObjectKey Content
BS EN ISO 10407-2:2008Inspection and classification of used drill stem elementsUsed drill pipe, drill collars, tool joints, etc.Inspection content, methods, defect assessment, classification, re-use determination

This part is one of the core parts of the ISO 10407 series, used together with Part 1 (general requirements for rotary drilling equipment) and ISO 10424 (drill stem elements and threaded connections), covering design, manufacture, inspection and re-use management of the drill string.

3. Inspection Content and Methods 🔬

3.1 Visual and dimensional inspection

Carry out visual inspection and dimensional measurement of drill stem elements, checking wear (outside-diameter wear, tool-joint wear), bending, ovality, thread damage, erosion and mechanical damage, and measuring wall thickness and diameter to determine whether allowable limits are exceeded.

3.2 Non-destructive testing

Use magnetic particle inspection (MPI), ultrasonic testing (UT), penetrant testing (PT) and other NDT methods to check surface and near-surface cracks, fatigue defects and inclusions, focusing on critical areas (such as thread roots, stress-concentration zones and upset transition zones).

3.3 Material and performance inspection

Where necessary, perform material property tests (such as hardness, metallography, chemical analysis) to assess the degree of material degradation (fatigue, hydrogen embrittlement, corrosion fatigue) and estimate remaining life from service history (cycle count, load spectrum).

🚨 Fatigue is the main cause of drill-string failure: fatigue cracks most readily initiate at thread roots and stress-concentration zones. NDT must cover these critical areas, and defect location and size should be recorded as the basis for classification.

4. Defect Assessment and Classification 🧪

Based on defect type, size, location and severity, the standard divides used drill stem elements into several grades (such as fit for continued use, downgraded use, use after repair, scrap) and specifies corresponding re-use criteria. The main factors considered in classification include:

  • 🔍 Defect type and size: type, size and number of cracks, wear, corrosion pits, erosion, etc.
  • 🔧 Defect location: whether the defect lies in a high-stress zone (threads, upset transition, tool joints) and its effect on load capacity.
  • 📊 Remaining wall thickness and load capacity: whether remaining wall thickness after wear meets strength and life requirements.
  • 📋 Service history: cumulative cycle count, service conditions and historical damage, to assess fatigue remaining life.

5. Engineering Practice and Application 🛠️

  • 🔍 Rig-site inspection: inspect and classify recovered drill tools per the standard to determine continued use or repair.
  • 🔧 Repair and re-use: repairable elements (e.g. thread repair, hardfacing) are re-inspected after repair and re-used only if conforming.
  • 📊 Quality traceability: maintain drill-tool records of inspection results, classification and service history for whole-life traceability.
  • 📋 Safety control: strictly control service conditions and monitoring for downgraded elements or those near their life limit.

6. FAQ ❓

❓ Q: Why must used drill stem elements be classified?
A: Classification determines re-use value by damage degree and remaining life, both ensuring drilling safety (preventing failure) and economically utilising elements that can still be used.
❓ Q: What is the most common failure mode of drill stem elements?
A: Fatigue failure is most common (especially at thread roots and stress-concentration zones), followed by wear, corrosion and erosion, identified by NDT and dimensional inspection.
🔍 Q: How is it decided whether drill pipe can continue in service?
A: By combined assessment of visual and dimensional inspection (wear, bending, wall thickness), NDT (cracks), material properties and service history, compared against the standard’s classification criteria.
❓ Q: How are repaired drill tools managed?
A: After repair, re-inspect (e.g. NDT after thread repair, dimension re-check), confirm compliance and record the repair information, then re-use at the corresponding grade.
🔒
正在加载下载地址,请稍候 10 秒