PD CEN TR 15339 — Thermal Spraying Equipment Safety Requirements Series

Thermal Spraying — Safety Requirements for Thermal Spraying Equipment Series (PD CEN/TR 15339)

🔥 PD CEN/TR 15339 is a Published Document series issued by BSI adopting the European Committee for Standardization technical report CEN/TR 15339, providing systematic requirements for machinery safety and occupational safety of thermal spraying equipment. Thermal spraying processes (flame spraying, arc spraying, plasma spraying, HVOF hyper-velocity oxy-fuel spraying, cold spraying, etc.) rely on high temperature, high velocity, combustible gases and powder feedstocks, so the equipment itself carries multiple risks of explosion, fire, burns, noise, dust and electricity. Developed by CEN/TC 240 (Thermal spraying), the series gives manufacturers a unified framework for designing safe equipment and users a framework for safe operation.

🚨 Thermal spraying equipment is a typical “dangerous machine”: the torch outlet temperature can reach several thousand degrees Celsius; if fuel gases (acetylene, propane, hydrogen, etc.) and oxidants (oxygen, air) leak, flash back or are mixed incorrectly, explosion and fire are highly likely. Equipment safety design must control these risks at source.

1. Series Structure and Document Scope 📌

DocumentSubjectEditionStatus
PD CEN/TR 15339-1General requirements2014Readable
PD CEN/TR 15339-3Torches for thermal spraying and their connection and supply units2014Readable
PD CEN/TR 15339-4Gas and liquid fuel supply2014Readable
PD CEN/TR 15339-5Powder and feeding systems (scanned)2014Scanned
PD CEN/TR 15339-6Auxiliaries and workshop layout (scanned)2014Scanned
⚠️ Parts 5 and 6 are scanned versions whose full text cannot be extracted; they are summarised here in line with the consistent framework of thermal spraying equipment safety. Always refer to the BSI official published versions for specific clauses.

2. General Requirements (Part 1) 🧭

Part 1 establishes the overall framework for thermal spraying equipment safety, centred on “safe machinery design + market placement compliance”. Its main content:

  • Design and construction of safe machinery: follow a safe design procedure, complying with the essential health and safety requirements (EHSR) of machinery legislation (e.g., the Machinery Directive).
  • Technical documentation and construction file: establish a technical file and construction file recording risk assessment and safety measures.
  • Placement on the market and putting into service: covers instructions, marking and declaration of conformity, ensuring equipment meets regulatory requirements when placed on the market.

This part stresses that risk assessment is the foundation of whole-life safety: identify hazards and take protective measures at each stage from design, manufacture, transport, installation, commissioning, use to maintenance.

💡 Part 1 puts “safety” onto a compliance path: manufacturers must not only design safely but also produce a complete construction file and declaration of conformity to legally place thermal spraying equipment on the EU/UK market.

3. Torches and Their Connection and Supply Units (Part 3) 🔫

The torch is the core actuating component of a thermal spraying system and the danger point closest to high-temperature, high-pressure gas flow. Part 3 gives safety characteristics of torches and their connection and supply units by spraying process type:

  • Flame and HVOF spray torches: emphasise flashback prevention, fuel/oxygen ratio control, cooling requirements and ignition procedures.
  • Cold spray torches: strength, pressure reduction and relief of high-pressure gas lines (up to several MPa).
  • Arc spray torches: wire feeding, electrical insulation and arc shielding.

The standard also specifies requirements for connectors between torch and supply units (mistake-proofing, anti-loosening, sealing), and safe design of spray nozzles and powder conveying lines.

Spraying ProcessKey Safety FeatureMain Hazard
Flame sprayingFlashback arrestor, ratio valve, ignition procedureFlashback, gas leakage
HVOFHigh-pressure combustion, cooling, explosion reliefDeflagration, high temperature
Arc sprayingInsulation, shielding, wire-feed interlockElectric shock, arc glare
Cold sprayingHigh-pressure line strength, pressure reduction and relief valvesHigh-pressure jet, line rupture

4. Gas and Liquid Fuel Supply (Part 4) ⛽

Part 4 focuses on the fuel and gas systems supporting thermal spraying. Its content covers:

  • Gases for thermal spraying: classification, purity and storage of fuel gases (acetylene, propane, hydrogen, natural gas), oxidants (oxygen, compressed air) and inert gases.
  • Safety-related features of gas, liquid fuel and cooling-water supply: line materials, connectors, pressure reducers, flow control, check valves and relief devices.
  • Potential hazards: leakage, flashback, overpressure, explosive mixtures and toxicity of combustion products.
  • Safety requirements and protective measures: ventilation, gas monitoring, emergency shut-off, marking and procedures.

The standard stresses that fuel-gas lines must be strictly separated from oxygen/air lines and protected against wrong connection; pressure reduction and flashback prevention are key safety barriers; and workshops should have adequate ventilation and gas detection.

⚠️ The gas supply system is the weakest link of thermal spraying safety: wrongly connecting fuel gas to the oxygen side, regulator failure or line leakage can all lead to catastrophic accidents. Part 4 requires a complete defence from line colour coding, connector mistake-proofing and check valves to periodic inspection.

5. Powder Feeding and Ancillary Systems (Parts 5/6) 📦

Part 5 covers powder and feeding systems, involving powder conveying, hoppers, metering devices and dust control; combustible metal powders (especially aluminium, magnesium) present dust-explosion hazards requiring explosion protection and dust extraction. Part 6 covers ancillaries (e.g., grit-blasting equipment, turntables, manipulators) and workshop layout, involving ventilation, noise insulation, fire compartments and ergonomics. Together they form the overall safe environment of thermal spraying workplaces.

6. Engineering Practice Application 🛠️

  • 🔍 Equipment selection: when purchasing thermal spraying equipment, check its CE/UKCA marking, compliance documents and construction file to confirm compliance with the series safety requirements.
  • 🔧 Installation and commissioning: per Part 4, standardise gas-line connections, implement leak testing, verify regulators and check valves, and establish ignition/shut-off procedures.
  • 📊 Operation management: establish work-permit systems, require certified operators, and periodically inspect hoses, connectors, sensors and alarm devices.
  • 📋 Dust and ventilation: implement dust extraction and explosion protection for combustible metal powders, maintain workshop ventilation and gas monitoring to prevent explosive atmospheres.

7. Frequently Asked Questions ❓

❓ Q: What parts does PD CEN/TR 15339 have?
A: The series includes general requirements (Part 1), torches and connection/supply units (Part 3), gas and liquid fuel supply (Part 4), plus powder feeding (Part 5) and ancillaries/workshop (Part 6) items.
❓ Q: Why is the flashback arrestor so important?
A: During thermal spraying, the flame is ejected at high speed; if the gas flow becomes unstable, the flame may be “sucked back” into the fuel hose or even the cylinder, causing explosion. The flashback arrestor is the key device blocking flame return.
❓ Q: Why must fuel-gas and oxygen lines be managed separately?
A: Mixing them forms an explosive mixture. Part 4 requires mistake-proof connectors (different threads/sizes), line colour coding and check valves to eliminate wrong connections.
❓ Q: What special risk do metal powders pose?
A: When the suspension concentration of aluminium, magnesium, etc., reaches the lower explosive limit, they ignite on contact with a flame; dust-extraction systems, explosion-proof electrical equipment and bonding are required to control dust accumulation.
❓ Q: What documents are needed to place equipment on the market?
A: Per Part 1, a technical document and construction file, risk-assessment report, instructions, marking and declaration of conformity are needed to satisfy EU/UK machinery legislation.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply