🛢️ BS EN ISO 23936 is the BSI series for non-metallic materials in the petroleum, petrochemical and natural gas industries, implementing the ISO 23936 family and classified under ICS 75.180.01 (equipment for petroleum and natural gas industries). The series specifies material selection, qualification and performance requirements for thermoplastics and elastomers in contact with oil and gas production media, and is the basis for material selection and validation of non-metallic components such as packers, seals, flexible pipes and downhole tools.
💡 Oil and gas media often contain CO₂, H₂S, hydrocarbons and high temperature/pressure environments; failure modes of non-metallic materials such as swelling, degradation and rapid gas decompression (RGD) directly affect wellbore safety, making systematic material qualification essential.
1. Series Overview and Structure 📌
| Part | Year | Corresponding ISO | Subject |
| BS EN ISO 23936-1 | 2009 | ISO 23936-1:2009 | Thermoplastics |
| BS EN ISO 23936-2 | 2011 | ISO 23936-2:2011 | Elastomers |
The series was prepared by ISO/TC 67 (materials, equipment and offshore structures for petroleum, petrochemical and natural gas industries); in the UK it is the responsibility of PSE/17/-/7 (UK experts in ISO TC 67 Working Groups).
⚠️ During the development of BS EN ISO 23936-1 the UK committee voted against its approval, considering that Subclause 4.2 did not adequately present the characteristic properties of some material variants and candidate materials for oil and gas service, and recommended combining API 17TR, NORSOK M-710, BS EN ISO 13628 and other related codes for more comprehensive qualification.
2. Part 1: Thermoplastics 🔧
BS EN ISO 23936-1 specifies material selection and qualification requirements for thermoplastics in oil and gas production service, covering mainly:
- Material selection: select suitable thermoplastic materials according to media composition, temperature, pressure and service conditions, considering ageing, swelling and chemical degradation.
- Qualification tests: expose materials to a defined simulated production medium (see the hydrocarbon mixture in Table B.1 of the standard) and service temperature, perform immersion ageing tests, and measure mass/volume change and retention of mechanical properties.
- Long-term performance: for large applications refer to API Technical Report 17TR:2003 to decide test methodology; for small applications refer to the latest revision of NORSOK M-710.
- Coordination with related codes: subsea applications per the BS EN ISO 13628 series, polyethylene pipe applications per BS EN 1555 and BS EN 12201 series, wellhead equipment per BS EN ISO 10423, and valves per BS EN 13942.
💡 Where the oil to be simulated for the area of interest differs so much from that in Table B.1 that incorrect liquid absorption characteristics would be measured, the optional hydrocarbon mixtures in the latest revision of NORSOK M-710 may be used.
3. Part 2: Elastomers 🔩
BS EN ISO 23936-2 specifies qualification requirements for elastomers (e.g. NBR, HNBR, FKM, AFLAS) in oil and gas production service:
- Media exposure tests: immersion in the simulated production medium at defined temperature, evaluating volume swelling, hardness change and retention of tensile properties.
- Rapid gas decompression (RGD): tests to prevent internal blistering and cracking of elastomers caused by rapid pressure release of dissolved gas.
- Compression set and sealing performance: persistent sealing capability of seals (O-rings, gaskets) at high temperature and pressure.
- Service life evaluation: estimate service life from long-term ageing tests to support maintenance intervals and replacement strategies.
🚨 Elastomer seal failure is a primary source of oil and gas well control risk: material selection must simultaneously consider media compatibility, temperature limits, decompression rate and installation conditions; the qualification report should be a mandatory part of design and procurement documentation.
4. Summary of Key Technical Requirements 📋
| Item | Part 1 (Thermoplastics) | Part 2 (Elastomers) |
| Simulated medium | Hydrocarbon mixture (Table B.1 and NORSOK optional oils) | Simulated production medium/fluid |
| Key tests | Immersion ageing, mass/volume change, mechanical property retention | Swelling, RGD, compression set, strength retention |
| Service conditions | Temperature, pressure, media composition | Temperature, pressure, decompression rate |
| Related codes | API 17TR, NORSOK M-710, ISO 13628, ISO 10423 | NORSOK M-710, ISO 13628, etc. |
| Output | Material qualification report, selection guidance | Seal life assessment, qualification report |
5. Practical Engineering Application ⚙️
- 🔍 Selection process: define media composition and operating conditions → preselect material → design qualification tests per the standard → issue qualification report → incorporate into design documentation.
- 🔧 Seal design: O-ring and sealing system design must incorporate elastomer qualification data, considering installation, compression and temperature cycling.
- 📊 Supply chain verification: require suppliers to provide ISO 23936 qualification test reports and material batch consistency certificates at procurement.
- 📋 Operations and maintenance: set inspection/maintenance intervals from life assessment and monitor seal and thermoplastic component condition to prevent sudden failures such as RGD.
6. Frequently Asked Questions ❓
❓ Q: How does this series relate to NORSOK M-710?
A: ISO 23936 provides an international framework for qualification of non-metallic materials in oil and gas service, while NORSOK M-710 is widely adopted on the Norwegian continental shelf, is more detailed and is often used as a supplement; the two are often combined in practice.
❓ Q: Why cannot material be selected directly from handbook data?
A: Handbook data usually come from standard environments and do not reflect coupled effects of swelling, degradation and high-pressure decompression in oil and gas media; qualification tests per the actual media and conditions are required.
❓ Q: What is rapid gas decompression (RGD)?
A: When pressurised gas dissolved in an elastomer is rapidly released from the system, the gas nucleates inside the material forming bubbles and cracks, which may cause seal failure; the standard evaluates RGD resistance through specific tests.
🔍 Q: How is this series used in subsea applications?
A: Subsea production systems should use the BS EN ISO 13628 series together with this series for selection and qualification of non-metallic components, considering additional effects of seawater and completion fluids.
❓ Q: Does the standard give specific temperature/pressure values?
A: The series mainly provides a method framework and requirements; specific test temperatures/pressures should be determined with reference to BS EN ISO 10423, NORSOK M-710 and the actual well conditions of the project.