🎨 The BS EN ISO 28199 series specifies methods for evaluating the properties of coating systems related to the application (coating) process, providing a systematic tool for process commissioning and quality improvement in industrial coating such as automotive and furniture. Published by BSI as the UK implementation of EN ISO 28199, the technical content is identical to ISO 28199 (Part 1 incorporates the December 2009 corrigendum) and was prepared by ISO/TC 35 (Paints and varnishes) in collaboration with CEN/TC 139 (Paints and varnishes), with UK participation entrusted to Technical Committee STI/10 (Test methods for paints). The series comprises three parts.
💡 The most common problems in coating production (sagging, bubbling, pinholing, insufficient hiding, colour inconsistency) are mostly related to the compatibility of the paint formulation and the application process. BS EN ISO 28199 converts these into quantifiable evaluation methods, helping coating and painting engineers quickly identify root causes.
1. Series Structure and Scope 📌
The series consists of three parts:
| Standard | Year | Title | Content |
| BS EN ISO 28199-1 | 2009 (inc. 2010 corrigendum) | Relevant vocabulary and preparation of test panels | Unifies terminology and specifies test panel preparation. |
| BS EN ISO 28199-2 | 2009 | Colour stability, process hiding power and other properties | Colour stability, process hiding power, re-dissolving, overspray absorption, wetting, surface texture and mottling. |
| BS EN ISO 28199-3 | 2009 | Visual assessment of sagging, bubbling, pinholing and hiding power | Visual assessment of sagging, bubble formation, pinholing and hiding power. |
All parts fall under ICS 87.040 (Paints and varnishes). The standard applies to evaluation of coating properties closely related to application processes such as spraying or roll coating, especially multi-layer systems (primer, intermediate, topcoat, clearcoat) on metal substrates.
⚠️ The series evaluates “process-related properties”, i.e., the behaviour of coatings under specific application conditions, which depend strongly on application equipment, spray booth environment and operating parameters. Evaluation should be as close as possible to actual production conditions with consistent parameters for comparison.
2. Vocabulary and Test Panel Preparation (Part 1) 📖
Part 1 (BS EN ISO 28199-1:2009) gives terminology definitions for process-related property evaluation and specifies test panel preparation methods. It unifies the meanings of terms such as overspray, sagging, hiding and mottling, ensuring consistent evaluation criteria across personnel and laboratories.
The panel preparation method specifies substrate selection, surface treatment, application method, film thickness control and drying/curing conditions, ensuring all parts of the series are tested on a standardized basis.
3. Colour Stability and Process Hiding Power (Part 2) 🎯
Part 2 (BS EN ISO 28199-2:2009) specifies evaluation methods for several process-related properties, including:
- Colour stability: Colour consistency of the coating during application and drying.
- Process hiding power: The ability of the coating to cover the substrate under actual application conditions.
- Re-dissolving: The tendency of the applied coating to be re-dissolved by the solvent of a subsequent coat.
- Overspray absorption: The degree to which the coating absorbs overspray particles.
- Wetting: The spreading/wetting behaviour of the coating on the substrate.
- Surface texture and mottling: Micro-texture uniformity of metallic/pearlescent coatings.
These properties are critical to the appearance quality of automotive topcoats (especially metallic and pearlescent paints), directly affecting first-pass yield and rework rate.
4. Visual Assessment of Sagging, Bubbling, Pinholing and Hiding Power (Part 3) 🔍
Part 3 (BS EN ISO 28199-3:2009) specifies visual assessment methods for sagging, bubble formation, pinholing and hiding power. These defects are the most common quality issues on the shop floor: sagging refers to the coating running down under gravity, bubbles and pinholes refer to bubbles or small pores formed within or on the coating, and insufficient hiding leaves the substrate visible.
This part prepares panels with a defined film-thickness gradient and uses reference patterns or criteria for visual assessment, providing a unified basis for defect grading, supporting quantitative defect statistics and process improvement.
5. Engineering Practice Applications 🛠️
- 🚗 Automotive coating: Topcoat colour consistency, process hiding and appearance defect control.
- 🔧 Paint development: Process-property verification of new formulations under application conditions.
- 🏭 Coating line commissioning: Correlation analysis between spray booth parameters (viscosity, flow, air pressure) and film defects.
- 📊 Quality improvement: Quantitative statistics and continuous improvement of coating defects.
✅ Combining quantitative process-property evaluation with production data can significantly reduce rework and material waste. For appearance-sensitive systems such as metallic and pearlescent paints, the mottling and colour stability assessment of Part 2 is especially critical.
6. Frequently Asked Questions ❓
❓ Q: What is the difference between the objects evaluated in Parts 2 and 3?
A: Part 2 evaluates performance-type indicators such as colour, hiding, wetting and texture; Part 3 addresses defect-type indicators such as sagging, bubbling and pinholing through visual assessment.
❓ Q: What is the difference between process hiding power and conventional hiding power?
A: Conventional hiding power is measured under standard conditions; process hiding power is measured under actual application conditions (film thickness distribution, spray parameters), closer to production reality.
❓ Q: Why is mottling evaluation important?
A: The metallic flakes in metallic and pearlescent paints can locally aggregate or segregate during spraying, forming light/dark mottling that seriously affects appearance, requiring dedicated uniformity assessment.
❓ Q: How can sagging and pinholing defects be reduced?
A: Through comprehensive optimization of paint rheology (thixotropy), application viscosity, film thickness control, flash-off and baking conditions, and spray booth temperature/humidity.