🛣️ PD CEN/TS 15901 is a series of Published Documents issued by the British Standards Institution (BSI) based on the European Technical Specification CEN/TS 15901 for road and airfield surface characteristics, whose core content is the determination of skid resistance (anti-skid performance). The two parts covered in this batch, PD CEN/TS 15901-14:2016 and PD CEN/TS 15901-15:2014, specify test procedures for determining skid resistance using two measurement devices based on the “longitudinal controlled slip” principle — ViaFriction and IMAG. Such devices can measure pavement friction performance continuously and at high speed, providing important technical support for road and airfield safety management and pavement maintenance decisions.
The CEN/TS 15901 series is prepared by the European Committee for Standardization (CEN) committee responsible for road and airfield surface characteristics; the UK participates through Technical Committee B/510/5. The series gives a separate procedure for each type of skid-resistance measurement device. The two parts in this batch are summarised below:
| Standard | Device | Principle | Year |
|---|---|---|---|
| PD CEN/TS 15901-14:2016 | ViaFriction (Road Analyser and Recorder ROAR of ViaTech AS) | Longitudinal Controlled Slip (LFCN) | 2016 |
| PD CEN/TS 15901-15:2014 | IMAG | Longitudinal Controlled Slip (LFCI) | 2014 |
The basic principle of longitudinal controlled slip (LFCN/LFCI) devices is: the test vehicle travels at a constant speed while the test wheel maintains a predetermined longitudinal slip ratio (usually a fixed value) with the pavement surface; the longitudinal force on the test wheel is measured and combined with the normal load on the tyre to calculate the pavement friction coefficient (often denoted by a specific symbol such as the LFCN coefficient).
This type of method can continuously collect pavement anti-skid data while maintaining a relatively high travelling speed, covering a long distance in a short time and with high test efficiency. It is particularly suited to wide-area surveys of long road sections or airfield runways, and is also useful for before/after maintenance comparison, black-spot investigation, and trend analysis of anti-skid degradation.
PD CEN/TS 15901-14:2016 specifies the procedure for determining skid resistance using the ViaFriction device (the Road Analyser and Recorder ROAR manufactured by ViaTech AS). Its content covers the device construction, test wheel and tyre conditions, slip ratio setting, test speed, wetting (wet-state) control, data acquisition and processing, and result reporting format.
The standard requires defined test environment and vehicle conditions: testing under specified wet conditions (ensuring a wet pavement), travelling at the specified speed, with the test-wheel tyre size and wear state complying with requirements, and recording and, where necessary, correcting for influencing factors such as temperature, to ensure repeatability and reproducibility of the measured values.
PD CEN/TS 15901-15:2014 specifies the procedure for determining skid resistance using the IMAG device. Like Part 14, IMAG also uses the longitudinal controlled slip principle (corresponding abbreviation LFCI), characterising anti-skid performance by measuring the longitudinal force at a predetermined slip ratio between the test wheel and the pavement.
This part likewise specifies device construction, test wheel and tyre, slip ratio, speed, wet-state control, data acquisition and result reporting, and provides its field of application and recommended uses, helping users judge the applicability of the device in different road and airfield scenarios.
Combining the two parts, the key requirements for determining skid resistance include:
In engineering practice, these methods are widely used for: acceptance testing of new pavements, periodic testing of in-service pavement anti-skid performance, investigation of accident-prone sections, evaluation of winter de-icing and anti-skid strategies, and monitoring and safety assessment of airfield runway friction characteristics.