Category ASTM Standards

ASTM Standards Interpretation

D1272-56 – Standard Test Method Technical Guide

🧪 Overview and Scope This specification, designated ASTM D1272-56 (Reapproved 2002), covers dry pentachlorophenol for use in the preservative treatment of wood. It was originally issued in 1953 and replaced D 1272-53T. The current edition is effective from September 10,…

D1274-95 – Standard Test Method Technical Guide

ASTM D1274 – 95 (Reapproved 2000) specifies standard test methods for the chemical analysis of pentachlorophenol intended for use in the preservative treatment of wood. The procedures ensure the chemical conforms to the requirements of Specification D1272. Sampling prior to…

D1267-23 – Standard Test Method Technical Guide

🧪 Overview and Scope of D1267-23 The ASTM D1267-23 standard defines a specific methodology for determining the gauge vapor pressure of liquefied petroleum gas (LP-Gas) products. This test method is applicable at temperatures starting from 37.8 °C (100 °F) and…

D127-19 – Standard Test Method Technical Guide

📌 Scope and Test Methods ASTM D127-19 (Designation: 133/79 (87)) is a standard test method for measuring the drop melting point of petroleum wax, including petrolatum. It is specifically utilized for petrolatums and microcrystalline waxes. The standard outlines two procedures:…

D1264-24 – Standard Test Method Technical Guide

🧪 Introduction and Test Objective The ASTM D1264‑24a standard, titled “Standard Test Method for Determining the Water Washout Characteristics of Lubricating Greases,” provides a controlled laboratory procedure for evaluating the resistance of a grease to washout by water from a…

D1265-23 – Standard Test Method Technical Guide

🛢️ Scope and Application of D1265-23 ASTM D1265-23a defines the manual method for sampling liquefied petroleum gases (LPG). This practice strictly requires the use of flow-through cylinders equipped with two valves. It is explicitly not applicable to single-valve cylinders or…

D1266-18 – Standard Test Method Technical Guide

📏 Scope and Specifications The ASTM D1266-18 (Designation: 107/86) standard specifies the Lamp Method for the determination of total sulfur in liquid petroleum products. This test method is widely used in the petroleum industry and has been approved for use…

D126-87 – Standard Test Method Technical Guide

🎯 Scope and Classification of Pigments ASTM D126-87 (Reapproved 2023), under the jurisdiction of ASTM Subcommittee D01.31, establishes standardized test methods for the chemical analysis of pigments containing lead chromate and chromium oxide green. This scope specifically covers Chrome Yellow,…

D1263-04 – Standard Test Method Technical Guide

🔬 Test Overview and Scope The ASTM D1263-94 (Reapproved 2005)e1 test method, formally the Standard Test Method for Leakage Tendencies of Automotive Wheel Bearing Greases, provides a standardized laboratory procedure for differentiating between grease products with distinctly different leakage characteristics.…

D1257-22 – Standard Test Method Technical Guide

This standard specification covers high-gravity glycerin with a minimum purity of 98.7 % by weight. It is intended for use in the manufacture of alkyd resins, synthetic resins, and similar industrial applications. The values stated in SI units are regarded…

D1258-05 – Standard Test Method Technical Guide

🧪 Scope and Significance of ASTM D1258-05 ASTM D1258-05 outlines the standard test methods for the sampling and testing of High-Gravity Glycerin (1,2,3-propanetriol), also known as glycerol. These methods are specifically designed for evaluating the purity and quality of glycerin…

D1259-06 – Standard Test Method Technical Guide

📐 Standard Overview and Method Selection ASTM D1259-06 (Reapproved 2018) provides standardized procedures for determining the nonvolatile content of resin solutions. This measurement is essential for coatings producers as it defines the total solids available for film formation and facilitates…