🧵 BS EN ISO 105 (files numbered BS EN ISO 00105 in this batch) is the UK national implementation by BSI of the ISO 105 family of colour-fastness test methods, comprising about 35 parts. It is the fundamental method system by which the textile, dyeing, garment and testing industries evaluate the ability of dyes and textiles to resist colour change during use and processing. Maintained under technical committee TCI/81 (Colour fastness and colour measurement of textiles), it uses the “Part — Series — Method” structure covering light, washing, rubbing, perspiration, water, weathering and assessment principles. The series is widely referenced by global procurement specs, eco-labels and regulations.
ISO 105 uses a “Part + letter-series + method-number” system: Part A is general and assessment, Part B light and weathering, Part C washing and domestic laundering, Part D colour-fastness to physical properties, Part E water/sweat/seawater/water spotting, Part F adjacent fabrics, Part G solvents and dry-cleaning, Part X special methods, Part P/N special-purpose methods.
| Standard No. | Subject | Series | Typical Content |
|---|---|---|---|
| EN ISO 105-A01 | General principles | Part A | Common conditions for all fastness tests |
| EN ISO 105-A02 | Grey scale for colour change | Part A | Visual 1–5 grade for colour change |
| EN ISO 105-A04 | Instrumental staining assessment | Part A | Measurement of adjacent-fabric staining |
| EN ISO 105-A11 | Digital imaging grading | Part A | Grades by digital-image techniques |
| EN ISO 105-B02 | Artificial light (xenon) | Part B | Xenon-arc light-fastness test |
| EN ISO 105-C06 | Domestic washing | Part C | Wash at varied temp/detergent |
| EN ISO 105-E04 | Perspiration | Part E | Acid/alkali artificial sweat staining |
| EN ISO 105-X12 | Rubbing | Part X | Dry/wet rubbing colour transfer |
| EN ISO 105-P01 | Dry heat (ironing) | Part P | Effect of hot pressing on colour |
| EN ISO 105-N05 | Chlorinated solvents | Part N | Colour stability in dry-cleaning solvent |
Assessment principles (Part A). A01 sets common conditions (temperature, humidity, adjacent-fabric combination, specimen size); A02 (colour change) and A03 (staining) use grey scales for 1–5 visual grading — grade 5 no change, grade 1 severe change; A04 quantifies adjacent-fabric staining instrumentally.
Light and weathering (Part B). B02 uses a xenon-arc lamp to simulate daylight, controlling exposure by blue-wool references or radiant dose and assessing colour change; B03 further assesses outdoor weathering (light + rain + temperature).
Washing and perspiration (Part C/E). C06 grades wash fastness by temperature, alkalinity and mechanical action; E04 uses acid/alkali artificial sweat to assess fastness of skin-contact textiles, relevant to skin-contact safety.
Rubbing (X12). A white cotton cloth rubs the specimen dry and wet to assess surface-colour transfer to the white cloth.
Reliable fastness grading depends on standardised equipment and grade management: light-fastness tests need a xenon lamp with the specified spectral irradiance (filter combinations, radiant-dose control) and exposure controlled by blue-wool references or dose; washing and perspiration tests use prescribed temperature/time and soap/artificial-sweat recipes, with specimens assembled with adjacent fabrics per each part’s stitching layout. Grey scales should be checked periodically for colour drift to avoid grade offset, and grading should be done under standard illumination (e.g. D65) in a light cabinet, by observers validated for normal colour vision and trained.
For result management, laboratories should keep condition records (exposure time, temperature, solution concentration) and Lab colour data (when using instrument/method A04/A11) for dispute review. Batch consistency can be monitored with reference fabrics run per batch to detect instrument and operator drift. On the eco/regulatory side, fastness grades are often combined with substance restrictions (banned azo dyes, sensitising disperse dyes), making grading part of supply-chain compliance — grades are thus both quality indicators and trade-compliance evidence and must be archived properly.