📐 The BS EN ISO 13565 series is a set of British Standards implementing the European standard EN ISO 13565 in the field of Geometrical Product Specifications (GPS), specifying the measurement and characterisation of surfaces having stratified functional properties using the profile method. Stratified functional surfaces are surfaces produced by honing, broaching, grinding and similar processes that have a distinct plateau-valley dual structure, such as the honed surface of an engine cylinder bore. Such surfaces cannot be adequately characterised by traditional parameters like Ra or Rz, so dedicated filtering and characterisation methods are required. UK participation was entrusted to Technical Committees MTE/27 and TDW/4/-/3 (Properties and metrology of surfaces). The ICS classification is 17.040.20 (surface properties).
💡 The “plateau” of a stratified functional surface supports loading and sliding, while the valleys store lubricant and trap wear debris. ISO 13565 is the dedicated assessment tool for such surfaces — its material ratio curve and material probability curve parameters are highly valuable for predicting bearing, wear and lubrication performance.
1. Series Composition 📌
The series comprises three documents, corresponding to the filtering/measurement conditions and two height characterisation methods of ISO 13565:
| Standard | Year | Title / Subject | Main Content |
| BS EN ISO 13565-1 | 1998 | Filtering and general measurement conditions | Filtering rules, cut-off wavelengths and general measurement conditions for stratified surfaces |
| BS EN ISO 13565-2 | 1998 | Height characterisation using the linear material ratio curve | Height parameters Rk, Rpk, Rvk, Mr1, Mr2 based on the linear material ratio (Abbott) curve |
| BS EN ISO 13565-3 | 2000 | Height characterisation using the material probability curve | Plateau and valley parameters Rpq, Rvq, Rmq based on the material probability curve |
⚠️ Stratified surfaces cannot be assessed with a normal Gaussian filter. The standard requires a special filtering method (such as splitting by the material ratio curve) to separate the plateau and the valleys, otherwise valley depth distorts the plateau parameters and the values become meaningless.
2. Filtering and General Measurement Conditions (Part 1) 🔧
Part 1 specifies the filtering and general measurement conditions for stratified functional surfaces. It defines filtering rules tailored to this surface type, and specifies the cut-off wavelength, evaluation length, sampling length and other conditions, and how the effect of waviness is removed before measurement, providing a consistent measurement basis for subsequent parameter evaluation. The probe geometry and sampling interval of the measuring instrument (stylus instrument) must also comply.
3. Linear Material Ratio Curve Characterisation (Part 2) 📊
Part 2 specifies height characterisation using the linear material ratio curve (the Abbott bearing area curve). By dividing the material ratio curve at its best-fit straight line, the following parameters are defined:
- Rk: core roughness depth (core region height).
- Rpk: reduced peak height (peak region, initial wear).
- Rvk: reduced valley depth (valley region, oil retention).
- Mr1, Mr2: material ratio at the split points (proportions of plateau and valleys).
4. Material Probability Curve Characterisation (Part 3) 🧪
Part 3 specifies height characterisation using the material probability curve. The material probability curve expresses the material ratio as a function of height in Gaussian probability coordinates, dividing the surface into a plateau region and a valley region as two straight lines, thereby defining:
- Rpq: height parameter corresponding to the plateau slope (plateau roughness).
- Rvq: height parameter corresponding to the valley slope (valley depth).
- Rmq: material ratio at the split between the plateau and valley regions.
The advantage of this method is that it quantifies the plateau region and the valley region independently, making it especially suitable for assessing plateau quality and oil-retention capacity, overcoming the limitations of a single height parameter.
🚨 The reliability of characterisation depends on correct filtering and measurement state beforehand. Ensure the stylus runs perpendicular to the lay direction, the sampling length covers enough texture periods, and the surface is clean and dry; otherwise the plateau parameters will not reflect the true functional characteristics.
5. Engineering Practice and Applications 🛠️
- 🔍 Engine manufacture: honed cylinder bore surfaces are assessed for bearing and oil-retention behaviour using Rk/Rpk/Rvk and Rpq/Rvq, guiding honing process optimisation.
- 📋 Quality acceptance: stratified surface parameters are included in drawings and inspection specifications, measured and judged per ISO 13565.
- 🏭 Tribology assessment: used to evaluate running-in, bearing and lubrication behaviour of sliding interfaces and to predict wear life.
- 📊 GPS integration: ISO 13565 belongs to the GPS surface texture family, used together with ISO 4287 (surface profile parameters), ISO 4288, ISO 3274 and related standards.
6. Frequently Asked Questions ❓
❓ Q: Why can’t Ra characterise a stratified surface?
A: Ra is the arithmetic mean deviation and is insensitive to the plateau-valley dual structure; it cannot distinguish “many plateaus with shallow valleys” from “few plateaus with deep valleys”. Only the material ratio/probability curve parameters of ISO 13565 reflect the stratified characteristics accurately.
❓ Q: What do Rk, Rpk and Rvk represent?
A: Rk is the core roughness depth, Rpk the reduced peak height (initial wear) and Rvk the reduced valley depth (oil retention); together with Mr1 and Mr2 they describe the bearing and lubrication characteristics.
❓ Q: What is the difference between Part 2 and Part 3?
A: Part 2 uses the linear material ratio (Abbott) curve with parameters Rk/Rpk/Rvk/Mr1/Mr2; Part 3 uses the material probability curve, splitting the surface into plateau and valley regions with parameters Rpq/Rvq/Rmq. They emphasise different aspects and can complement each other.
🔍 Q: What should be noted when measuring?
A: Ensure the stylus runs perpendicular to the lay, the sampling and evaluation lengths comply with the standard, waviness is removed by correct filtering, and the surface is clean and dry, to obtain reproducible results.