🪟 BS EN ISO 12543 is the complete technical standard series for laminated glass and laminated safety glass used in building. Laminated glass is made of two or more sheets of glass bonded together by a polymeric interlayer (PVB, EVA, ionoplast and others), combining safety, sound insulation, impact resistance and UV protection. When the glass breaks, the fragments remain adhered to the interlayer and do not fall dangerously, making it widely used for curtain walls, skylights, balustrades, floors, doors and ballistic/blast-resistant applications. The series is the CEN adoption of the ISO 12543 series, implemented in the UK as British Standards, providing the basis for design selection, production inspection and construction acceptance of laminated glass products.
The performance of laminated glass depends on the substrate glass type, interlayer material and thickness, number of plies, lamination process and edge finishing. To standardise products and control quality, the series is organised logically: definitions (Part 1), product requirements for safety glass (Part 2), general laminated glass (Part 3), durability tests (Part 4), dimensions and edge finishing (Part 5), and appearance (Part 6). The six parts complement each other to form a complete chain of requirements for laminated glass products.
| Standard | Part Subject | Main Requirements |
|---|---|---|
| BS EN ISO 12543-1 | Definitions and description of component parts | Terminology, classification of glass/interlayer/edge types |
| BS EN ISO 12543-2 | Laminated safety glass | Safety performance, post-impact fragment state, penetration resistance |
| BS EN ISO 12543-3 | Laminated glass | General building performance, defect classification and limits |
| BS EN ISO 12543-4 | Test methods for durability | High-temperature/humidity, UV radiation, post-aging appearance and performance |
| BS EN ISO 12543-5 | Dimensions and edge finishing | Finished-dimension tolerances, edge grinding and chamfering |
| BS EN ISO 12543-6 | Appearance | Assessment of bubbles, inclusions, scratches, edge defects |
The interlayer is decisive for laminated-glass performance. PVB (polyvinyl butyral) is the most common thermoplastic interlayer, offering excellent adhesion, transparency and impact resistance; EVA and ionoplast (e.g., SentryGlas) suit structural and outdoor weathering applications. The standard requires the interlayer thickness, ply count and total thickness to meet the product requirements, and specifies the adhesion quality between glass and interlayer to avoid delamination and bubbles.
Part 2 requires laminated safety glass, when subjected to pendulum-impact and drop-ball tests, to fracture with fragments retained by the interlayer as an integral, non-fragmenting whole, with defined fragment-state and penetration criteria. For ballistic and blast applications, additional performance verification against the relevant specialised standards is required.
Part 4 durability tests simulate the high-temperature/humidity and UV aging conditions experienced by building glass in service. After aging there should be no significant discoloration, blistering or delamination, and light transmittance and safety performance must remain compliant. For outdoor components, durability is a key indicator of long-term service performance.