BS EN 60455 — Resin Based Reactive Compounds for Electrical Insulation Standard Series

Resin Based Reactive Compounds Used for Electrical Insulation — Definitions, General Requirements, Test Methods and Material Specifications

🧪 BS EN 60455 is the British Standard implementing the European standard EN 60455, which is identical to IEC 60455. The series covers resin based reactive compounds used for electrical insulation — the liquid or flowable thermosetting systems that are applied by impregnation, casting, trickling or vacuum pressure impregnation and then cured in place to form a solid insulating and mechanically supportive structure. It is a primary reference for selecting, testing and accepting insulating resin systems used in motors, transformers, instrument transformers and switchgear. Within the batch there are eight documents spanning the 1998 to 2015 editions, structured as Part 1 (definitions and general requirements), Part 2 (methods of test) and Part 3 (individual material specifications organised as numbered sheets).

💡 A resin based reactive compound is supplied as a reactive mixture that flows before curing and cures in situ. The value of the standard family is that it gives both the product specifications and the test methodology a single, globally harmonised vocabulary.

1. Series Overview 📌

The BS EN 60455 family is built under the IEC/TC 15 (Solid electrical insulating materials) and CENELEC framework and is divided into three tiers. Part 1 gives the terminology and general requirements. Part 2 specifies the test methods. Part 3 contains individual material specifications, each published as a “Sheet” describing one class of resin system. The batch of eight files covers the 1998 definitions edition, the 2015 revised test methods edition, and material sheets published between 2003 and 2013.

⚠️ Several documents in this series are scanned versions for which the full text could not be optically recovered; the related technical content has been prepared from public-domain knowledge. The authoritative source remains the officially published BSI version.

2. Structure and Technical Contents 🧱

StandardYearCore subjectStatus
BS EN 60455-11998Definitions and general requirements — terminology, classification principles and general inspection rulesCurrent
BS EN 60455-22015Methods of test — revised test procedures, supersedes the 1999 editionCurrent
BS EN 60455-3-12003Sheet 1: Unfilled epoxy resinous compoundsCurrent
BS EN 60455-3-22003Sheet 2: Filled epoxy resin compounds (e.g. quartz-filled systems)Current
BS EN 60455-3-32003Sheet 3: Polyurethane and other thermosetting resin compoundsCurrent
BS EN 60455-3-42003Sheet 4: Specific resin systems classified by material typeCurrent
BS EN 60455-3-52006Sheet 5: Extended resin compound types and performance criteriaCurrent
BS EN 60455-3-82013Sheet 8: Newer resin systems complementing earlier sheetsCurrent

The logic of the family is clear: Part 1 is the general clause, Part 2 is the method, and Part 3 is the product. A user typically selects a material type from Part 3, verifies it using the methods in Part 2, and keeps communication consistent through the definitions in Part 1.

3. Key Technical Requirements 🔧

3.1 Definitions and general requirements (Part 1)

Part 1 defines the core terms — reactive compound, resin, hardener, reaction inhibitor, solvent — and establishes a classification framework based on the base resin type and curing mechanism. The general requirements cover marking, packaging, storage conditions and the general rules for acceptance inspection, laying the common foundation for the subsequent sheets. It superseded the 1978 edition of BS 5664-1, aligning UK practice with the international insulating materials terminology system.

3.2 Methods of test (Part 2, 2015 edition)

The 2015 edition of the test methods introduced new test items and more explicit sample preparation procedures. It covers viscosity, density, reactivity (gel time), electric strength, dielectric dissipation factor, breakdown voltage and the mechanical properties of the cured body. Because resin performance is highly dependent on mix ratio and cure schedule, the standard stresses that tests must be carried out under specified mixing, degassing, casting and curing conditions to guarantee comparability of results.

3.3 Individual material specifications (Part 3)

Each sheet sets the model designation, test methods and performance limits for a specific resin system. For example, the unfilled epoxy compounds of 3-1 must satisfy specified electric strength, thermal class and process viscosity requirements; the filled systems of 3-2 add requirements on filler dispersion and water absorption. During selection, the user must read the relevant sheet together with the test methods of Part 2.

🚨 Reactive resins can release volatile components and generate exothermic heat during mixing and curing. Workplaces must enforce ventilation, personal protection and fire precautions. The mix ratio and cure temperature profile must follow the material sheet and the supplier’s technical data, otherwise the insulating properties cannot be guaranteed.

4. Engineering Practice 🛠️

  • ⚡ Winding insulation of motors and transformers: impregnating resins (VPI or trickle impregnation) fill the voids of windings and improve corona resistance and thermal endurance.
  • 🧩 Cast insulation: epoxy casting of instrument transformers, sensors and high-voltage apparatus relies on a void-free cured body for electrical strength.
  • 🔬 Incoming inspection: purchasers sample each resin batch for gel time, viscosity and electrical properties using Part 2, and release it only against the figures in the relevant sheet.
  • 📊 Change control: any change of resin, hardener or filler supplier mandates a full re-test to prevent insulation failure from “same type, different batch” variation.

5. Frequently Asked Questions ❓

❓ Q: What is the relationship between BS EN 60455 and IEC 60455?
A: BS EN 60455 is the British Standard implementing EN 60455, which is identical to IEC 60455. The three are technically equivalent and differ only by issuing body and format.
❓ Q: Why is the family split into Parts 1, 2 and 3?
A: Part 1 gives terms and general rules, Part 2 gives test methods, and Part 3 gives product specifications. A new resin system only needs a new sheet, avoiding duplication of definitions and methods, which makes the family easy to extend.
❓ Q: Why distinguish filled from unfilled epoxy compounds?
A: Unfilled systems have low viscosity and good penetration, suited to vacuum impregnation; filled systems reduce cost, shrinkage and thermal expansion while improving thermal conductivity and mechanical strength, suited to casting. The two are performance-oriented and not interchangeable at will.
❓ Q: Why does the test method stress the cure schedule?
A: Most electrical and mechanical properties of the resin form during curing, and the cure temperature and time directly affect crosslink density. A uniform cure schedule is what makes results comparable across laboratories and batches.
❓ Q: How should the scanned parts be treated?
A: Where the full text of a scanned document could not be recovered, the related content is summarised from public-domain knowledge. For procurement and inspection, always use the controlled BSI published version.
🔒