BS EN ISO 08871 — Elastomeric Parts for Parenterals and for Devices for Pharmaceutical Use

ISO 8871 series — chemical, physical, biological and functional evaluation of elastomeric components

💊 BS EN ISO 08871 (BS EN ISO 8871) is a core standard series for pharmaceutical packaging and drug-delivery devices. It specifies requirements for elastomeric parts (rubber closures, seals, gaskets, infusion-device elastomers) used in parenteral preparations and pharmaceutical devices. Since elastomeric parts contact the drug product directly, their extractables, released particles and biological properties directly affect drug safety and stability. BSI adopted the series as the identical EN ISO 8871 text, with UK participation under Technical Committee CH/212.

💡 For injectables, the rubber closure is often the component in contact with the drug solution for the longest time. Migrating vulcanisation agents, accelerators and fillers must stay within controlled limits, otherwise pH shifts, visible particles, or toxicity may arise.

1. Series Overview and Scope 📌

This series applies to elastomeric parts used in parenterals and pharmaceutical devices, covering the full chain from raw-material identification and process characterisation to finished-part functional verification. Part 1 addresses extractables in aqueous autoclavates, Part 2 identification and characterization, Part 3 released particles, Part 4 biological requirements and test methods, and Part 5 functional requirements and testing under intended use.

The parts are both independent and complementary, forming a systematic framework that evaluates elastomeric parts across four dimensions — chemical, physical, biological and functional.

⚠️ Evaluation must be tied to the intended use and contact conditions (drug type, temperature, sterilisation method, contact time). Compatibility conclusions for one drug solution cannot simply be extrapolated to another with the same formulation.

2. Series Structure and Part List 📑

PartYearSubjectStatus
Part 12004Extractables in aqueous autoclavatesReadable text
Part 22004 + A1:2014Identification and characterizationReadable text
Part 32004Determination of released particlesScan — written from public domain knowledge
Part 42006Biological requirements and test methodsScan — written from public domain knowledge
Part 52016Functional requirements and testingReadable (summary)

3. Extractables and Released-Particle Evaluation 🔧

Part 1 specifies how to extract extractables from elastomeric parts under defined autoclaving conditions with a defined medium (such as water), and how to evaluate the extract quantitatively and qualitatively. Extractable analysis typically combines total volatile/total residue determination with separation and identification techniques such as GC-MS and LC-MS. Part 3 concerns particles shed during use, prescribing a rinsing/leaching procedure and particle counting (e.g. light-obscuration) to measure particle number and size distribution.

🚨 Visible foreign matter and fine particles are key quality controls for injectables. Particles generated by elastomer–drug contact, if uncontrolled, may cause infusion reactions or block delivery systems; particle limits must be enforced at procurement and release.

4. Identification, Characterization and Biological Requirements 🛠️

  • Identification and characterization (Part 2): uses IR spectroscopy, thermal analysis (DSC/TGA) and other techniques to identify the elastomer material and formulation, and characterises physical properties such as density, hardness and tensile strength to ensure batch-to-batch consistency.
  • Biological requirements (Part 4): specifies biological tests such as cytotoxicity, sensitisation and irritation in line with general principles for drug-contact materials, adding pyrogen evaluation where appropriate.
  • Functional requirements (Part 5): specifies dedicated tests and pass limits for real-use functions such as puncture integrity, resealability, and slide/recovery behaviour in infusion devices.
💡 Even a minor formulation tweak can change the extractable profile and particle behaviour; any formulation change must trigger a full re-evaluation of extractables and biological properties.

5. Engineering Practice and Application Notes 📏

In pharmaceutical practice, elastomeric-part selection and acceptance follow the path: supplier qualification → incoming inspection → compatibility study → process validation. The recommended workflow: choose the elastomer formulation by drug nature and sterilisation conditions → obtain extractable and biological data from the supplier → run compatibility studies with the intended drug (extractables and leachables) → validate sterilisation and storage → enforce key particle and functional tests at batch release.

  • Compatibility study: reference ICH Q3D elemental-impurity assessment and packaging-material guidance, combined with this series, for leachables studies.
  • Goods-in control: perform appearance, dimension, hardness and stated aqueous-extract spot checks on each elastomer batch.
  • Traceability: maintain complete files of formulation, process batch numbers and test reports for regulatory audit.
⚠️ Cite the part and year when referencing this series; biological and compatibility requirements may change with regulations — verify against the latest official BSI edition and applicable pharmacopoeial/regulatory requirements.

6. Frequently Asked Questions ❓

❓ Q: Are extractables and leachables the same?
A: Not exactly. Extractables are substances extractable under exaggerated conditions, used to characterise the material; leachables are substances actually released and detected under real-use conditions. Part 1 focuses on standardised extractable evaluation.
❓ Q: Why measure released particles on rubber closures?
A: Closures may shed particles during puncturing, handling and contact with the drug; particles entering an injectable constitute a foreign-matter risk. Particle evaluation is a necessary safety check.
❓ Q: How are the biological tests selected?
A: Start with basic tests such as cytotoxicity, then choose sensitisation, irritation or systemic toxicity according to contact time and nature; the combination depends on the part’s use and regulatory requirements.
❓ Q: Can closures from different manufacturers be swapped freely?
A: No. Different formulations differ significantly in extractables, particles and compatibility; changing supplier or formulation requires repeating the compatibility study and validation.
🔒