BS EN ISO 00179 — Plastics Charpy Impact Properties Determination Standard Series

Plastics — Determination of Charpy Impact Properties — Non-Instrumented and Instrumented Impact Tests (ISO 179 series)

🥊 BS EN ISO 00179 (i.e. BS EN ISO 179) is the British adoption of the European standard EN ISO 179, identical to the ISO 179 series, which specifies methods for determining the Charpy impact properties of plastics. Impact properties reflect a material’s toughness under high-speed deformation and are a key selection criterion for plastics in structural parts, packaging, automotive components, and other applications. The Charpy impact test applies an impact load to a notched or unnotched specimen via a pendulum and measures the energy consumed in fracture, thereby evaluating the material’s impact resistance. The series was prepared by ISO/TC 61 (Plastics) in cooperation with CEN/TC 249 (Plastics), providing a standard method for the uniform evaluation of plastics impact properties.

💡 Charpy and Izod are the two most common pendulum impact tests: the Charpy (simply supported) specimen rests on two supports and is struck in the middle; the Izod (cantilever) specimen is clamped at one end. ISO 179 belongs to the Charpy pendulum impact system.

1. Positioning and Scope 📌

This series applies to rigid plastics and plastic products for Charpy impact determination, and also to reinforced plastics and fibre composites. Tests are carried out under specified specimen geometry, notch type, and impact conditions to determine the energy-absorption characteristics under impact loading. The standard gives complete requirements for specimen dimensions, notch types, pendulum parameters, test procedure, and result calculation.

Two parts are included in this batch:

  • BS EN ISO 179-1:2010 — Part 1: Non-instrumented impact test, measuring impact strength directly from pendulum energy loss.
  • BS EN ISO 179-2:1999+A1:2012 — Part 2: Instrumented impact test, recording the force-time curve during impact to obtain richer fracture information.
⚠️ The non-instrumented test gives only the fracture energy; the instrumented test records the force-displacement/time curve and can further analyse the initiation and propagation stages. They differ in accuracy and purpose — choose according to need.

2. Series Structure and Technical Highlights 📋

StandardCorresponding ISOMain ContentFeature
BS EN ISO 179-1:2010ISO 179-1:2010Non-instrumented impact test: specimen, pendulum, procedure, impact-strength calculationRoutine quality control, simple and fast
BS EN ISO 179-2:1999+A1:2012ISO 179-2:1997+Amd.1:2011Instrumented impact test: force-time recording, initiation and propagation energy analysisMaterials research and failure analysis

2.1 Part 1 — Non-Instrumented Impact Test

BS EN ISO 179-1 is the basic method. The specimen is a rectangular bar that may be V-notched, U-notched, or unnotched. After the pendulum is released and strikes the specimen, the energy absorbed in fracture is determined from the pendulum’s potential-energy loss. The standard specifies standard specimen dimensions (e.g. 80 mm × 10 mm × 4 mm), notch dimensions, pendulum energy, impact velocity, and gives the impact-strength (kJ/m²) calculation formula. The 2010 edition supersedes the 2001 edition, revising some test details.

2.2 Part 2 — Instrumented Impact Test

BS EN ISO 179-2 adds a load transducer and signal-recording system to the specimen and pendulum, continuously recording the load as a function of time during impact to produce a force-time or force-displacement curve. This allows the total impact energy to be decomposed into initiation energy and propagation energy, providing deeper insight into toughness and fracture behaviour. Amendment A1:2012 updates Clause 9 and adds Annex D. Instrumented testing demands more from equipment and operators and is suited to materials development, failure analysis, and quality tracing.

💡 The “force-time curve” of an instrumented test can distinguish whether a material “fractures on initiation” (brittle) or “propagates extensively after initiation” (tough) — key information a single impact-strength value cannot provide.

3. Key Technical Requirements 🔧

3.1 Specimen Preparation and Conditioning

Specimens should be prepared by the specified method (injection moulding, compression moulding, or machining), with a flat, defect-free surface and dimensions per the standard. Before testing, specimens should be conditioned (temperature and humidity) as required to ensure comparable results.

3.2 Pendulum and Impact Conditions

The pendulum’s nominal energy should be adequate so the residual energy after fracture is not less than a specified proportion; impact velocity and pendulum geometry should meet standard requirements. Notch type (V/U) and notch machining quality directly affect results and must be tightly controlled.

3.3 Result Calculation and Expression

Impact strength is calculated as the fracture energy divided by the specimen cross-sectional area (for notched specimens, the net area at the notch). Results should report impact-strength value, specimen type, notch type, and test conditions, and where appropriate the mean and scatter.

3.4 Instrumented Data Acquisition

Part 2 requires the load transducer to have sufficient frequency response and a sampling rate that meets the resolution of the force-time curve. The determination of initiation and propagation energy relies on characteristic points of the curve (such as peak load) and gives a clear data-processing method.

🚨 Impact testing is a high-speed dynamic process; pendulum release and specimen fracture present fragment-projection risk. Test machines should be fitted with protective guards and operators should follow safety procedures.

4. Engineering Practice 🛠️

  • 🔍 Material selection: compare the toughness of different plastics using impact strength to choose a grade that meets impact requirements.
  • 🔧 Quality control: use the non-instrumented test as a batch-inspection means to quickly judge material consistency.
  • 📊 Failure analysis: use the instrumented test to analyse fracture mechanisms and distinguish brittle from tough fracture.
  • 📋 Design verification: combine impact data with product drop and collision conditions to verify structural reliability.

5. Frequently Asked Questions ❓

❓ Q: What is the difference between Charpy and Izod impact tests?
A: The Charpy (ISO 179) specimen is simply supported at both ends and struck in the middle; the Izod (ISO 180) specimen is clamped at one end and struck at the free end. The support and impact points differ, so results are not directly comparable.
❓ Q: How do notched and unnotched specimens differ?
A: The notch creates a stress concentration, so notched impact strength is usually markedly lower than unnotched. Different notch types (V/U) and sizes also cause different results — they must be stated in the report.
❓ Q: How to choose between non-instrumented and instrumented tests?
A: Use the non-instrumented test (Part 1) for routine quality control and acceptance; use the instrumented test (Part 2) when analysing fracture mechanisms, distinguishing initiation from propagation energy, or carrying out materials development.
❓ Q: Why must specimens be conditioned?
A: Plastic impact properties depend strongly on temperature and moisture content. Conditioning brings specimens to equilibrium at a uniform temperature and humidity, ensuring comparable and repeatable results.
🔒