BS EN 62047 — Semiconductor Devices Micro-electromechanical Devices Standard Series

Semiconductor devices — Micro-electromechanical devices (IEC 62047 / EN 62047 family, 20 documents)
⚠️ Most of the 20 documents in this series are scanned copies (SCAN>0) and cannot be read line by line. This article is written from publicly available domain knowledge; always refer to the official BSI (British Standards Institution) published edition for exact requirements.

🔬 BS EN 62047 is the British Standards Institution (BSI) adoption of the International Electrotechnical Commission standard IEC 62047 (Semiconductor devices — Micro-electromechanical devices) as the European standard EN 62047 (via CENELEC). The series defines the terminology, test methods, mechanical and material characterisation means for Micro-Electro-Mechanical Systems (MEMS) devices, providing a unified technical language for the design verification, material screening and reliability assessment of MEMS accelerometers, gyroscopes, pressure sensors, micromirrors, RF switches and similar devices. It is maintained by BSI Technical Committee EPL/47 (Semiconductors) and classified under ICS 31.080.99 (other semiconductor devices).

1. Series Overview 📌

MEMS devices integrate mechanical structures with electronic circuits on silicon substrates or thin films, and their performance heavily depends on thin-film mechanics, residual stress, thermal expansion behaviour and fatigue life. The IEC 62047 family uses Part 1 (Terms and definitions) to unify the basic concepts of the MEMS field, then defines “micro-scale mechanical tests” and “material characterisation methods” in individual parts: micro-pillar compression (Part 10) for compressive/yield behaviour of thin films, coefficient of linear thermal expansion (Part 11) for temperature stability, and cantilever/film bending and fatigue tests for long-term reliability. These methods are designed specifically for specimens at the micro-to-sub-millimetre scale and cannot directly use macroscopic material test standards.

💡 Value: MEMS materials exhibit “size effects” differing from bulk materials; IEC 62047 directly measures mechanical behaviour using standardised micro-specimens (micro-pillars, micro-beams, micro-films), filling the gap left by traditional macro tests and serving as a key data source for MEMS design simulation and process scale-up.

2. Structure of the Series and Technical Highlights 📚

Part / DocumentMain ContentTopic
BS EN 62047-1 (2016)Terms and definitionsUnified MEMS terminology system
BS EN 62047-5 (2011)Mechanical tests on thin-film materialsTensile/compressive mechanical properties of thin films
BS EN 62047-7 / 8 / 9 (2011)Beam and film bending testsCantilever deflection, Young’s modulus, residual stress
BS EN 62047-10 (2011)Micro-pillar compression testCompression strength and stress-strain of sub-micro/micro columns
BS EN 62047-11 (2013)CTE of free-standing materialsThermal stability and thermal matching design
BS EN 62047-12~14 (2011–2012)Fatigue and adhesion testsMicrostructure fatigue life, static friction, stiction
BS EN 62047-15~17 (2015)Impact / vibration / acceleration testsShock resistance, vibration, dynamic reliability
BS EN 62047-18~22 (2013–2014)Device characteristics & process testsFilm stress gradient, electro-thermal actuation, process characterisation
BS EN 62047-25 / 26 (2016)Electrochemical / functional testsFunctional verification of MEMS actuators and sensors

3. Key Technical Requirements 🔧

3.1 Micro-pillar compression test (Part 10)

A micron-scale cylinder (micro-pillar) fabricated on a thin-film or bulk-silicon material is loaded with a nanoindenter / micro-compression rig to obtain the compressive strength, plastic deformation and fracture characteristics of the material at micro scale, used to validate process materials (e.g. polysilicon, silicon nitride, metal films).

3.2 Linear thermal expansion coefficient (Part 11)

For free-standing (substrate-unconstrained) MEMS thin-film materials, the linear expansion coefficient is determined through controlled heating and deformation measurement, providing a basis for thermal matching and temperature-drift compensation in bimorph structures.

3.3 Bending and fatigue tests (Parts 7–9, 12–14)

  • Young’s modulus and residual stress: invert modulus and stress gradient from load-deflection of micro-cantilevers / micro-bridges;
  • Fatigue life: cyclic loading determines S-N behaviour and fatigue limit;
  • Adhesion and static friction: measure stiction and static friction of microstructures to assess MEMS failure risk.
✅ Compliance: specimen preparation (lithography, etching, release) and test conditions (temperature/humidity, loading rate, specimen size) must strictly follow the relevant part; the test report should record process information and measurement configuration to ensure reproducibility and comparability.

4. Engineering Practice and Application 🛠️

  • 📐 Design verification: obtain real material parameters (Young’s modulus, yield strength, residual stress) with micro-pillar/beam tests and correct the simulation model.
  • 🧪 Process monitoring: test standard specimens alongside wafer runs to monitor consistency of etch, deposition and anneal processes.
  • 🛡️ Reliability assessment: fatigue, shock, vibration and stiction tests support MEMS product life prediction and failure analysis.
  • 🔄 Supply chain: suppliers and airframers (OEMs) sign material/device acceptance specs based on IEC 62047, unifying the test basis.

5. Frequently Asked Questions ❓

❓ Q: Why can’t MEMS materials use conventional macro test standards?
A: At micro scale the materials show size effects (higher strength, changed ductility), and the process (deposition, etch) determines microstructure; only micro-pillars, beams and films give parameters consistent with real device behaviour.
❓ Q: What is the role of Part 1 terminology?
A: It unifies terms for MEMS devices, materials, processes and tests so manufacturers, designers and test houses communicate consistently — it is the basis for the rest of the series.
❓ Q: Why is the linear thermal expansion coefficient important?
A: MEMS devices often use multi-layer heterogeneous materials; temperature changes induce thermal mismatch stress and drift (e.g. accelerometer zero drift, micromirror angle drift); determining the CTE of free-standing material is the prerequisite for thermal design and compensation.
❓ Q: Does the scanned version affect engineering use?
A: This article is a scanned-version write-up from public knowledge. For formal testing, purchase and verify the official BSI/IEC edition to ensure correct parameters, specimen sizes and acceptance criteria.
🔒