BS EN ISO 17652 — Test for Shop Primers in Relation to Welding and Allied Processes Standard Series

Welding — Test for Shop Primers in Relation to Welding and Allied Processes (2003 Edition, identical to ISO 17652)

🔥 BS EN ISO 17652 is the European standard adopted by BSI specifying test methods for shop primers (prefabrication primers) in relation to welding and allied processes, including thermal cutting and gas-shielded welding. Developed by ISO/TC 44 (Welding and allied processes) with related CEN working groups, it was prepared in the UK by Technical Committee WEE/42 (Prefabrication primers) under ICS 25.160.10. The series is essential for assessing whether the temporary protective primer applied after steel surface preparation affects welding quality, cutting performance and welding fume generation.

💡 Shop primers are widely used in shipbuilding, bridges and steel fabrication as temporary protection after grit blasting, before the final coating. Thin and containing zinc dust or inert pigments, a poorly designed primer can reduce weld penetration, cause porosity or increase welding fume.

1. Scope and Position 📌

The series applies to the assessment of the interaction of shop primers (prefabrication primers) with welding and allied processes such as thermal cutting. It does not replace welding procedure qualification standards (e.g. ISO 15614); it specifically evaluates the effect of this intermediate primer layer on weld metallurgy, thermal-cutting quality and occupational health. Part 2 supersedes BS 6084-1:1997 (withdrawn) in the UK.

⚠️ Welding-property tests are normally performed under standard welding conditions; actual welding parameters, groove geometry and primer thickness may differ, so results should be reviewed against the specific procedure.

2. Structure and Technical Highlights 🔧

PartStandard No.Main Content
Part 1BS EN ISO 17652-1:2003General requirements: terminology, test principles, specimen preparation and acceptance criteria
Part 2BS EN ISO 17652-2:2003Welding properties of shop primers: assessment of weld defects, mechanical properties and metallurgical effects
Part 3BS EN ISO 17652-3:2003Thermal cutting: assessment of the effect of the primer on oxy-fuel and plasma cutting quality
Part 4BS EN ISO 17652-4:2003Determination of emission of fumes and gases (scanned edition, written from public domain knowledge)

Part 1 provides the common test framework; Part 2 assesses weld quality (porosity, slag inclusions, cracks, lack of fusion) and welding performance; Part 3 assesses cut quality and cutting speed for thermal cutting (gas cutting, plasma cutting); Part 4 addresses fumes and harmful gases (e.g. ozone, nitrogen oxides) produced during welding and cutting.

3. Key Technical Requirements 🔥

  • Primer thickness and condition: tests use primers at a specified dry film thickness (typically 15–30 μm) with controlled drying and curing to simulate actual workpiece conditions;
  • Welding-property assessment: through weld appearance, radiography or ultrasonic testing, metallography and mechanical tests (tensile, bend, impact, etc.), judge whether the primer causes porosity, slag or reduced joint performance;
  • Thermal-cutting assessment: check cut-surface quality (slag adhesion, kerf width, heat-affected zone), cutting speed and squareness to judge interference of the primer with the cutting process;
  • Fumes and gases: collect welding fume and gases in an enclosed or extracted environment, measure generation rate and composition to assess potential health effects on operators;
  • Assessment report: record primer brand, thickness, welding parameters, test methods and results, and decide whether the primer is suitable for a given welding procedure.
✅ A qualified shop primer should, under the specified welding procedure, produce no weld defects or fume beyond the limits and maintain acceptable cut quality after cutting, balancing steel protection with processability.

4. Engineering Practice 🛠️

Practice points:

  • 🔍 Selection: when choosing a shop primer, treat welding properties, cutting performance and fume emission as evaluation criteria as important as anti-corrosion performance;
  • 🔧 Process matching: choose test conditions according to the actual welding method (shielded metal arc, MIG/MAG, submerged arc, etc.) and primer type to avoid mismatch between primer and filler metal;
  • 📊 Thickness control: strictly control dry film thickness — too thick increases the risk of porosity and slag, too thin gives insufficient protection;
  • 📋 Traceability: establish records linking primer batch and welding procedure as part of steel structure fabrication quality control.

5. Frequently Asked Questions ❓

❓ Q: Why do shop primers affect weld quality?
A: The organic resin, zinc dust or pigments decompose or vaporise under the heat of the arc, generating gas that can cause porosity, or forming slag and reducing penetration; a poorly designed formulation can also lower joint mechanical properties.
❓ Q: Can this series replace welding procedure qualification?
A: No. It specifically evaluates the effect of the primer on welding, cutting and fume emission; the welding procedure itself is qualified under standards such as ISO 15614.
❓ Q: What is the significance of the Part 4 fume-emission determination?
A: Welding and thermal-cutting fume contains metal particulates and harmful gases; measuring emissions helps assess occupational exposure risk in the workplace and guides ventilation and personal protective equipment design.
🔍 Q: Does primer thickness strongly affect welding performance?
A: Yes. Excessively thick primer causes porosity, slag and reduced penetration in the weld; dry film thickness should be kept within the standard or manufacturer’s recommended range and reduced near groove edges where appropriate.
🔒