Category ASTM Standards

ASTM Standards Interpretation

D607-82 – Standard Test Method Technical Guide

📐 Composition and Grade Specifications ASTM D607-82 (Reapproved 2019) establishes the requirements for wet ground muscovite mica pigments intended for use in protective coatings. This standard defines two specific grades based on particle fineness: Type A (Regular 325 M Grade)…

D6068-10 – Standard Test Method Technical Guide

📐 Specimen Geometry and Types ASTM D6068-10 specifies two primary bend-type specimen configurations for generating J-R curves in polymeric materials: the three-point bend (SE(B)) specimen and the pin-loaded compact tension (C(T)) specimen. Both configurations are designed with in-plane dimensions of…

D6069-01 – Standard Test Method Technical Guide

🧪 Scope and Application This test method is specified for the determination of total nitrogen (both organic and inorganic) in aromatic hydrocarbons, their derivatives, and related chemicals. It is applicable for nitrogen concentrations in the range of 0.3 to 2…

D6067 – Standard Test Method Technical Guide

🌍 Scope and Purpose for Environmental Site Characterization The electronic cone penetrometer test is frequently used to determine subsurface stratigraphy for geotechnical and environmental purposes. However, ASTM D6067/D6067M-17 specifically addresses the unique facets of this test when applied to environmental…

D6065-21 – Standard Test Method Technical Guide

📐 Scope and General Principles of D6065-21 The ASTM D6065-21 Standard Practice provides comprehensive guidance for suppliers, reclaimers, purchasers, and users involved in the distribution chain of HFC-227ea (1,1,1,2,3,3,3-Heptafluoropropane, CF3CHFCF3). The primary objective is to ensure this fire-extinguishing agent is…

D6066-11 – Standard Test Method Technical Guide

ASTM D6066-11 provides a standardized procedure for determining the normalized penetration resistance of sands for the evaluation of liquefaction potential. This practice builds directly upon Test Method D1586 (Standard Penetration Test), incorporating specific modifications to the drilling and sampling process…

D6064-11 – Standard Test Method Technical Guide

ASTM D6064-11 (Reapproved 2022) specifies the requirements for HFC-227ea (1,1,1,2,3,3,3-heptafluoropropane, CF3CHFCF3) as a fire-fighting medium. This standard covers the material properties, testing methods, and safety considerations for this hydrofluorocarbon compound. Below are key details derived from the standard. 📐 Definition…

D6063-11 – Standard Test Method Technical Guide

📐 Scope and Purpose This guide provides comprehensive information, including flow charts, for field personnel to collect samples from drums and similar containers. It aims to assist in planning and obtaining samples using equipment and techniques that ensure the objectives…

D6062-19 – Standard Test Method Technical Guide

📐 Scope and Applicability of D6062-19 ASTM D6062-19 is a standard guide that defines the essential conventions for personal samplers used to measure specific particle-size-dependent fractions of non-fibrous airborne aerosols. These conventions are fundamental for assessing health effects, establishing permissible…

D6062M-96 – Standard Test Method Technical Guide

This guide defines conventions for personal samplers of specific particle-size-dependent fractions of any given non-fibrous airborne aerosol. Such samplers are used for assessing health effects and in the setting of and testing for compliance with permissible exposure limits in the…

D6061-01 – Standard Test Method Technical Guide

The ASTM D6061-01 practice provides standardized procedures for evaluating personal samplers of non-fibrous respirable aerosol. It aligns with international conventions to ensure consistency in health effects assessment and exposure monitoring. The values stated in SI units are to be regarded…

D6059-96 – Standard Test Method Technical Guide

📐 Scope and Fiber Definitions This test method (ASTM D6059‑96, reapproved 2011) specifies sampling and analysis for airborne single‑crystal ceramic whiskers (SCCW) such as silicon carbide and silicon nitride in workplace environments. The method involves filtration of a known air…