BS EN 60831 — Shunt Power Capacitors of the Self-Healing Type for a.c. Systems (Rated Voltage Up to 1000 V) Standard Series

Performance, Testing and Rating, Safety Requirements, and Ageing, Self-Healing and Destruction Tests (IEC 60831 Series)

⚡ BS EN 60831 is the British Standards Institution series adopting European Standard EN 60831, identical to IEC 60831, which covers self-healing shunt power capacitors for a.c. systems having a rated voltage up to and including 1000 V, used for reactive power compensation. These capacitors use metallised polypropylene film as dielectric: when a local dielectric breakdown occurs, the metallised electrode evaporates locally and restores insulation, giving the capacitor a self-healing property. Part 1 specifies general requirements — performance, testing and rating, safety requirements, and a guide for installation and operation; Part 2 specifies the ageing test, self-healing test and destruction test. The series was prepared by Technical Committee PEL/33, Power capacitors, and is the basis for design, testing, safety and operation of low-voltage reactive power compensation capacitors.

💡 Self-healing shunt capacitors are compact, low-loss and maintenance-free, making them the mainstream device for reactive power compensation in low-voltage distribution systems. The self-healing property lets them continue operating after local dielectric breakdown — a key safety advantage distinguishing them from traditional capacitors.

1. Scope and General Framework 📌

The BS EN 60831 series is identical to IEC 60831, prepared by IEC/TC 33 “Power capacitors and their applications”, and was adopted in the UK by Technical Committee PEL/33. Part 1 (2014 edition, incorporating the May 2014 corrigendum amending clause B.4.3) supersedes the 1998 edition; Part 2 (2014 edition) supersedes the 1996 edition. The series applies to self-healing shunt power capacitors with rated voltage up to and including 1000 V at 50 Hz (or 60 Hz), specifying performance, ratings, test methods, safety requirements and installation/operation guidance.

⚠️ Self-healing capacitors at end of life or under severe faults (e.g. short-circuit of internal elements) may bulge, leak or even rupture. The series specifies safety protection requirements (e.g. bursting devices, overpressure protection) and destruction-test criteria; safety protection deserves full attention in selection and installation.

2. Structure of the Series 📋

Standard NumberTitleIEC ReferenceMain Content
BS EN 60831-1:2014Shunt power capacitors of the self-healing type for a.c. systems up to and including 1000 V — Part 1: General — Performance, testing and rating — Safety requirements — Guide for installation and operationIEC 60831-1:2014 (incl. May 2014 corrigendum)Ratings, performance requirements, test methods, safety requirements and installation/operation guide
BS EN 60831-2:2014Shunt power capacitors of the self-healing type for a.c. systems up to and including 1000 V — Part 2: Ageing test, self-healing test and destruction testIEC 60831-2:2014Test methods and acceptance criteria for ageing, self-healing and destruction tests

3. Key Technical Requirements 🔧

3.1 Ratings and Performance Requirements

Part 1 specifies ratings such as rated voltage, rated capacitance, rated frequency, maximum permissible overvoltage, maximum permissible overcurrent (including harmonics), insulation level and temperature category, together with performance requirements such as capacitance tolerance, loss tangent (dielectric loss) and insulation resistance. These parameters are the basis for capacitor selection and operation, directly affecting compensation effectiveness and service life.

3.2 Types of Tests

Part 1 specifies routine tests and type tests, including: voltage test between terminals, voltage test between terminal and case, capacitance measurement, loss tangent measurement, insulation resistance measurement, withstand voltage tests and discharge test, with test voltage, duration and acceptance criteria. Tests are performed under the specified environmental and charge/discharge conditions.

Test ItemProperty AssessedKey ParametersTypical Criterion
Voltage test between terminalsDielectric withstand capabilityTest voltage, durationNo breakdown, no flashover
Voltage test terminal-to-caseInsulation to caseTest voltage, durationNo breakdown, no flashover
Capacitance and loss measurementCapacitance and dielectric lossCapacitance tolerance, loss tangentWithin specified limits
Discharge testSafe discharge performanceDischarge resistor, residual voltageVoltage falls to a safe value within the specified time
Destruction test (Part 2)Fault safety performanceDestruction current, temperature riseCase does not rupture or eject burning material

3.3 Ageing, Self-Healing and Destruction Tests (Part 2)

Part 2 specifies the ageing test, self-healing test and destruction test for self-healing shunt capacitors. The ageing test applies overvoltage and temperature cycling to simulate long-term operation and assess capacitance decay; the self-healing test verifies the capacitor’s self-healing capability after dielectric breakdown (capacitance change before and after healing within limits); the destruction test verifies safe behaviour under fault conditions (e.g. internal short-circuit, overvoltage breakdown) — the case must not rupture or eject burning material, preventing harm to surrounding equipment and personnel.

3.4 Safety Requirements and Installation/Operation Guide

Part 1 includes safety requirements (such as discharge devices, bursting and overpressure protection, case earthing, fire and explosion protection) and an installation/operation guide (such as overvoltage/overcurrent protection, harmonic management, temperature monitoring and periodic inspection). Correct installation and operation significantly extend capacitor life and prevent fault escalation.

4. Engineering Practice and Application 🛠️

  • 🔍 Reactive power compensation design: determine compensation capacity from the load power factor and target, select the rated voltage and reactor matching against the harmonic environment, avoiding harmonic resonance and overcurrent.
  • 🔧 Harmonic management: in systems with non-linear loads (drives, rectifiers), check the capacitor against the overcurrent capability specified in the standard, adding series reactors where necessary to suppress harmonics.
  • 📊 Safety protection: select capacitors with bursting devices and discharge devices, earth correctly, and provide overvoltage/overcurrent protection and temperature monitoring in the capacitor bank to ensure safe isolation at fault.
  • 📋 Operation and maintenance: periodically check capacitance, loss tangent and appearance (bulging, leakage), assess life from ageing and self-healing test results, and replace capacitors with degraded performance promptly.
✅ Selecting, testing, and maintaining self-healing shunt capacitors per the BS EN 60831 series ensures performance and safety under rated conditions and harmonic environments, providing an important guarantee for the long-term reliable operation of low-voltage reactive power compensation systems.

5. Frequently Asked Questions ❓

❓ Q: What is “self-healing” and why is it important?
A: Self-healing means that when a local dielectric breakdown occurs, the metallised electrode near the breakdown point evaporates instantly, forming an insulating isolation and restoring the capacitor’s insulation without failure. This allows the capacitor to continue operating with local defects, significantly improving reliability and life — the core advantage of metallised film capacitors.
❓ Q: How do BS EN 60831-1 and BS EN 60831-2 relate?
A: Part 1 specifies ratings, performance, test methods, safety requirements and installation/operation guidance — the general requirements; Part 2 gives dedicated test methods and acceptance criteria for the ageing, self-healing and destruction tests, assessing long-term reliability and fault safety.
❓ Q: Why must capacitors be equipped with discharge devices?
A: After disconnection, a capacitor retains stored charge; residual voltage can endanger maintenance personnel and damage equipment. The discharge device (discharge resistor) reduces the terminal voltage to a safe value within the specified time after disconnection, ensuring maintenance safety.
🔍 Q: How do harmonics affect self-healing capacitors?
A: Harmonic currents superimposed on the fundamental cause capacitor overcurrent and overheating, accelerating dielectric ageing and capacitance decay, and can even lead to faults. Check the capacitor’s effective current and temperature rise under harmonics, and add reactors or choose capacitors with higher rated voltage/overcurrent capability where necessary.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply

Your email address will not be published. Required fields are marked *