BS EN ISO 21627 — Determination of Chlorine Content of Epoxy Resins

Plastics — Epoxy Resins — Chlorine Content Testing

🧪 The BS EN ISO 21627 series specifies methods for determining the chlorine content of epoxy resins, serving as an important basis for quality control and electrical-performance evaluation. Chlorine residues in epoxy resins (inorganic chlorine, easily saponifiable chlorine and total chlorine) significantly affect the resin’s insulating properties, corrosion resistance and the electrical characteristics of the cured product, making chlorine content a key quality indicator especially in electrical, electronic packaging and composite applications. Published by BSI, the technical content is identical to ISO 21627:2002, with UK participation entrusted to Technical Committee PRI/42 (Fibre reinforced thermosetting plastics and prepregs).

💡 Chlorine in epoxy resins mainly originates from residual epichlorohydrin in the synthesis process. High chlorine content degrades the dielectric properties and moisture resistance of the cured product and can cause metal contact corrosion, so electrical-grade epoxy resins typically have strict chlorine limits.

1. Series Structure and Scope 📌

The series consists of three parts, each determining a different type of chlorine:

StandardYearAnalyteSupersedes
BS EN ISO 21627-12003Inorganic chlorineBS EN ISO 11376:2001
BS EN ISO 21627-22003Easily saponifiable chlorineBS EN ISO 4583:1998
BS EN ISO 21627-32003Total chlorineBS ISO 13651:1996

All three parts fall under ICS 83.080.10 (Thermosetting plastics) and apply to liquid or solid epoxy resins, including pure resins, modified resins and related prepreg systems. By measuring the three types separately, the chlorine species distribution can be fully understood: inorganic chlorine is mostly free chloride ions, easily saponifiable chlorine is hydrolyzable organic chlorine, and total chlorine is the sum of all chlorine.

⚠️ The methods, sample preparation and reagent requirements differ among the three parts. Choose the relevant part according to the control objective and state clearly the method and chlorine type in the report to avoid confusion between different methods.

2. Inorganic Chlorine Determination (Part 1) 🧂

Part 1 (BS EN ISO 21627-1:2003) specifies the determination of inorganic chlorine (free chloride ions) in epoxy resins. Inorganic chlorine usually exists as chloride ions (Cl⁻), which may be introduced by the synthesis process or raw materials. The resin sample is dissolved or extracted so that inorganic chlorine enters the aqueous phase, then chloride content is quantified by a suitable analytical method (e.g., potentiometric titration, argentometric method).

Inorganic chlorine is an important factor affecting resin electrical performance and metal corrosion; epoxy materials for high-end applications such as mobile phones and semiconductor packaging often have strict inorganic chlorine limits.

3. Easily Saponifiable Chlorine Determination (Part 2) 🔬

Part 2 (BS EN ISO 21627-2:2003) specifies the determination of easily saponifiable chlorine. This is organic chlorine that can be released by saponification (alkaline hydrolysis), mainly including active chlorine structures such as chloropropanol-type and chlorohydrin end groups. The sample is saponified under alkaline conditions to convert easily saponifiable chlorine to chloride ions, which are then quantified.

Easily saponifiable chlorine affects the curing reaction, storage stability and final properties of the resin; higher levels may influence the cured network structure and electrical performance.

4. Total Chlorine Determination (Part 3) ⚗️

Part 3 (BS EN ISO 21627-3:2003) specifies the determination of total chlorine content. Total chlorine covers all forms of chlorine in the resin, including inorganic chlorine and various organic chlorine structures. The sample is typically decomposed or mineralized at high temperature or under specific conditions to convert chlorine into a quantifiable form, followed by total chlorine quantification.

Total chlorine content is a comprehensive quality-control indicator for epoxy resins, used to verify the total chlorine introduced and as a common basis for procurement acceptance and batch-consistency inspection.

5. Engineering Practice Applications 🛠️

  • ⚡ Electrical insulation: Chlorine content control for electrical-grade epoxy resins in transformers, instrument transformers and casting compounds.
  • 📱 Electronic packaging: Ionic impurity control of epoxy molding compounds for semiconductor and IC packaging to prevent corrosion and leakage.
  • 🏗️ Composites: Resin quality inspection for fibre-reinforced thermosetting plastics and prepregs.
  • 🧾 Procurement acceptance: Incoming inspection and supplier batch-consistency evaluation of epoxy resin raw materials.
✅ By separately determining inorganic chlorine, easily saponifiable chlorine and total chlorine, the full chlorine distribution of the resin can be understood, providing a quantitative basis for formulation optimization, process improvement and quality grading, thereby improving cured-product reliability and electrical performance.

6. Frequently Asked Questions ❓

❓ Q: Why measure three types of chlorine separately?
A: Different chlorine types affect resin properties differently: inorganic chlorine mainly affects electrical performance and corrosion, easily saponifiable chlorine affects curing and structure, and total chlorine is a comprehensive indicator. Separate measurement reveals the full species distribution.
❓ Q: What problems does high chlorine content cause?
A: Excess chlorine degrades dielectric properties and moisture resistance of the cured product, can cause metal contact corrosion, and may affect the cured network structure, reducing reliability.
❓ Q: Can the three parts be used interchangeably?
A: No. They target different chlorine species with different sample preparation and analytical methods. Choose the relevant part according to the control objective and state the method in the report.
❓ Q: How can the chlorine content of epoxy resins be reduced?
A: Through optimized synthesis (e.g., reduced residual epichlorohydrin, enhanced washing/purification), high-purity raw materials, and post-treatment refining.
🔒