👁️ BS EN ISO 18369 specifies the terminology, classification, labelling specifications, dimensional tolerances and material physicochemical requirements for contact lenses in ophthalmic optics. A contact lens is an optical correction device worn directly on the corneal surface; its geometrical parameters (back vertex power, base curve, diameter, centre thickness) and material properties (water content, oxygen permeability, refractive index) directly determine wearing comfort, visual correction and corneal safety. BSI implemented the series as an identical adoption of the ISO 18369 International Standards in the EN ISO series, prepared jointly by ISO/TC 172 (Ophthalmic optics and instruments) and CEN/TC 170 — the base standard for contact lens design, manufacture, inspection and fitting management.
💡 Contact lens specification marking (e.g., -3.00 D, 8.6 mm base curve, 14.2 mm diameter) must match the wearer’s corneal parameters; if the geometry or material exceeds limits, it can cause blurred vision, corneal hypoxia or corneal damage. Standardised terminology, tolerances and material requirements are therefore critical.
1. Series Structure and Scope 📌
| Part | Standard | Subject | Key Content |
| Part 1 | BS EN ISO 18369-1:2006+A1:2009 | Vocabulary, classification system and labelling specifications | Terms (back vertex power, base curve, diameter, water content), material classification and specification-marking recommendations (incl. A1) |
| Part 2 | BS EN ISO 18369-2:2012 | Tolerances | Permissible deviations of geometrical and optical parameters (back vertex power, base curve, diameter) |
| Part 4 | BS EN ISO 18369-4:2006 | Physicochemical properties of contact lens materials | Determination of water content, oxygen permeability (Dk), refractive index and other material properties |
⚠️ ISO 18369 also includes Part 3 (measurement methods and instruments) among others; this batch of source material covers Parts 1, 2 and 4. Use the latest complete series for engineering/fitting applications.
2. Vocabulary, Classification and Labelling (Part 1) 📖
Part 1 establishes the unified terminology and classification system of the contact-lens field:
- Geometrical parameters: back vertex power, base curve, diameter, centre thickness, edge form;
- Material parameters: water content, refractive index, oxygen permeability (Dk), soft/hard lens classification;
- Classification system: by material (hydrogel, silicone hydrogel, rigid gas-permeable, etc.) and optical performance;
- Labelling specifications: specification marking on packaging and instructions (e.g., lens name, material, back vertex power, base curve, diameter) and recommended notation.
🚨 Incorrect labelling is a major hazard in contact lens fitting: if the marked base curve, diameter or back vertex power does not match the product, the practitioner may fit a mismatched lens, causing corneal damage or poor correction. Production and fitting must strictly label and verify per Part 1.
3. Tolerances (Part 2) 📏
Part 2 specifies the permissible deviations of the main parameters from their nominal values, for example:
- Back vertex power: tolerances graded by power magnitude (e.g., ±0.25 D), ensuring correction accuracy;
- Base curve: permissible deviation of the base-curve radius, ensuring match with the corneal curvature;
- Diameter: permissible deviation of total diameter, ensuring coverage and comfort;
- Centre thickness: thickness tolerance affecting oxygen transmission and mechanical performance.
✅ Tolerance control ensures batch-to-batch consistency: practitioners assess whether a lens is suitable for a given cornea from its nominal parameters and tolerance range, while manufacturers control quality per batch by tolerance inspection.
4. Material Physicochemical Properties (Part 4) 🔬
Part 4 specifies the methods for determining the key properties of contact lens materials:
- Water content: the water fraction of hydrogel materials, affecting oxygen transmission, wettability and protein adsorption;
- Oxygen permeability (Dk): the ability to transmit oxygen, directly related to corneal oxygen supply and long-term wearing safety;
- Refractive index: optical property of the material used to compute lens optical parameters;
- Others: material density, mechanical and surface properties (as specified).
5. Engineering Practice Applications 🏥
- 🔍 Product development and registration: define lens parameters and material properties per this series to support product registration and type testing.
- 📐 Production quality control: factory inspection of back vertex power, base curve, diameter and water content to ensure batch consistency.
- 🔧 Fitting and prescription management: practitioners interpret lens parameters from standard marking and select a lens matching the cornea and correction need.
- 📋 Regulation and compliance: contact lenses as medical devices are tested and marked per this series and applicable regulations to ensure wearer safety.
6. Frequently Asked Questions ❓
❓ Q: What is the “back vertex power” of a contact lens?
A: It is the vertex power measured in air with the lens back surface as the reference (in dioptres, D); it is the core optical parameter determining visual correction, and the negative/positive power in a fitting prescription corresponds to the back vertex power.
🔍 Q: Why is the “base curve” important?
A: The base curve is the radius of curvature of the lens back surface and must match the anterior corneal curvature; an improper base curve can cause a too-tight fit (corneal damage) or too-loose fit (movement, blur), so the practitioner measures corneal curvature and selects an appropriate base curve.
🔧 Q: What is the significance of the oxygen permeability (Dk)?
A: Dk reflects the ability of the material to transmit oxygen and is directly linked to corneal oxygen supply. High-Dk materials (e.g., silicone hydrogel) suit extended wear and reduce corneal hypoxia risk; for soft lenses permeability is often expressed as Dk/t (transmissibility).
📋 Q: Is a higher water content always better?
A: Not necessarily. High-water-content soft lenses are comfortable initially but dehydrate more easily, deposit more protein and can worsen dry-eye symptoms; water content, oxygen permeability, mechanical strength and wettability must be balanced according to the ocular condition.
❓ Q: How is contact-lens safety ensured as a medical device?
A: Perform design verification, type testing and factory inspection per this series (parameters, tolerances, material properties) and applicable medical-device regulations; wearers must be fitted by a qualified practitioner, attend regular follow-ups, and stop wearing and seek care immediately if discomfort occurs.