🧪 BS EN ISO 7539 is the British Standard series published by BSI as an identical adoption of the ISO 7539 series for corrosion of metals and alloys — stress corrosion testing, prepared by UK committee ISE/NFE/8 (Corrosion of metals and alloys). The series specifies uniform test procedures, specimen preparation and test methods for evaluating the susceptibility of metallic materials to stress corrosion cracking (SCC) under the combined action of a corrosive environment and tensile stress. It is an important basis for evaluating the environmental fracture performance of metallic materials in nuclear power, petrochemical, offshore engineering, aerospace and other industries.
The BS EN ISO 7539 series is organised by specimen type and loading method. Current parts include BS EN ISO 7539-1 (general guidance on testing procedures), 7539-3 (U-bend specimens), 7539-4 (uniaxially loaded tension specimens), 7539-6 (pre-cracked specimens under constant load or constant displacement), 7539-10 (reverse U-bend method) and 7539-11 (guidelines for testing the resistance to hydrogen embrittlement and hydrogen-assisted cracking). Parts 1, 10 and 11 are readable text; the rest are scanned copies.
| Standard | Subject | Core Content |
|---|---|---|
| BS EN ISO 7539-1:2012 | General guidance on testing procedures | General SCC testing principles, environmental conditions, stress application and result assessment guidelines |
| BS EN ISO 7539-3:1995 | U-bend specimens (scanned) | Preparation and testing of U-bend specimens |
| BS EN ISO 7539-4:1995 | Uniaxial tension specimens (scanned) | Constant-load/constant-strain uniaxial tension test methods |
| BS EN ISO 7539-6:2011 | Pre-cracked specimens (scanned) | SCC testing of pre-cracked specimens under constant load or constant displacement |
| BS EN ISO 7539-10:2014 | Reverse U-bend method | Reverse U-bend test method |
| BS EN ISO 7539-11:2014 | Hydrogen embrittlement and hydrogen-assisted cracking | Guidelines and procedures for testing resistance to hydrogen embrittlement and hydrogen-assisted cracking |
BS EN ISO 7539-1 specifies general principles for SCC testing, including the test environment (corrosive medium composition, temperature, pH, oxygen content), stress application methods (constant load, constant strain, constant displacement), selection of specimen type, test duration, and post-test assessment (crack detection, time to failure, threshold stress/stress intensity). It provides the general methodology for the other parts of the series.
BS EN ISO 7539-10 specifies the preparation and application of reverse U-bend specimens. Compared with the conventional U-bend, the reverse U-bend bends the specimen in the opposite direction so that tensile stress is generated on the outer surface; it is suitable for evaluating SCC susceptibility of thin sheets, tubes and other components under surface-tension service conditions.
BS EN ISO 7539-11 addresses hydrogen-induced cracking (hydrogen embrittlement) and hydrogen-assisted cracking (HAC), giving guidelines and procedures for testing under hydrogen-containing media or hydrogen-charging conditions, covering environmental fracture evaluation of hydrogen-sensitive materials such as high-strength steels and titanium alloys.