Category ASTM Standards

ASTM Standards Interpretation

D3862-13 – Standard Test Method Technical Guide

ASTM D3862-13 (Reapproved 2024) provides a standardized test method for user laboratories to evaluate the retention characteristics of 0.2‑µm membrane filters. These filters are widely employed in routine microbiological water quality testing. The method determines whether the membrane can retain…

D3860-98 – Standard Test Method Technical Guide

ASTM D3860-98 (Reapproved 2020), officially the Standard Practice for Determination of Adsorptive Capacity of Activated Carbon by Aqueous Phase Isotherm Technique, establishes a standardized methodology for evaluating the performance of both granular and powdered activated carbons in removing soluble contaminants…

D3858-95 – Standard Test Method Technical Guide

📐 Method Scope and Applications ASTM D3858-95 (Reapproved 2014) establishes a standard test method for measuring the volume rate of flow of water in open channels. This is achieved through the velocity-area method, which involves determining the flow velocity and…

D3859-15 – Standard Test Method Technical Guide

ASTM D3859-15 (Reapproved 2023) provides standardized atomic absorption methods for determining dissolved and total recoverable selenium in water. Selenium monitoring is critical due to its toxicity profile, and the standard specifies two principal techniques (Gaseous Hydride AAS and Graphite Furnace…

D3855-84 – Standard Test Method Technical Guide

🧪 Scope and Significance of the Test Method ASTM D3855-84 (Reapproved 2010) provides a standardized laboratory procedure for evaluating the resistance of bare rubber threads to deterioration when exposed to a standard washing solution, followed by room-temperature drying and accelerated…

D3856-11 – Standard Test Method Technical Guide

ASTM D3856-11 provides consensus good laboratory practices for laboratories involved in water sampling and analysis. It establishes minimum criteria for management systems to ensure data quality and organizational competence, serving as a foundational framework for laboratories seeking compliance with recognized…

D3853-22 – Standard Test Method Technical Guide

📐 Scope and General Application ASTM D3853-22 provides a comprehensive compilation of standard abbreviations for chemicals used in compounding rubber products. This terminology is essential for clear, consistent technical writing across the rubber industry. It specifically covers abbreviations for accelerators,…

D3854-90 – Standard Test Method Technical Guide

This test method, officially designated D3854-90 (Reapproved 2010) — Standard Test Method for Rubber Thread—Resistance to Dry Heat — evaluates the resistance of rubber thread to deterioration when exposed to elevated temperatures. Unlike conventional rubber aging tests performed on unstretched…

D3852-20 – Standard Test Method Technical Guide

📝 Product Description and Physical Properties ASTM D3852-20 provides standardized guidance for the safe sampling and handling of phenol, cresols, and cresylic acid. The standard describes phenol as a colorless to light pink crystalline material with a melting point of…

D3850-19 – Standard Test Method Technical Guide

📐 Scope and Key Limitations ASTM D3850-19 outlines a standardized procedure for obtaining thermogravimetric (TGA) data on solid polymeric materials intended for electrical insulation. This test method is crucial for evaluating the rapid thermal degradation behavior of materials by measuring…

D3851-17 – Standard Test Method Technical Guide

📐 Scope and Classification of Microcellular Polyurethane Shoe Soling Materials ASTM D3851-17 (2022) establishes the standard specification for microcellular polyurethane (MPU) materials intended for shoe soling applications. This specification defines the minimum physical property requirements and identifies the specific ASTM…

D3848-03 – Standard Test Method Technical Guide

ASTM D3848‑03 (Reapproved 2022) provides a standardized methodology for the evaluation of acrylonitrile-butadiene rubber (NBR) when compounded with carbon black. It defines the standard test formula, mixing procedures, and specific test methods necessary for consistent characterization across laboratories. The values…