💧 BS EN ISO 22391 is the European/international standard adopted by BSI specifying requirements for plastics piping systems made of polyethylene of raised temperature resistance (PE-RT) for hot and cold water installations. Developed by ISO/TC 138 (Plastics pipes, fittings and valves for the transport of fluids) with CEN/TC 155, it was prepared in the UK by Technical Committee PRI/88/2 (Plastic piping for pressure applications) under ICS 23.040.20, 91.140.60 and 93.025. The series applies to building hot/cold water, heating and underfloor heating systems; PE-RT combines the toughness and chemical resistance of polyethylene with better high-temperature creep resistance.
⚠️ The UK national foreword notes that compliance with this Standard does not necessarily mean products are fit for non-potable hot water pipes and does not replace BS 7291 (Class S). The normal maximum operating cold-water supply pressure in the UK is 12.5 bar, which some application classes do not meet; the malfunction temperature in Table 1 is 100 °C, whereas boilers to BS EN 297/483/625 can reach 110 °C — refer to current UK practice in BS 7291-1.
1. Scope and Position 📌
The series applies to PE-RT piping systems for hot and cold water installations inside buildings, covering pipes, fittings and jointing methods, and specifies design requirements for defined temperature, pressure and service life. Part 1 gives general requirements and application classes; Part 2 specifies pipes; Part 3 specifies fittings; Part 5 specifies the fitness for purpose of the system. Application must also be assessed against UK drinking-water and water fittings regulations.
💡 PE-RT is a “medium-density heat-resistant polyethylene” whose molecular structure incorporates comonomers, giving better long-term hydrostatic strength and creep resistance at elevated temperature, allowing it to withstand sustained hot-water temperatures.
2. Structure and Technical Highlights 🔧
| Part | Standard No. | Main Content |
| Part 1 | BS EN ISO 22391-1:2009 | General: terminology, application classes, pipe series, materials and common test criteria |
| Part 2 | BS EN ISO 22391-2:2009 | Pipes: dimensions, mechanical properties, long-term hydrostatic strength and marking |
| Part 3 | BS EN ISO 22391-3:2009 | Fittings: types, dimensions, mechanical and sealing performance |
| Part 5 | BS EN ISO 22391-5:2009 | Fitness for purpose of the system: verification of combined system and joint performance (scanned edition, written from public domain knowledge) |
The series is organised on two levels — “component” and “system”: the earlier parts specify pipe and fitting requirements individually, while Part 5 verifies the overall performance of the complete system, including joints, under actual service conditions.
3. Key Technical Requirements 🔥
- Material classification: PE-RT materials are graded by long-term hydrostatic strength (e.g. PE-RT type I/II); the minimum required strength (MRS) determines pressure capability;
- Application class and pipe series: define application classes by water temperature–pressure–time combinations, compute the required wall thickness from design stress, and select the pipe series (S) value for the design life;
- Pipe properties: outside diameter, wall thickness, ovality and wall uniformity meet tolerances; strength and creep are verified by short-/long-term hydrostatic, burst, tensile and heat-resistance tests;
- Fittings and joints: mechanical press-fit, crimp or fusion joints should pass sealing, pull-out and thermal-cycle tests to ensure no leakage;
- Fitness for purpose: the combined system should pass internal-pressure, thermal-cycle and pull-out resistance tests, verifying reliability under installation and service conditions;
- Hygiene compliance: when conveying drinking water, meet local contact-material regulations (e.g. Regulation 31/27/30 under the relevant UK regulations).
🚨 Pipe systems selected and certified per UK practice in BS 7291-1 ensure adequate safety margin under actual conditions such as boiler malfunction temperature (110 °C) and 12.5 bar supply pressure; otherwise, application classes in the Standard must be used to evaluate and verify the design.
4. Engineering Practice 🛠️
Practice points:
- 🔍 Design and selection: determine the application class and pipe series from design water temperature, pressure and service life, and calculate expansion compensation and support spacing;
- 🔧 Installation and jointing: perform press-fit/crimp or fusion connections per the manufacturer’s process, avoiding under-/over-crimping or poor fusion;
- 📊 Testing and acceptance: after installation, perform hydrostatic testing and flushing, verify joint sealing, and confirm compliance with local water regulations;
- 📋 Documentation: retain material certificates, test reports and installation records as a basis for acceptance and maintenance.
5. Frequently Asked Questions ❓
❓ Q: How does PE-RT differ from ordinary PE?
A: PE-RT introduces comonomers into the polyethylene backbone, keeping good toughness and chemical resistance while significantly improving long-term hydrostatic strength and creep resistance at high temperature, making it more suitable for hot water and heating systems.
❓ Q: How do BS EN ISO 22391 and BS 7291 relate?
A: 22391 is the international/European standard for PE-RT piping systems; BS 7291 (Class S) is the UK additional requirement for polybutylene and PEX pipe performance and drinking-water contact. UK practice often requires certification to BS 7291; they are not interchangeable.
❓ Q: How is the pipe series (S value) determined?
A: From the application class and design pressure, using the material design stress to calculate the required wall thickness, which determines the pipe series and diameter combination.
🔍 Q: Why is the fitness-for-purpose test important?
A: Individually qualified pipes and fittings can still fail at joints; system fitness tests verify overall performance through internal-pressure, thermal-cycle and pull-out tests, preventing joint leakage and quality problems in projects.