🧱 PD CEN TS 16637 is the British Standards Institution (BSI) Published Document implementing the European Technical Specification CEN/TS 16637, dedicated to assessing the release of dangerous substances from construction products. Prepared by UK technical committee B/557 “Construction products — Assessment of dangerous substances,” it is classified under ICS 13.040.20 (ambient air quality), 19.040 (environmental testing), and 91.100.01 (building materials in general). It provides a harmonised system of leaching and percolation test methods for concrete, mortar, aggregates, masonry, coatings, and many other construction products, forming a key technical basis for release assessment under the EU Construction Products Regulation (CPR).
The PD CEN TS 16637 series comprises 3 parts: Part 1 is the test guidance, while Parts 2 and 3 specify two categories of test method. All three share the same ICS classification and cross-reference each other, together forming a coherent methodology for release assessment.
| Part | Year | Title | Core Content |
|---|---|---|---|
| PD CEN/TS 16637-1 | 2014 | Guidance for the determination of leaching tests and additional testing steps | Sets out how to choose the appropriate leaching test and further testing steps based on product form and exposure scenario |
| PD CEN/TS 16637-2 | 2014 | Horizontal dynamic surface leaching test | Defines a dynamic leaching test for monolithic or block products in contact with water |
| PD CEN/TS 16637-3 | 2016 | Horizontal up-flow percolation test | Defines a percolation test for granular products with water flowing upwards through the bed |
Part 1 provides the methodological foundation of the whole series. It guides the user to choose correctly between the “monolithic/block product” and “granular/bulk product” categories according to product characteristics and use scenario, and to determine the corresponding test steps:
The guidance stresses that test design should reflect the product’s real exposure conditions, including the composition of the contact medium (e.g., pH, salinity), liquid-to-surface/solid ratio, contact time, and temperature, so results are representative and comparable.
Part 2 specifies the Horizontal Dynamic Surface Leaching Test, applicable to monolithic or block products. A test specimen with a defined surface area is contacted with a leachant (typically deionised water or a simulated medium) under controlled conditions, with the leachant renewed or replaced at prescribed time intervals. The concentration of substances released into the liquid phase at each interval is measured, yielding release rates and cumulative release per unit surface area and time.
| Key Parameter | Description |
|---|---|
| Surface area to volume ratio | Governs the relationship between contact area and leachant volume, affecting release kinetics |
| Leachant renewal interval | Leachant is replaced at set time steps to obtain a release curve over time |
| Liquid-to-surface ratio (L/S) | Ratio of leachant volume to specimen surface area — the basis for expressing and comparing results |
| Temperature and agitation | Controlled temperature and uniform liquid-solid interface contact |
This method suits surface-dense products such as coatings, panels, and blocks; results can be used to estimate the long-term diffusive flux of pollutants to the water environment.
Part 3 specifies the Horizontal Up-flow Percolation Test, applicable to granular or bulk products. A sample of defined particle size distribution and compaction is packed into a percolation column; leachant flows upwards at a constant rate through the sample bed. The eluate is collected in volume fractions, and the concentration of dangerous substances in each fraction is measured to characterise release from particles under dynamic flow.
| Key Parameter | Description |
|---|---|
| Column dimensions and packing | Column diameter, particle size distribution, and packing density set per standard to ensure uniform flow |
| Up-flow velocity | A constant flow rate simulates rainwater or groundwater passing through a material layer |
| Liquid-to-solid ratio (L/S) | Expressed as cumulative eluate volume per unit sample mass — the x-axis variable of percolation results |
| Fraction collection | Eluate collected in L/S fractions to obtain release concentration versus L/S curves |
The percolation test is especially suited to loose products such as aggregates, recycled materials, and soil amendments, and is often combined with leaching data in life-cycle environmental assessment.