BS EN ISO 10675 — Non-Destructive Testing of Welds — Acceptance Levels for Radiographic Testing

Part 1: Steel, nickel, titanium and their alloys; Part 2: Aluminium and its alloys

🎯 BS EN ISO 10675 specifies acceptance levels for the radiographic testing (RT) of welds, an important basis for weld quality control and NDT acceptance. The series is split by material: BS EN ISO 10675-1 applies to steel, nickel, titanium and their alloys, and BS EN ISO 10675-2 applies to aluminium and its alloys. The Standard defines the allowable sizes and assessment rules for various weld imperfections (gas pores, slag inclusions, lack of fusion, lack of penetration, cracks, undercut, etc.) as imaged on the radiograph, providing a common criterion for accepting or rejecting RT results.

💡 Radiographic testing reveals internal weld defects as images on a film or digital image through the differential attenuation of radiation in the workpiece. Acceptance levels define what “acceptable” defect images are — the bridge between the detection result and the quality judgement.

1. Series Overview and Scope 📌

In the UK this series is the responsibility of Technical Committee WEE/46 (Non-destructive testing). BS EN ISO 10675-1:2016 was prepared by ISO/TC 44 “Welding and allied processes” with CEN/TC 121 “Welding and allied processes”, approved by CEN in December 2016, and published as a British Standard on 31 January 2017, superseding the withdrawn BS EN ISO 10675-1:2013. BS EN ISO 10675-2:2013 is identical to ISO 10675-2:2010, was approved by CEN in August 2013, and published on 30 November 2013, superseding the withdrawn BS EN 12517-2:2008.

PartSubjectICSISO EquivalentMaterial
BS EN ISO 10675-1:2016Steel, nickel, titanium and their alloys25.160.40ISO 10675-1:2016Welds in steel, nickel, titanium and their alloys
BS EN ISO 10675-2:2013Aluminium and its alloys25.160.40ISO 10675-2:2010Welds in aluminium and its alloys
⚠️ The acceptance levels in this series are the pass/fail criteria for radiographic results; they do not themselves set the weld quality level or extent of testing. In practice, determine the weld quality level and test percentage per the product standard or design documents, then use this series to set the acceptance criteria.

2. Acceptance Levels and Defect Assessment (Part 1) 🔧

BS EN ISO 10675-1 specifies acceptance levels for radiographic testing of welds in steel, nickel, titanium and their alloys. The Standard typically gives several acceptance levels (e.g., levels 1, 2, 3), where a lower number means stricter limits on allowable defect size. Assessment covers:

  • Gas pores: size, number and distribution of individual pores.
  • Slag inclusions: size and distribution.
  • Lack of fusion / lack of penetration: allowable length of elongated imperfections.
  • Cracks: generally not permitted — a critical defect.
  • Undercut and other surface defects as projected on the radiograph: assessed per the relevant rules.

The Standard gives a unified method for size measurement, grouping, conversion and acceptance of defects, ensuring consistent assessment of the same radiograph by different inspectors and laboratories.

3. Aluminium and Its Alloys (Part 2) 🔩

BS EN ISO 10675-2 specifies acceptance levels for radiographic testing of aluminium and aluminium-alloy welds. Aluminium has low density and weak radiation absorption, and aluminium welds commonly contain pores, slag, lack of fusion and oxide inclusions; the assessment rules differ from steel. The Standard gives defect allowable sizes and assessment methods suited to aluminium.

Radiographic testing of aluminium welds is widely used in aerospace, shipbuilding, rail transport and chemical equipment. Because aluminium has high thermal conductivity and a large coefficient of thermal expansion, welding tends to produce pores and distortion, so the acceptance level must balance structural safety with process feasibility.

ComparisonSteel, Nickel, Titanium (Part 1)Aluminium and Alloys (Part 2)
Typical defectsPores, slag, lack of fusion, lack of penetration, cracksPores, slag, oxide inclusions, lack of fusion
Radiation absorptionStrongerWeaker (adjust exposure)
Typical applicationPressure vessels, steel structures, pipingAerospace, shipbuilding, rail transport
Acceptance levelsSeveral, chosen as requiredSeveral, chosen as required

4. Test Method and Image Quality 🛠️

Acceptance assessment is based on a satisfactory radiographic image. The Standard requires the RT to comply with the relevant method standard (e.g., ISO 17636) and that image quality meets the requirements for image-quality indicator (IQI) sensitivity, density and contrast. Only with acceptable image quality can the defect images on it be used for assessment.

  • Radiation source and exposure: select a suitable source (X-ray or γ-ray) and exposure parameters.
  • IQI: place the image-quality indicator per the Standard to verify the required sensitivity.
  • Film/digital image quality: density, grey scale, contrast and geometric unsharpness must meet requirements.
  • Viewing environment: film viewing should be performed under specified illumination and masking.

5. Engineering Application Practice 🌐

The BS EN ISO 10675 series is widely used in weld quality control of pressure vessels, boilers, steel structures, piping, storage tanks, ship hulls and aerospace structures. Manufacturers use it to judge RT results, supervisors and third parties to re-assess and accept, and inspection bodies to issue reports. In practice, the chosen acceptance level should match the structure’s stress level, load type, material toughness and service conditions, ensuring safety without excessive conservatism.

🚨 Crack-type defects (cracks, lack of fusion, lack of penetration and other linear defects) are generally regarded as unacceptable critical defects. Once such a defect is found, regardless of size, the weld should be judged nonconforming and repaired or treated.

6. Frequently Asked Questions ❓

❓ Q: Does a lower acceptance-level number mean stricter?
A: Usually a lower acceptance-level number (e.g., level 1) means stricter allowable defect sizes; a higher number (e.g., level 3) allows larger defects. Refer to the standard text for the exact correspondence.
❓ Q: Why are cracks generally not permitted?
A: Cracks are planar defects that readily propagate under load and are a main cause of brittle fracture and fatigue failure, so the Standard treats them as unacceptable.
❓ Q: How do BS EN ISO 10675 and ISO 17636 relate?
A: ISO 17636 specifies the method of RT (how to test); BS EN ISO 10675 specifies acceptance levels (how to judge). They are used together: first perform the test per the method standard, then assess per the acceptance level.
❓ Q: How does RT of aluminium differ from steel?
A: Aluminium has lower density and weaker absorption, requiring adjusted radiation energy and exposure to obtain a satisfactory image; and aluminium welds’ common defects (pores, oxide inclusions) have different assessment rules from steel, hence two parts.
🔒
正在加载下载地址,请稍候 10 秒

Leave a Reply