D5348-95 – Standard Test Method Technical Guide

ASTM D5348-95 (Reapproved 2019) establishes a standardized method for determining the moisture content of sulfonated and sulfated oils through azeotropic distillation with xylene. Derived from ASTM D500, this test method is specifically designed for quality assurance in the leather industry,…

D5345-98 – Standard Test Method Technical Guide

📋 Scope and Intended Application ASTM D5345-98 defines the requirements for a prediluted, low-silicate, aqueous ethylene glycol engine coolant with a minimum concentration of 50 volume percent. This specification is specifically tailored for heavy-duty engines, particularly those employing wet cylinder…

D5344-22 – Standard Test Method Technical Guide

📏 Scope and Summary of D5344‑22 This test method covers the measurement of the extension force developed when a partially oriented filament yarn (POY) is drawn between pairs of rolls operating at different surface speeds. The measured force provides an…

D5342-97 – Standard Test Method Technical Guide

ASTM D5342 – 97 (Reapproved 2007) defines a standard procedure for measuring the resistance to bending of paper and paperboard using a Taber-Type Tester in its basic configuration. This test method determines the bending moment required to deflect the free…

D5343-06 – Standard Test Method Technical Guide

📐 Scope, Definitions, and Test Summary This standard guide, designated D5343 – 06 (Reapproved 2018), is developed under the jurisdiction of ASTM Committee D12 on Soaps and Other Detergents (Subcommittee D12.16 on Hard Surface Cleaning). It specifically covers the evaluation…

D5341 – Standard Test Method Technical Guide

📐 Overview and Scope of ASTM D5341/D5341M‑19 ASTM D5341/D5341M‑19, officially titled “Standard Test Method for Measuring Coke Reactivity Index (CRI) and Coke Strength After Reaction (CSR),” is a critical standard under the jurisdiction of ASTM Committee D05 on Coal and…

D5340-24 – Standard Test Method Technical Guide

Important Scope Caveat: The Pavement Condition Index (PCI) is a composite measure reflecting collective engineering judgment based on visible surface distress. It is not intended to replace the direct measurement of roughness, structural capacity, texture, or friction. 📐 Scope and…

D5338-15 – Standard Test Method Technical Guide

🧪 Test Scope and Environment ASTM D5338-15 (Reapproved 2021) establishes a standardized method for determining the degree and rate of aerobic biodegradation of plastic materials. The test is conducted under controlled laboratory conditions that simulate a thermophilic composting environment. By…

D5339-94 – Standard Test Method Technical Guide

📘 Scope and Overview This standard practice, D5339-94 (Reapproved 1998), establishes procedures for a quality assurance plan (QAP) for structural steel fabrication in highway structures. It outlines inspections, measurements, and tests for the fabricator and owner to confirm material and…

D5337-23 – Standard Test Method Technical Guide

🎯 Scope and Applicability of D5337-23 ASTM D5337-23 establishes a standardized practice for setting and verifying the flow rate of personal sampling pumps. These pumps are commonly used for monitoring personal airborne exposures in the workplace. The practice details procedures…

D5336-22 – Standard Test Method Technical Guide

The ASTM D5336-22 standard establishes a comprehensive classification system and basis for specification for Polyphthalamide (PPA) injection molding materials. This system provides a structured method for identifying and specifying PPA compositions, which are high-performance thermoplastics known for their superior mechanical…

D5334-22 – Standard Test Method Technical Guide

📐 Specimen Geometry and Types This test method is applicable for determining thermal conductivity (λ) of soil and rock using a transient heat method. It covers both intact specimens and reconstituted soil specimens, and is effective in both laboratory and…

D5335-24 – Standard Test Method Technical Guide

📐 Scope and Specimen Selection Designation D5335‑24 establishes a standardized laboratory test method for determining the linear (one‑dimensional) coefficient of thermal expansion of intact rock cores using bonded electric resistance strain gauges. This method is intended for evaluation under unconfined…

D5333-03 – Standard Test Method Technical Guide

ASTM D5333-03 establishes a standardized test method for measuring the magnitude of one-dimensional collapse that occurs when unsaturated soils are inundated with fluid. This procedure is critical for evaluating collapsible soils, which can withstand high loads at low water content…

D5332-00 – Standard Test Method Technical Guide

ASTM standard D5332-00 provides a standardized methodology for determining fiber length and length distribution in cotton fibers. Utilizing the Fiber Length Measuring Unit AL-101, this test method is applicable to staple fibers up to 100 mm (4 in.) in length…

D5330 – Standard Test Method Technical Guide

📋 Scope and Classification of Filament-Reinforced Tapes (D5330) ASTM D5330/D5330M – 06 (Reapproved 2020) defines the requirements for pressure-sensitive adhesive tape reinforced with filaments intended for packaging applications. The standard is directly under the jurisdiction of ASTM Committee D10 and…