Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
🧵 BS EN 60684 is the European (CENELEC EN) and UK (BS) implementation of IEC 60684, “Flexible insulating sleeving”, mirrored by BSI Technical Committee GEL/15 (Solid electrical insulating materials) and subcommittee GEL/15/5 (Flexible insulating sleeving for electrical purposes). Sleeving is the flexible tubular insulator slipped over wires, terminations and harnesses for insulation, mechanical protection, identification and thermal shielding. The series uses Part 2 (methods of test) as the common test base and Part 3-xxx (specifications for individual sleeving types) to cover extruded silicone, extruded polychloroprene, heat-shrinkable, braided glass-fibre, acrylic-coated, PVC-impregnated/coated, low-smoke zero-halogen, flame-retardant and high-temperature sleeving — the authoritative basis for sleeving selection and acceptance in electrical apparatus, automotive harnesses, aerospace and appliances.
📌 Note: the series comprises 17 documents, most scanned copies. Where temperature ratings, bore series and test conditions are discussed, the text is based on public-domain knowledge and marked “扫描版本,依据公开领域知识撰写” (scanned version, written from public-domain knowledge); the authoritative requirements must be taken from the official BSI publication.
Flexible insulating sleeving plays a “small part, big role” in electrical equipment: it prevents conductor abrasion, insulates terminations, bundles harnesses neatly and shields against heat at hot spots. IEC 60684 unifies sleeving products and tests: Part 2 defines tests for dimensions, temperature index, impregnation, voltage (withstand), mechanical (tension, elasticity, bending), burning, chemical and climatic ageing; Part 3 sheets specify, per material and process, the concrete performance requirements of each sleeving type (bore series, wall thickness, colour, grade and test requirements). The series was published from 1995–2002 and continuously revised (e.g. Part 2:2011, 3-116:2011, 3-280:2010+A1:2014), partly superseding the old BS 6893.
Scope: insulation and protection sleeving for motors, transformers, appliances, automotive and rail harnesses, and aerospace equipment — covering extruded, braided, coated and heat-shrinkable products.
The table below lists the main parts of EN 60684 and their Chinese subject descriptions.
| Part | Subject | Typical edition |
|---|---|---|
| EN 60684-2 | Part 2: Methods of test | 2011 |
| EN 60684-3-116 | 3-116/117: Extruded polychloroprene, general purpose | 2011 |
| EN 60684-3-121~124 | 3-121~124: Braided glass fibre (impregnated/coated) sleeving | 2001 |
| EN 60684-3-205 | 3-205: Heat-shrinkable sleeving (polyolefin general) | 2011 |
| EN 60684-3-209 | 3-209: Flame-retardant/high-temperature heat-shrinkable | 2010 |
| EN 60684-3-214 | 3-214: LSZH heat-shrinkable / sleeving | 2014 |
| EN 60684-3-216 | 3-216: Cross-linked, higher-temperature resistant sleeving | 2005 + A2:2014 |
| EN 60684-3-247 | 3-247: PVC-type sleeving | 2011 |
| EN 60684-3-271 | 3-271: Extruded silicone rubber sleeving | 2011 |
| EN 60684-3-280 | 3-280: Acrylic-coated glass fibre sleeving | 2010 + A1:2014 |
| EN 60684-3-281 | 3-281: Polyurethane/resin-impregnated braided sleeving | 2010 |
| EN 60684-3-282 | 3-282: Silicone-resin-impregnated glass fibre sleeving | 2010 |
| EN 60684-3-283 | 3-283: Flame-retardant braided glass fibre sleeving | 2011 + A1:2014 |
| EN 60684-3-284 | 3-284: High-temperature (Nomex-type) braided sleeving | 2014 |
| EN 60684-3-285 | 3-285: Metal-reinforced/EMI shielding sleeving | 2014 |
| EN 60684-3-400~402 | 3-400~402: Heat-shrinkable end caps / boots | 2002 |
| EN 60684-3-403~405 | 3-403~405: Branch/division protection sleeving | 2002 |
Dimensions and construction. Each sheet prescribes the preferred bore series, wall thickness and length tolerances; braided sleeving also specifies braid density and coating adhesion.
Temperature rating and ageing. Classification by continuous operating temperature (e.g. 105/130/155/180/200 °C grades) verified by accelerated thermal-ageing tests.
Electrical performance. Withstand voltage (electric strength) at the specified voltage, insulation resistance and (where relevant) dielectric constant must be met.
Mechanical and flexibility. Tensile strength, elongation, bending and elastic recovery (extruded) are controlled so the sleeving does not crack during threading and bending.
Flame retardancy and LSZH. Burning tests verify vertical flame self-extinguishing; LSZH grades restrict halogens and smoke density for rail and marine requirements.
Chemical and climatic resistance. Oil, solvent, humidity and UV-ageing tests are executed per the corresponding sheet for long-term environmental suitability.