SAE J3179-2022: Standardized Corrosion Testing for MAC Condensers

This article provides a comprehensive overview of SAE J3179-2022, a standardized test procedure for evaluating the corrosion behavior of aluminum-brazed mobile air conditioning (MAC) condensers. It outlines the two primary accelerated corrosion tests—CCCT and DeCa—their methodologies, safety requirements, and key…