BS EN 846 — Methods of Test for Ancillary Components for Masonry Standard Series

Methods of Test for Ancillary Components for Masonry — BSI National Standard (identical adoption of the EN 846 series)

🧱 BS EN 846 is the UK national standard implementing the European standard series EN 846 “Methods of test for ancillary components for masonry”, prepared by CEN/TC 125 (Masonry) with UK participation through Technical Committee B/519 and its Subcommittees B/519/3 (Ancillary components) and B/519/1 (Masonry units). The series specifies test methods for the load-bearing performance, dimensions, deformation, and durability of ties, anchors, lintels, brackets, hangers, and similar ancillary components, serving as the companion test standard to the EN 845 product specification series.

💡 The EN 846 series is the “method partner” of EN 845 (product specifications for ancillary components): EN 845-1 covers ties, anchors, and hangers, and EN 845-2 covers lintels, while EN 846 provides the unified test methods needed to verify these requirements, supporting CE marking when used together.

1. Overview of the Series 📌

Although ancillary components for masonry (such as wall ties, lintels, brackets, and hangers) are small in size, they are critical to the overall stability of masonry structures and the load-bearing and safety of door/window openings. The EN 846 series is organised by component type and performance parameter: from tension/compression and shear performance of wall ties, load capacity of anchors, to dimensions and bow of lintels, load-deflection characteristics of brackets, and the resistance to impact, abrasion, and corrosion of organic (anti-corrosion) coatings. During the transition period, the UK retained existing BS standards; once the EN 845/846 package is complete, the corresponding old BS standards are progressively withdrawn.

PartTest Object / PerformanceEdition
Part 2Tension and compression tests of ties/anchors2000
Part 3Shear (transverse) tests of ties/anchors2000
Part 4Bending (fatigue/flexural) tests of ties/anchors2002 (2005)
Part 5Deformation (lateral displacement) characteristics of ties/anchors2012
Part 6Ultimate slip/pull-out of ties/anchors in masonry2012
Part 7Tension and compression of ties/anchors (in mortar)2012
Part 8Load-displacement and shear stiffness of anchors/connections2000 (2006)
Part 9Flexibility/deformation of flexible ties2016
Part 10Load capacity and load-deflection characteristics of brackets2000
Part 11Dimensions and bow of lintels2000
Part 13Resistance to impact, abrasion and corrosion of organic coatings2001
Part 14Performance of masonry/components under environmental conditions (durability)2012
⚠️ Most parts of this series are scanned files with limited readable content; the technical points below are summarised from the readable text of Parts 10, 11, and 13, the forewords, and public domain knowledge. Detailed clauses follow the current official BSI edition.

2. Key Technical Requirements 🔧

1. Bracket load capacity and load-deflection characteristics (Part 10 / EN 846-10:2000)

Brackets support cantilevered masonry or decorative elements. This standard specifies the test method for applying a vertical load to a bracket and measuring its load capacity (ultimate load) and load-deflection characteristic curve: the bracket is mounted in a specified test rig, loaded in stages to failure or to a specified deflection, and the load-displacement relationship is recorded to evaluate load capacity and stiffness.

2. Lintel dimensions and bow (Part 11 / EN 846-11:2000)

Lintels span door/window openings to support the masonry above. This standard specifies the method of measuring the length, cross-section dimensions, and bow (the camber/warp along the length) of lintels, to control straightness and ensure accurate opening dimensions and uniform loading after installation. Measurements are made under defined support and datum conditions, with allowable tolerances for dimensions and bow.

3. Organic coating resistance to impact, abrasion and corrosion (Part 13 / EN 846-13:2001)

Ancillary components (especially ties and brackets) often use organic coatings (e.g. a further protective coating over galvanising) to improve corrosion resistance. This standard specifies test methods for the resistance of organic coatings to impact (falling weight/ball), abrasion (wear test), and corrosion (salt spray/immersion), important for evaluating long-term durability. This part supports the EN 845-1 and EN 845-2 product specifications.

4. Mechanical performance of ties and anchors (Parts 2–9)

The series specifies tension, compression, shear (transverse), bending, and deformation tests for wall ties and anchors, together with ultimate slip/pull-out, load-displacement, and shear-stiffness determinations, ensuring ties reliably connect inner and outer leaves, transmit lateral wind loads, and accommodate temperature/moisture movements.

3. Engineering Practice Essentials 🛠️

  • 🔍 Selection and verification: select ties, lintels, and brackets per the EN 845 product specification and carry out type testing per the relevant EN 846 part to verify load capacity, stiffness, and durability meet the design requirements.
  • 🔧 Construction quality control: lintel straightness (Part 11) affects opening dimensions and door/window installation; bracket positions and loads (Part 10) should be design-calculated; tie spacing and embedment depth should follow the specification.
  • 📊 Durability assessment: for components in corrosive environments, evaluate the corrosion-protection class through coating impact, abrasion, and corrosion tests (Part 13), upgrading the plating/coating class where necessary.
  • 📋 CE marking: EN 845-1/-2 are harmonised product standards whose type-test methods are provided by the EN 846 series; manufacturers issue a declaration of performance and affix CE marking accordingly.
🚨 Failure of lintels or brackets can lead to masonry collapse. Never overload, cut openings, or change support conditions arbitrarily; before installation check the lintel’s allowable-load marking and bearing length, and fix brackets to reliable structural substrate.

4. Frequently Asked Questions ❓

❓ Q: What is the relationship between EN 846 and EN 845?
A: EN 845 specifies the performance requirements and product specifications for ancillary components (ties, anchors, hangers, lintels, etc.), while EN 846 specifies the test methods to verify them — the two are used together for type testing and CE marking.
❓ Q: Why measure the “load-deflection characteristics” of brackets rather than only the ultimate load?
A: Brackets must satisfy stiffness requirements in normal service (deflection not excessive), otherwise masonry cracks and finishes loosen; the load-deflection curve provides both capacity and stiffness information, giving a fuller evaluation than a single ultimate load.
❓ Q: Why is the “bow” of a lintel important?
A: If a lintel is excessively bowed, the opening dimensions are inaccurate and loading uneven after installation, preventing proper door/window installation and causing cracking; controlling bow ensures straightness and load-bearing performance.
🔍 Q: How can scanned parts be made workable for testing?
A: Scanned parts offer limited readability. Actual testing should follow the current official BSI printed/electronic edition, executing the specimens, apparatus, and steps in the original text, and cross-checking with the corresponding CEN text.
🔒