Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
Physical Address
304 North Cardinal St.
Dorchester Center, MA 02124
☀️ The BS EN ISO 22975 series specifies durability and performance evaluation methods for solar collector components and materials, making it an important standard for ensuring long-term reliable operation of solar thermal collectors. Published by BSI as the UK implementation of EN ISO 22975, the technical content is identical to ISO 22975 and was prepared by ISO/TC 180 (Solar energy) in collaboration with CEN/TC 312 (Thermal solar systems and components), with UK participation entrusted to Technical Committee RHE/25 (Solar Heating). The series comprises three parts addressing evacuated tubes, solar thermal heat-pipes and absorber surfaces.
The series consists of three parts:
| Standard | Year | Title | Subject |
|---|---|---|---|
| BS EN ISO 22975-1 | 2016 | Evacuated tubes — durability and performance | Evacuated collector tubes (all-glass and heat-pipe type) |
| BS EN ISO 22975-2 | 2016 | Heat-pipes for solar thermal application — durability and performance | Heat-pipes for solar thermal systems |
| BS EN ISO 22975-3 | 2014 | Absorber surface durability | Selective absorber coatings |
All three parts fall under ICS 27.160 (Solar energy engineering). The standard applies to key components of flat-plate and evacuated-tube collectors, evaluating durability and performance retention under long-term outdoor service, providing a component-level basis for collector lifetime prediction and quality certification.
Part 1 (BS EN ISO 22975-1:2016) specifies durability and performance test methods for evacuated tubes used in solar collectors. The vacuum layer between two glass tubes reduces heat loss, making it the core of all-glass and heat-pipe evacuated collector tubes. This part evaluates vacuum retention (vacuum aging), glass structural strength, thermal performance (absorptance, emittance), temperature cycling resistance and damp-heat resistance.
Through accelerated aging and performance tests, it can be determined whether evacuated tubes will suffer vacuum loss, coating degradation or glass breakage in long-term service, providing an important basis for quality certification and engineering selection.
Part 2 (BS EN ISO 22975-2:2016) specifies durability and performance test methods for heat-pipes for solar thermal applications. Heat-pipes transfer heat through phase change of the working fluid, offering fast start-up, freeze protection and one-way heat conduction, and are widely used in heat-pipe evacuated collector tubes. This part evaluates start-up characteristics, heat transfer performance, operating temperature range, durability (working-fluid stability, sealing) and performance retention under long-term thermal cycling.
Heat-pipe reliability directly affects collector output power and service life, so this part is important for production quality control and engineering application.
Part 3 (BS EN ISO 22975-3:2014) specifies durability test methods for selective absorber coating surfaces. Absorber coatings typically require high solar absorptance and low thermal emittance; the retention of their optical properties under long-term high temperature, UV irradiation and damp heat directly determines collector efficiency.
This part evaluates surface durability by comparing optical properties (absorptance, emittance) before and after accelerated aging (high temperature, thermal cycling, damp heat, irradiation), providing a basis for absorber coating material selection and quality grading.